The Sawing and
Drying Directory:
Find a Sawyer
Find a Kiln Dryer
Find a Grader
Create Your FREE
Listing

Looking for Lumber? Submit an Request for Quote

Related Information:
Products:
Lumber &
Plywood

Forums:
Sawing & Drying

Exchanges:
Lumber

Resources:
Timber & Lumber
Calculators

______________


Today's
Sponsors:


BetterVacuumcups.com

Biesse America

Biewer Lumber

Binks

Black Bros. Co.

Blackhawk Machinery

Briquetting Solutions by Sunomi LLC

Brown Wood Products Co.

Business Management Solutions

Byrd Tool

C.R. Onsrud

Cab Parts

Cabinet Door Service Co.

Cabinet Pro

CabinetCRUNCHER Cutlist & 3D Cabinet Design Software

Cabinetmakers Association

CADCABINETS.COM

CADCode

Cag Lumber

Cantek America

Carolina Woodworking Consultants

Carter Products

Carving Technologies

Castle

Catskill Timber Industries

Charles G.G. Schmidt Co.

Chicago Dowel Company, Inc.

Clear Lake Lumber

CNC Parts Dept.

1-800-Cabinets.com

2Sand.com

3M Corporation

A O M Spray Equipment

Abrasive Resource

Accu-Router, Inc.

AceCo Precision Wood Tooling

Activa

Air Handling Systems

Alan McIlvain Company

Algoma Lumber Co.

All Star Adhesives

Alliance Millsoft

Allied Machinery Inc.

AllRout

Amana Tool

Ameitech South

American Fabric Filter Co.

American Institute of Building Design

American National Woodworking Knife

American Rotary Converters

Andreou Machinery

ANEST IWATA USA, Inc.

Antique Beams and Boards

Antique Building Materials

Anver Corporation

Apollo Sprayers Inc.

Arbor Processing Inc.

Architectural Elements

ArtCam

ATEMAG

Atlantic Machinery Corp.

Auton Motorized Systems

AWFS

B.H. Davis Company

Bailey's Inc.

Baker Products

Banks Hardwoods

Barn Detail

Barn Door Lumber

BC Wood Specialties Group

BeamsRUS

Beaver Tools

Benz Incorporated

Best Cabinets


The figures in each column are prices per thousand board feet of kiln-dried lumber purchased in quantities of 1000 bd/ft and 200 bd/ft. (Divide these numbers by 1,000 to get median per-board-foot prices for respective species and grades.)

These are estimated distribution-yard prices for rough lumber; actual pricing may vary by distributor.

To get a specific price quote from suppliers on material that you need, click here

FAS stands for firsts and seconds, typically the best grade of kiln-dried, hardwood lumber. #1 Common is a lower grade, often used in cabinet and furniture making where piece sizes are smaller and defects can be eliminated by selective cutting.

All prices are based on a net tally or measurement after kiln drying.

Species

FAS

#1Common

Alder 4/4

2690-3530

1400-2250

Alder 5/4

3480-4330

1460-2300

Alder 8/4

2850-3700  

Ash 4/4

1160-2000 820-1660

Ash 5/4

1270-1810 960-1800

Ash 8/4

1410-2250 1110-1960

Basswood 4/4

1100-1950 730-1570

Basswood 5/4

1200-2050 730-1570

Basswood 8/4

1320-2170 770-1610

Cherry 4/4

2480-3330 950-1790

Cherry 5/4

2970-3820 1290-2140

Cherry 8/4

3530-4380 2330-3180

Hard Maple 4/4

1690-2530 1080-1940

Hard Maple 5/4

2160-3010 1180-2020

Hard Maple 8/4

2590-3440 1640-2480

Poplar 4/4

940-1780 650-1500

Poplar 5/4

970-1810 720-1570

Poplar 8/4

1080-1930 860-1710

Soft Maple 4/4

1440-2290 1030-1800

Soft Maple 5/4

17602610 990-1830

Soft Maple 8/4

2000-2850 1460-2300

Red Oak 4/4

1190-2040 940-1780

Red Oak 5/4

1500-2340 1040-1890

Red Oak 8/4

1920-2760 1360-2200

White Oak 4/4

1390-2230 860-1700

White Oak 5/4

1760-2600 1030-1880

White Oak 8/4

2660-3500 1570-2410

Walnut 4/4

3010-3860 1520-2370

Walnut 6/4

3950-4800 2190-3030

Walnut 8/4

4270-5120 2420-3270

Yellow Birch 4/4

2110-2960 1110-1960

Yellow Birch 8/4

   

 




Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

Contact us to discuss advertising or to report problems with this site.

To report a problem, send an e-mail to our Webmaster

Copyright © 1996-2009 - WOODWEB ® Inc.
All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
Review WOODWEB's Copyright Policy.

The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

WOODWEB, Inc.
RR4 Box 265A
Montrose, PA 18801

Contact WOODWEB













 Home » Resources » Lumber Buying Guide » Eastern Region
 
Lewis Lumber Products TigerwoodDecking.com
Request a Lumber Quote || Request a Machinery Quote