Adhesives

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Laminating Beams Advice

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Laminating Beams Advice

6/20/13       
Joe Wood  Member

Website: http://woodsshop.com/

So a customer would like a curved roof structure next to their pool here in San Diego, and I have a few questions.

This will need a permit, so for the adhesive I'd use either plastic resin or epoxy. Which glue would cost me less?

Could anyone help me estimate how much I'd need? There are 9 beams, each with 5 1x4s.

What type of epoxy would I use if I go that route?

since this would be structural I'm thinking I'd use doug fir 1x4s instead of my usual wr cedar. The fir I can get is still pretty wet, would this be an issue for the laminations?

here are a few conceptual images to give you an idea on the structure.


View higher quality, full size image (1000 X 650)


View higher quality, full size image (1000 X 650)


View higher quality, full size image (1000 X 650)

6/21/13       #3: Laminating Beams Advice ...
Adam Spees

That thing is going to cost a few bucks. I would be inclined to have an architect spec it to keep you out of any liability issues. If that's not in the budget, I would be slightly concerned.

I could be wrong, but I believe that epoxy is okay outside, but not inside because of fire and the low melting temp(200 F) of epoxy.

Brands of epoxy: West System, System 3, and MAS epoxy. There are a several other semi generic brands. All are good. Most people use West System because of availability and the medium viscosity. MAS is the most user friendly and cost effective, but not as available.

Doug Fir is strong, but not rot resistant. I would try to stick with cedar or redwood if possible.

The customer should have enough money to pay for proper design. Do not do this because its a "cool" project. They could always scale down the spans and size or do without the curves. All of those features drive up the cost by orders of magnitude.

Nice drawings and design. You may have to get a engineer or architect to sign off on it in order to get a permit depending on your location.

6/21/13       #4: Laminating Beams Advice ...
Joe Wood  Member

Website: http://woodsshop.com/

Thanks Adam, appreciate the advice, especially about the liability!

I'll probably go with the plastic resin glue. I called Dap and found out the coverage and these 9 beams up would cost about $70 for the glue, not bad at all.

I'll go with the cedar, and explain the probable need for an engineer or architect.

I did another laminated beam job quite a few years ago using redwood 1x4s and the original TBond and it held up fine.
http://woodsshop.com/arbors.htm

thanks again Adam :-)

6/24/13       #5: Laminating Beams Advice ...
Rich

Cedar doesn't have much structural strength, and can be brittle around knots. You should check with the adhesive folks if their glue likes cedar or redwood because of the oils in the wood. I agree with Adam, hire an licensed engineer to do the calculations.

6/26/13       #6: Laminating Beams Advice ...
GeneWengert-WoodDoc

There are two issues that need to be addressed. First is the strength of the wood. Although you do not need high strength for snow or roof components, you do need strength enough for someone, now or in the future climbing on the top, perhaps for maintenance or as a joke. Cedar and redwood are not strong species. At the same time, you need to avoid species that might decay, especially at the joints where water can be trapped. If you use pressure treated, then special fasteners must be used as well.

Second, we need to consider the durability of the adhesive subject to uv, heat and moisture. Special epoxy formulations are needed to avoid uv degradation. The adhesive must withstand wetting...some are called moisture resistant, but you need more protection. The adhesive must also be rated for construction use. For example, TB is not as it will slip too much...it is not rigid enough. Most often we use phenol or resorcinol based adhesives.

Due to liability issues, you do need advice from a professional on both species and adhesive.

6/26/13       #7: Laminating Beams Advice ...
Mark B Member

Some pretty impressive work on your site Joe.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)