accu-system glue
4/6/16
Website: http:// Rudolph specialty.com
We just installed a accu-system glue bore and dowel cnc machine,it was purchased used . Just wanted to know if we should use the pre-glued dowel's and water or inject glue with the dowels . Can any one tell me which way is the better way to go . Thanks Pete Rudolph .
4/8/16 #2: accu-system glue ...
Website: http://www.calwoodinc.com
We've used preglued dowels in our Accu HPJ for 10 years now. We've dealt with some minor rust issues on a few of the machine parts but I'd imagine wood glue would be quite messy. No complaints with the preglued dowel system. Good luck.
4/8/16 #3: accu-system glue ...
We tested both pre-glued and glue injection when we got our machine over 10 years ago. Went with glue because it tested stronger. To tell the truth pre-glue is probably strong enough. Pre-glue precautions: keep them enclosed during high humidity, cover the hopper to keep dust out. Glue precautions: keep the system clean, make a test shot of glue before starting each session. Don't know why a properly setup glue injection system would be "quite messy?" The only exposed part is the nozzle, and all you have to do is wipe the outside of it clean @ the end of the day.