Dispensing glue from a barrel

4/29/19       
Bill

For years we dispensed blue from a barrel by putting an elbow in the bung with a length of PVC pipe and rotating it down to let the glue flow. Then we would tip it back up and plug it. We changed glue vendors and the new glue seems to clump up towards the end of the barrel. We think it is drying and leaving a skin.

We recently tried a knife valve so we know we are getting a seal. We still have clumps and the valves sticks and does not seal well. Does anyone know a better way?

4/29/19       #2: Dispensing glue from a barrel ...
Mark B Member

My guess is the make up air thats coming into the barrel as you pour off over time is enough to create a large thick layer on the top just as if you were to leave that surface area of glue out on the bench. Would seem other than to use the glue faster, buy in smaller containers, you'd just have to deal with it, stir, mix, or perhaps invest in a small cylinder of Argon and periodically remove the small bung at the top of the barrel and feed a bunch of Argon into the drum to displace the air thats in contact with the glue.

Have a MIG welding setup in the shop and I will top off partial gallons/quarts of paints/finish, bottles of polyurethane glue that are going to sit for a while, of the mig tank and it works fine. My cylinder is a 75/25 Argon/CO2 mix and Id imagine straight argon would be best but I think Argon or some other inert is all thats in products like Bloxygen. Around here the small cylinders can be purchased outright (no lease) for around $100 bucks. Small regulator, and you could give it a try.

4/29/19       #3: Dispensing glue from a barrel ...
Bill

We have used glue in barrels for years and never had this problem even when we went through glue much more slowly. National Casein went out of business and forced us to change vendors.

Is there a better valve scenario?

4/29/19       #4: Dispensing glue from a barrel ...
Mark B Member

The knife style is the only other style Ive seen for viscous materials. I wonder when the glue companies will come to their senses and start selling bulk quantities of glue in large totes like box wine where the material is contained in a sealed bag that collapses as its used and the contents never see a molecule of air.

4/29/19       #5: Dispensing glue from a barrel ...
Bill

I agree.

4/30/19       #6: Dispensing glue from a barrel ...
Kirk

Buy a 35 dollar barrel pump from Harbor Freight.They work great for about a year or so. Then you throw it away and buy another one.

4/30/19       #7: Dispensing glue from a barrel ...
Mark Elliott Member

Mark B,

I agree as well with having the glue come in the sealed bag the way box wine comes. It just doesn't cost that much money and it sure does seem that that would give an adhesive suppler an advantage in the market place.

I made this post to try to build support for this idea just in case a supplier comes across this thread.

Mark

5/1/19       #8: Dispensing glue from a barrel ...
Chris H.

Website: https://www.csaw.com/lamello/

Bill, It does seem strange that you're having this problem now, but never with your other supplier.... I would have to say that it's got something to do with the chemical make-up of the new glue. You could check with Jeff or Eric at CP Adhesives - those guys know a LOT about glue and offer all kinds (even custom adhesives):

https://www.cpadhesives.com/

And Mark E., CP may already have your glue bladder idea in production, or if not, may be interested to hear about it.

One other option to consider is the LK glue systems from Lamello, designed for water-based glues. They're self-contained, pressurized, stainless steel tanks where the glue is always under pressure, right up to the pistol. I've had glue in my system for 3 months (with no use) in between trade shows, and the glue has been just fine. Lots of other advantages too, but that's the one the addresses your concern.

Lamello Glue Systems

5/1/19       #9: Dispensing glue from a barrel ...
Mark Elliott Member

Chris,

I already have 2 of them and they work great. It's the bulk glue we're talking about before it goes into the dispenser.

I address the problem by purchasing my glue in 1 gallon jugs and fill the tanks from those.

Mark

5/2/19       #10: Dispensing glue from a barrel ...
Bill

Chris we have several Jolly Colla's which is a similar glue dispensing system. We go through a lot of glue and a devise like that is not appropriate for many operations.

We considered breaking down 50 gallons into smaller containers but I am not sure that is the right answer over time.

I suggested the wine box thing to the vendor and he said he would look into it. I don't have high hopes.

5/2/19       #11: Dispensing glue from a barrel ...
Jeff Pitcher

Website: http://www.cpadhesives.com

Some years back we were very excited about a tote packaging system that was essentially what you described, a corrugated shell with a bag liner. They came unassembled and we less costly than bottle in cage totes. After two or three spills however, we decided they simply couldn't provide the necessary stability for the weight of the glue. We've also toyed with the wine box type dispenser. Ultimately, it's more expensive and very problematic to fill. Still something I'd like to pursue but haven't found a cost effective alternative to the old gallon jug. There are pumping systems available that will allow you to keep a drum upright and pump on demand. Let me know if you'd like more information.

5/2/19       #12: Dispensing glue from a barrel ...
Chris H.

Hi Mark,
Didn't realize that was you until now! Good to see you at the Charlotte show and glad to hear the LKs are working well for you!
Best,

9/28/20       #14: Dispensing glue from a barrel ...
Eric Burke Member

Website: http://cpadhesives.com

Coming to this thread a little late...

We do have 275 gallon totes with the bag in (plastic) box type system you mentioned. We do not currently have this for 55 gallon drums, though. Sorry.

Another thought is that the company drierite has a desiccant cartridge system for drum bungs that would at least help keep the air coming in dry (link included). It is more commonly used for reactive adhesives like polyurethanes, though.

You mentioned having to switch to another vendor. Is it possible that the shelf life on the replacement product is shorter than your prior adhesive?

Conversely, there are usually unfilled/filtered versions of the adhesive you use that are designed to be less likely to clump or clog up. They tend to be a little more expensive, but you may want to check if there is an alternative version of the adhesive you are using from your supplier.

Another option that is much more expensive than the harbor freight pump is the ez drum dock pump system that you would still be able to use to fill your Lamello LK tanks you have. The main trick to it is that the small bung remains closed and the special fittings for the large bung are self venting as needed and this works to help keep the adhesive more protected over time.

Just a few thoughts from the glue guys at CP/ Spectrum. Thanks

Drierite


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors
    • Vacuum Pressing Systems, Inc.
      Vacuum Pressing Equipment - Including Bag and Frame Systems
    • Supergrit Abrasives
      Industrial Quality Abrasives Manufactured by Leading US and Foreign Companies
    • CP Adhesives
      Supplying Quality Adhesives to the Woodworking Industry
    • Excel Dowel and Wood Products Inc.
      Plain and Pre-glued Dowel Pins, and Wood Parts - Servicing Small Hobby Shops to Large OEM's
    • Rangate
      Woodworking Machinery, Supplies and Knowledge
    • Veneer Systems Inc.
      Specializing in Veneer Equipment and Veneer Supplies
    • ULTI-BOARD
      The Ultimate Spoilboard - ULTI-BOARD - Specifically Engineered and Formulated for the Ultimate in Spoilboard Performance - Not Your Ordinary Sheet of MDF.

    Become a Sponsor today!