Architectural Woodworking

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: True Divided 60 Lite Sash

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

True Divided 60 Lite Sash

7/18/17       
Dave Member

Looking for some feedback on a project I just took on. Hopefully I can explain w/o pictures.

Single Fixed sash window. Sash roughly 4' tall x9' wide. Sash 1-3/4" thick.
Material is vg fir.
Traditional style sash with 1/4" rabbets, single pane glass.
Muntins 3/4" wide-
Mortise tenon joinery - 3/8" x 3/4" mortises for muntins in the flat of profile adjacent to interior of glass.
Grid: 4 rows by 15 columns, each opening roughly 6.5" x 10"

I believe I have the mechanics of how to do this worked out but still have a few questions as 18 lites is the biggest unit I have done to date.

Would it be better to have the three 3/4" wide rails run the full length or have the vertical muntins run top to bottom rail? Why?

I have typically glued my sash with titebond 3. There is no way I'll have enough open time to do that. If the joinery is tight do I even need to glue this up?- it's fixed sash- where's it going to go and the glazing bed should provided the necessary seal. Any ideas on this greatly appreciated.
Thanks
Dave

7/18/17       #2: True Divided 60 Lite Sash ...
Harold Pomeroy

Make all the vertical muntins full length, through tenons.
The horizontal muntins will need to vary in length to close any gaps in the middle rows. The middle row muntins will need to be sever hundredths longer than the top and bottom row muntins.

Don't glue the muntins, to allow for fitting after assembly. To fit after assembly, clamp along the rails. In the middle, spread the stiles with a sash stile spreader. It's shaped like an "H". put a clamp across the top of the "H", and the bottom of the "H" goes in the stile rabbets. you can open the stiles 1/2", allowing you to replace muntins as needed to get the right length muntins in.

If you only glue the stiles, you will have plenty of time for assembly with Titebond III.

Don't tell anyone about the sash spreader, it's a trade secret.

Harold

7/18/17       #3: True Divided 60 Lite Sash ...
David R Sochar Member

I also would advise to run the verticals the full height, with the horizontals coped and tenoned in place. The stiles at the side can also be run full length - same length/cope/tenon - as the vertical muntins, unless that would a be problem for someone, traditionally.
Now, the sash spreader is a new one for me. And it sort of makes sense, but I would not start making some mutts longer than others. I learned (trade secret) to intentionally crown the stiles so that the opening without mutts is narrower at the center that at the ends. This will provide tension to all your horizontals as they go in. At 6.5' tall, I would crown the stiles about e/8" to 3/4" each.
I would use TBII or even a slow set epoxy for assembly. The epoxy will give you the time you need. Glue the copes lightly and the tenons with a bit more glue. Use spacers to keep you spacing and alignment. The tension from the crown will be enough to 'clamp' the epoxy copes since you do not want a lot of pressure.

Even though some old guy would not have glued much in an older sash, you have the opportunity to improve on the old guy's work but using epoxy as a sealant. He may have put some white lead into the joints, and said 'good enough!' He also did not have much in the way of glue to choose from.

If this is painted or stained a dark color and then get direct sun in service, the TBIII is prone to failure with a serious loss of strength at even 175 degrees.

7/18/17       #4: True Divided 60 Lite Sash ...
rich c.

I'd consult a structural engineer on this one. Depending on the location of the window. and your state, you could very easily have a wind load issue with this one. Might even be against code in tornado or hurricane country. Unless there is some historical district override, you may have to build multiple units for strength.

7/18/17       #5: True Divided 60 Lite Sash ...
Dave Member

The spreader is also new to me. I've been looking all over for one with no luck yet. Harold: would you be interested in doing this project for me- I bid $1600, would think that leaves plenty of cushion.

Kidding aside, thank you all for the tips. Running verticals full length makes more sense structurally. Just not thrilled about machining the 6-1/2" muntins.TB3 temperature sensitivity is news to me. Have not had any failures to date but certainly something to keep in mind for future.

Why use spacers? If the verticals and stiles are all mortised at same measurements that will register everything without spacers or measurement during assembly.

Thanks
Dave

7/18/17       #6: True Divided 60 Lite Sash ...
Harold Pomeroy

The sash spreader was invented out of need. When building sash, sometimes a muntin gets broken, or muntins are too short. Being able to remove and replace muntins has saved some jobs. It works on French doors, and old sash, too. You may wonder why someone working in a shop would keep on putting sash together if the muntins were too short. However, consider the most screwed up thing you have ever seen an employee do.

Another way to deal with the flex in a big sash is to put a groove in a row of horizontal muntins, and run a stainless steel cable across the sash, under the putty. It's a lot like the way pre-stressed concrete is made. The cable goes through the stiles. Anchor it at one end, and run it around the end of the hole and down to a screw at the adjustment end. It would be interesting ti get an engineer's opinion on the wind load viability of a cable reinforced sash. The biggest reinforced sash I have made was only six feet wide, and was a storm window.

7/19/17       #7: True Divided 60 Lite Sash ...
David R Sochar Member

The cable is a good idea. I have run a kerf in the assembled sash 1/8 x 3/8" deep and splined it the full length or width as needed. Sure does help keep things in place.

I learned in a shop that rarely tenoned short muntins (mutts as they called them). They would use a tight cope for placement and location. Gluing the end was hit or miss - no rules.

I like a tight cope still today, and often omit a tenon on short muntins - usually verticals. Our normal today is 9/16" or wider rabbets, with the tight cope and stick, 1/2" to 3/4" insulated glass in RTV silicone and wood stops, also with the RTV. This makes a rock solid, stiff unit, so the tenons are not missed.

A large sash as the OP is faced with does not get much strength from the glass and putty. I'd use epoxy on every joint, buttering the copes as you go. Yep, 1600 ought to do it, with money left over for new truck.

The photos are of a large sash with long verticals and short horizontals to facilitate the radius. The horizontals were not tenoned, but were coped nicely. The vertical are tenoned as well as coped. We used spacers to locate the mutts, then set the glass and mitered the stops with RTV both sides. Once it was cured, it had almost no ability to twist - it was rigid. The dry fit photo has the straps on it to hold the verticals in place. We had two of these, both just a hair too big to fit out the shop doors.


View higher quality, full size image (1800 X 1350)


View higher quality, full size image (1800 X 1350)

7/19/17       #8: True Divided 60 Lite Sash ...
Sam

David

Couldn't help but notice in the picture
of the porch ... that's a funky looking
beam support arrangement that the
porch rafters sit on .... any back story
to that?

Sam

7/19/17       #10: True Divided 60 Lite Sash ...
David R Sochar Member

Sam - Yes, it is true that I am not a framer. Adequate, but not proficient.

That arrangement came about because I wanted a thin beam to span from post to post - did not want it be low enough to be in my field of view. Also, I wanted a certain angle of drop to the porch roof. Being OCD about such things does not always make for logical pathways.

I moved the beam back off the post tops to where is was half on (or half off), helping preserve the angle by some fraction or another. The beam - two 2x6 and some 3/4" ply - is heavily nailed at the point where is is on the half laps on top of the posts. The rafters are deeply notched.

The odd part is that I built the shop as a hobby shop before quitting my last real job, running a 12 man shop for a full service wholesale lumberyard. No one there - estimators, draftsman, salesmen - could tell me what I needed to span the 12' distance. They asked what I planned and said it ought to work. It does work fine, even with a good snow load.

You may notice the Summer Office - porch swing and rocker - is open in this picture. The porch has come in handy for everything from assembly, to lumber storage, to weddings.


View higher quality, full size image (1800 X 1350)

9/8/17       #11: True Divided 60 Lite Sash ...
Steve

I know I'm late to the table on this but if Dave is still opinion searching, I would offer this.

As David Sochar has stated, a tight cope with no tenon has served me well on several odd sash that I have made. There was a machine that was specifically designed for that purpose in the early part of the 20th century.

I also strongly recommend epoxy glue or at least using an epoxy sealer on all copes, tenons and indeed the entire fabrication. Paint fails where water gets in an that is always at the cut ends or copes. I wouldn't build anything of this nature without the epoxy sealer. Vertical full length munts is the proper approach.

9/9/17       #12: True Divided 60 Lite Sash ...
Dave

Steve- thanks for the advice. I'm in process of doing a dry fit of the mutts this weekend- this isn't my day job.
I did take both David's and Harold's advice (thanks you ) and ran the full length muntins vertical. The stiles and rails are haunched mortise and tenon and the verticals were full tenons. I had a buddy help me glue up the rails and verticals with TB3.

I do plan on epoxying in the mutts. Had a bit more trouble machining these 6.5" parts than I anticipated but finally got it. I think having the longer tenons on these part would have made it easier.

As far as epoxy sealing entire unit would you go with Smith's or West Systems?
Will try to post pics at some point.

9/9/17       #13: True Divided 60 Lite Sash ...
Steve

I use both Smith and West system. Smith's is deeper penetrating, I believe. Of course it depends on the wood you are using. If you have a very light profile then the Smiths will not build up and crowd the detail.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)