Stave core vs. 10/4 -- 0 -- 
2/23

Say you were making 24 interior doors 7'8" tall, 1 3/4" thick, sapele. 8/4 doesn't work, too thin. Which would you do?
2/23 #2: Stave core vs. 10/4 ...

I use 8/4 to make 1 3/4" doors. Why doesn't it work? To wavy?
Stave core is the way to go for stability if you can manage to make or get them for a reasonable price. One or two doors it's probably going to be to expensive.
But then again, a failed door is pretty expensive all by itself.
2/24 #3: Stave core vs. 10/4 ...

We recently used Carolina Engineered Wood Components to supply engineered stiles for a large interior door job and were happy with the product, and felt they were quite reasonable. The staff is very knowledgeable and flexible, as well - willing to tailor the product for special requirements.
I don't think there is any question that an engineered product of this sort is superior to a solid stile.
2/24 #4: Stave core vs. 10/4 ...

(24) doors
7' 8" doors
That much sapele doors
3 good reasons not to use solid wood
As Leo mentioned if you were going to make a smaller number(4 or less) it would be reasonable to laminate.
You might make more money by outsourcing. That is a fair amount of milling(72 sticks for every part) and gluing.
2/25 #5: Stave core vs. 10/4 ...

Website: http://kdunphy.com
I think first you have to ask your self why is the client hiring me .
Laminate is a huge amount of time i see that you can buy laminated lumber which saves time and money
Then let me get this straight you make the door with laminated lumber then you veneer [I assume you have a press ]
8/4 you can easily get 1 3/4 thick ( long door like that I would want 2 1/4 thick)
I have not done only because in are area no one willing to pay .We do a far amount of exterior doors I have none that have warped .
92 in tall door will take a lot of skill to hang
Read David post on doors there more information than most books .
If I was hiring a shop I would want solid doors
pic of door we done last pic of a 175 year old door from Montreal
View higher quality, full size image (5312 X 2988)
View higher quality, full size image (5312 X 2988)
View higher quality, full size image (470 X 626)
2/25 #6: Stave core vs. 10/4 ...

Laminated refers to 3 pieces of timber glued together to achieve a stable thicker timber. (24) doors x 3 pieces = 72 pieces of wood for every part(stiles & bot/lock/top rails). That is a ton of milling gluing & sapele.
Laminated core typically refers to a lower quality of the same or less costly species of wood laminated together then thick veneered.
Engineered core refers to lvl or parallam door specific(not the stuff from the lumber yard) which is then thick veneered.
I would go with a engineered core for your project. Based upon number of doors, species of wood, and height of the doors.
2/26 #7: Stave core vs. 10/4 ...

To me, the inappropriately named "engineered core" (there is no engineering involved in the process whatsoever) is an assembly of solid wood rips glued to make up the stiles in width (not thickness). This assembly will have exposed hardwood edges that will show after the face laminations are applied. The core parts might be quartered, flat or indeterminate, as oriented to the face.
If you have a good lumber source, 8/4 in the rough should easily make your 1-3/4" product. S2S will be too thin to joint and still get the thickness you need. I have never used 10/4 to make a 1-3/4" door.
Which is cheaper? Labor or wood? Cored stiles (and rails and panels?) will have 2-3 times the labor in each part. Solid stiles are much faster. 8 hrs for a simple door in solids, vs 20 hrs for assembled stiles and rails.
Our labor is based upon the idea that the trees are growing, and there are more today than yesterday. But our time is gone once it is gone. So time is more valuable to us, and we will make from solids whenever possible.
Out of thousands of interior doors with solid stiles, I have had 3 warp enough to warrant replacement. Two had wet wood, and one was reaction wood.
2/26 #8: Stave core vs. 10/4 ...

When I'm doing solid stiles I process them slowly. Flatten one side and plane it and let it sit over night to see what it does. Do that again and again until you get to the proper thickness. See if it's stable before you put the door together.
Hard to do if you got a ton of doors to make. But if it's one or two then you don't ever have to worry about movement.
2/26 #9: Stave core vs. 10/4 ...

Kevin,
Where is this David’s post that you mentioned? Thanks
2/26 #10: Stave core vs. 10/4 ...

Website: http://www.acornwoodworks.com
One more thing about solid doors vs most other methods.
The door craft for about 100 years or more crowned the latch stile to hold the latch in tension when closed. This gave a better seal and prevented rattles. A good shop will still do this today if they pre-hang. If they don't, they may still mark the door for a crown so the carpenter that is hanging the door will know which face goes where.
Try to get your outsourced materials with a 3/16" crown in half the stiles. Or, try to do it when you are laminating for thickness, veneers or whatever. But, in solids, it is relatively easy to do at the joiner.
Then, in a few months when you visit the job for some photos, you can point out this detail to the owners and the builder and show them how the door snaps shut, while being tight top and bottom.
Most people that make a living from making doors today know nothing of this simple point of craft. It makes me wonder what else has been lost as one 'method' supplants another.
2/26 #11: Stave core vs. 10/4 ...

Scott just type in his name he's all ready answered on this thread .The big question I have while I have David's ear [ I don't want to hijack] any pic or words of wisdom on through mortise and tendon
The weather here is brutal compare to my snow challenged friend from the south
2/26 #12: Stave core vs. 10/4 ...

No need to through mortise. A deep blind mortise is more than enough. Back in the day they would do a mortise and then pin the door, and they are still together today. I feel that a through mortise just allows moisture to get inside the door easier.
2/26 #13: Stave core vs. 10/4 ...

The thru mortise with wedges is a UK method. The stopped mortise with pins is a US method.
Those methods are all dry. No glue. Some reproduction shops still do it and glue. More of an aesthetic.
Our threshold's are also the opposite. As well as riser/tread fastening in stairs.
2/26 #14: Stave core vs. 10/4 ...

David,
I agree in general with your comments about solid vs not-engineered. In the original posters case. I thought it would be more economical for him to outsource these to a shop that is tooled up for not-engineered work. He's effectively outsourced a large chunk of risk and created a fixed price as part of his overall estimate.
I've never bought 8/4 sapele. No idea on cost, or stability. I love the look and workability.
2/27 #15: Stave core vs. 10/4 ...

Through wedged tenons were used in the US also. A lot of mass produced doors were made this way in the late 1800s and early 1900s. With a chain mortiser it is quick.
I would never intentionally build a crown into a stile. I find that whatever method we build with- solid, stave core or laminated there is always a slight crown. Always good practice to crown your stiles, even on cabinet doors.
3/1 #16: Stave core vs. 10/4 ...

Save yourself a lot of frustration and outsource some "non-engineered" engineered components. Works awesome for us mere mortals (hacks to some), you'll have straight doors, consistent faces, and you can make some money. It works and is preferred for 99.9% of door manufactures across all market segments, it'll surely work for you.
And just to ease your mind a little on the use of "non solid" components, it has been a staple of door building for easily over a century.
3/4 #17: Stave core vs. 10/4 ...

We no longer make doors because we can buy nicely made doors cheaper than we can make them. We have rarely done residential work, so when we made doors they were always to some specification. Where architectural match was required they were always veneer staved. Other wise it depended on the finish but mostly solid because it is cheaper by far. Exterior doors were always stave, with back to back panels and a plastic separator, because of our extreme climate.
3/5 #18: Stave core vs. 10/4 ...

Thank you for all the informed responses, I appreciate it.
Jeff
3/8 #19: Stave core vs. 10/4 ...

I think part of it depends on the wood and I'm not sure I'd consider sapele all that stable? I've only used it once and found it moved all over the place, so personally I wouldn't use solid for a tall door like that.
I've made a bunch of doors from solid with good results, and then for a short while tried the 3 piece glue up. These days most of my doors are stave core but I'm making the cores. I use the same material for the cores as the faces, just re-saw all my skins from the best stock and mill the remainder into strips to glue up the cores. Mill those flat and then glue on the skins. A LOT more work than just making out of solid, but they are stable as heck.
just my opinions though, good luck!
JeffD
0 -- 
Buy & Sell Exchanges | Forums | Galleries | Other Resources | Site Map
Buy and Sell Exchanges
Job Opportunities and Services Exchange
Employment opportunities and services within the woodworking industry
Lumber Exchange
A worldwide buy/sell exchange for lumber and wood products
Machinery Exchange
A worldwide buyer and seller exchange for woodworking machinery and equipment.
Classified Ad Exchange
Classified advertising for the woodworking industry (for advertisements that do not include machinery, lumber products and employment listings)
Forums
Adhesives Forum
Discussing topics related to adhesives within the woodworking industry
Architectural Woodworking Forum
Discussing quality standards and production of architectural wood products
Business and Management Forum
A forum for the discussion of business topics: from sales and marketing to dealing with difficult customers.
Cabinet and Millwork Installation Forum
Discussing all aspects of installation issues encountered by cabinet and millwork installers.
Cabinetmaking Forum
Discussing 32mm and face frame cabinet construction including fabrication, casegoods design, and installation.
CAD Forum
Shedding light on the all-too-often shadowy world of CAD.
CNC Forum
Discussing CNC (computer numerically controlled) woodworking equipment, software, and automated product manufacturing.
Dust Collection, Safety and Plant Operation Forum
Discussing topics related to maintaining a safe and productive working environment.
Professional Finishing Forum
Finishing issues for the production environment
Forestry Forum
The science and art of forest cultivation and timber management, planting, surveying, tree diseases, silviculture and timber harvesting
Professional Furniture Making Forum
Helping professional furniture makers improve quality, save time, and increase profits
Laminating and Solid Surfacing Forum
Issues related to laminating and solid surface materials and processes
Commercial Kiln Drying Forum
Discussions covering issues faced be commercial drying operations that process at least 750,000 bd. ft. of lumber per year
Sawing and Drying Forum
Discussing topics related to primary processing and drying of lumber
Solid Wood Machining Forum
Discussing topics related to the machining of solid wood
Value Added Wood Products Forum
Learn how to improve your output, find new markets, and boost sales of your lumber products
Veneer Forum
Discussing topics related to veneer processing, manufacturing, and fabrication
WOODnetWORK
An electronic discussion group for woodworkers throughout the world
Galleries
Project Gallery
Where professional woodworkers can post examples of their work
Sawmill Gallery
Professional primary processing companies display and describe their sawmill facilities
Shop Gallery
Professional woodworkers display and describe their shop facilities, products and equipment
Shopbuilt Equipment Gallery
Professional woodworker's jigs, rigs, and shopbuilt equipment
Other Resources
Industry News
Late-breaking news from all sectors of the wood industry
Video Library
Index of industrial woodworking related digital videos on the web
Auctions, Sales and Special Offers
Advertisers offering woodworkers discounted prices on good and services, and announcements of upcoming auctions
FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)
WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
A valid email return address must be included with each message.
Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
Subject lines may be edited for length and clarity.
"Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
(return to top).
Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.
You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.
WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.
Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).
Libel: Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.
Improper Decorum: Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).
Advertising: The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).
Repeated Forum Abuse:
Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.
There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).
The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)
Forum Posting Form Guidelines
|
Your Name
|
The name you enter in this field will be the name that appears with your post or response (return to form).
|
Your Website
|
Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
|
E-Mail Address
|
Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
|
Subject
|
Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
|
Thread Related Link and Image Guidelines
|
Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
|
Thread Related File Uploads
|
Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .FLV .MP4 (Image Upload Tips) If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
|
|
|
|