Is high end work dying? -- 1 -- 
8/25

I have been in the high end of the millworker niche for the last 15 years. My small company makes money but I am not getting rich by any means. Increasingly, I see that the high end contractors I've always worked with are skipping the cabinetmaker and using their trim carpenters to make on site cabinetry using MDF. The on site painter then finishes it up. My cost of finishing (which I sub out) is admittedly ridiculous. Some of the designers I work with are now targeting the higher volume, low end market because the profit margin for their portion of the work is much higher. All the condos I see going up are cheap to say the least. So is the quality, high end market disappearing?
8/26 #2: Is high end work dying? ...

I won't pretend I know, but I don't think so. I'm working on a $3m home right now through a developer. My cabinetry is closer to high end and not inexpensive, but I'm only doing an office and a vanity. Basically providing a little WOW factor with some stained rift white oak cabinetry to contrast a lot of painted millwork.
I was honestly surprised at how much mdf site-built cabinetry there was in this home! I didn't think that stuff would fly in this price range? I guess once it's painted it will look good enough in the short term. But I don't think if it was the owner of a home it would fly.
Condos and townhouses around this area don't usually get much high end cabinetry at all when built. It's the owners that fix them up later who will spend a little money. I'd say roughly half of my work is in condo's in the city. Figuring starting prices are close to the $1m range, plus staggering condo fees, and parking spots $60k and up……there are still plenty of people with expendable income! The trick is finding the ones who appreciate quality and craftsmanship.
good luck,
JeffD
8/26 #3: Is high end work dying? ...

I think folks like you and I have been asking that question for about 2,000 years or more. We look around, see a change, and extend it out, and predict a dire future. While there is plenty to agree with - that it is dying - there are exceptions.
First, 'high-end' is a subjective, relative term. What is 'high' to me may not be to the next guy. Just as climbing a mountain peak gives the reward of standing on the top of that peak, it also offers a view of all the other, higher peaks that you have not scaled. I think that almost any shop along a spectrum - from low end to true high end can ask the same question you ask, as they see their price (relative price) stand as too 'high' in the context of the competition. We all can say that the customer is deteriorating.
As the niche you work within becomes (apparently) smaller, you do become more valuable. At times it seems like you are merely endangered, but look at it in context. For the person that wants hardwood frame and panel case work or general better quality, but can only find MDF disposa-wod, you become a rare commodity. I hear it all the time: "I didn't think anyone knew how to do this anymore..."
Now, everyone appreciates craft, knows to look for dovetails, etc. But the pressure to find 'value' (whatever that is?) makes people think they can't afford the things they want. It also makes for vinyl drawer sides with printed dovetails. Add in the fact that many of my younger customers have never seen nice architectural work or lived with good design, and it is an uphill battle all the way. They will buy a new table every 2-3 years, instead of having one nice table made that will cost less in the long run, and give them the pleasure of uniquely good design, and great materials, as well as good service and retained value.
A positive is that it doesn't take too much work to keep your small shop busy - relatively speaking, yet again. When I first hit 50k a year, I thought I had saturated the market. Where could I find more work? At 1.1m, I think I did hit the market saturation, and was moving beyond my own area to grow further. Again, all relative.
Your job - and mine - is to find the people that want good work, authentic woodwork, competent joinery and design, and connect to them. As the Wal-Marting of America continues to drive prices down and bring ever worse materials up, we need to step aside and consciously not take part in that fruitless (for us) pursuit. How we find 'our kind of people' is the problem, and one I confess to not having an easy solution to.....
8/26 #4: Is high end work dying? ...

We do high end furniture both wood and frame up upholstered. We were dead all summer and now we are buried up to our eyeballs. There are plenty of wealthy clients for our interior designers and I am finding fewer that want to beat me up for lower pricing. I would have agreed with you last week but we got $250000 in furniture orders since Monday. :-) Hang in there.
8/26 #5: Is high end work dying? ...

Worked for a client that built a million dollar plus house. Made 3 vanities for them. When we got there to install that's what we saw. MDF built ins. 5 piece doors made from all MDF, who would want to subject their cutters to that?
FJ molding, cheap pine, and MDF. Cover it with some primer and paint and I guess that's what goes into a million dollar home.
The kitchen cabinets were lackluster and on of the stained set of cabinets was just horrible.
My cabinets were the best cabinetry in the house. FYI, I'm doing more work for them. I'm sure they noticed the quality difference between what they got and what I could give them.
High end work is spotty and comes and goes. Right now my work load is up. Lets hope it continues.
8/27 #6: Is high end work dying? ...

Side by side comparison will make better work stand out. But by then, it is a bit too late. Leo's customer with the FJ moldings and the MDF is learning, and will benefit from the association with Leo. But I will bet he had no idea his house had the same materials as the vinyl village down the road. Most of my customers that only get a few doors from us honestly think all their other doors are wood when they are hardboard or MDF. No one ever told them differently, and when they ask their builder about it, they are told that the 'near' doors they have are all they can afford. In a 2.4m house.
I see it as a problem of specifications.
Lack of, or there is such a common downgrading that even the $3m Personal Monuments have crappy woodwork. This allows more square footage, which is the cash cow for the General and most trades.
Perhaps you have worked a commercial job where 'specs' are covered in a small book (tho it is often lawyer-speak boilerplate), with those specs meant to give an adequate description of what is needed so bids are all apples to apples.
You will never see specs for a residential job, much less anyone that checks after the delivery, so I think you should write your own specs, and make it known that XYZ is how you propose to do the work, and then let them know that if they would like a bid with different specs, you would be more than able to do so, once those specs were supplied. You could even add a bit of why you build to such and such specs - tighter joints, less finish problems, more solid boxes, etc. Show some samples if you have the choice.
With the entire world moving towards everything made from some sort of printed cardboard, it is very easy to write specs and make a sample or two that stand out from all the crap.
8/27 #7: Is high end work dying? ...

It's funny, I've read countless other threads where mdf moldings are touted as superior to solid wood for their stability, paintability, and sustainability. Also as substrates for veneers in frameless cabinetry for the same reasons.
The site built aspect is interesting; in some regions it was common traditionally for cabinets to be built on site by experienced carpenters/joiners. I've actually worked on a trim/cabinet. crew that did just that and the owner took great pride in his work and woodworking expertise.
8/27 #8: Is high end work dying? ...

We will never run out of people with more money than brains.
8/28 #9: Is high end work dying? ...

"...more money than brains" I hope you are right. There might also be some that do have brains, and also money. Then there is luck (lottery) or inheritance. Lots of reasons why someone has a lot of money to spend.
I used to agonize over some of my proposal that were in the tens of thousands of dollars - more than the first house I bought. I'd sleep on it, reduce it a few percent, rework numbers, tighten waste factors, etc.
Then one day, I was talking to a young couple about a 40k project. I was sweating, trying to justify the expense for what would be a knock out room. He was hesitant, and I was thinking about backing down a bit on the price. Finally she spoke up and said "You know, that is really just a good morning on the Market". She explained that he made that much more than once in the last couple of weeks. He agreed once he saw it in that context, and went with it. They were delighted and never mentioned the price again except that it was easily worth it.
That $40k was like $150 to me - significant, but not monumental.
Remember, almost no one needs what we make, they buy because they want it. Everyone "needs" a car, but some pay $10k and some pay $100k, and some even pay 5 or 10 times more. They will all do the job of transport, so why the additional expense? Because they want it.
9/2 #10: Is high end work dying? ...

We are commercial only and have been seeing more higher dollar work. We are in the middle of a dental clinic with lots of curved maple moldings and casework. Just finished a bank that was mostly curves. I think curves add a lot of style and of course price. It eliminates some shops from the bidding also, that's always good, for us.
Site built MDF cabinets, painted! YUK. But can look OK, for a little while.
1 -- 
Buy & Sell Exchanges | Forums | Galleries | Other Resources | Site Map
Buy and Sell Exchanges
Job Opportunities and Services Exchange
Employment opportunities and services within the woodworking industry
Lumber Exchange
A worldwide buy/sell exchange for lumber and wood products
Machinery Exchange
A worldwide buyer and seller exchange for woodworking machinery and equipment.
Classified Ad Exchange
Classified advertising for the woodworking industry (for advertisements that do not include machinery, lumber products and employment listings)
Forums
Adhesives Forum
Discussing topics related to adhesives within the woodworking industry
Architectural Woodworking Forum
Discussing quality standards and production of architectural wood products
Business and Management Forum
A forum for the discussion of business topics: from sales and marketing to dealing with difficult customers.
Cabinet and Millwork Installation Forum
Discussing all aspects of installation issues encountered by cabinet and millwork installers.
Cabinetmaking Forum
Discussing 32mm and face frame cabinet construction including fabrication, casegoods design, and installation.
CAD Forum
Shedding light on the all-too-often shadowy world of CAD.
CNC Forum
Discussing CNC (computer numerically controlled) woodworking equipment, software, and automated product manufacturing.
Dust Collection, Safety and Plant Operation Forum
Discussing topics related to maintaining a safe and productive working environment.
Professional Finishing Forum
Finishing issues for the production environment
Forestry Forum
The science and art of forest cultivation and timber management, planting, surveying, tree diseases, silviculture and timber harvesting
Professional Furniture Making Forum
Helping professional furniture makers improve quality, save time, and increase profits
Laminating and Solid Surfacing Forum
Issues related to laminating and solid surface materials and processes
Commercial Kiln Drying Forum
Discussions covering issues faced be commercial drying operations that process at least 750,000 bd. ft. of lumber per year
Sawing and Drying Forum
Discussing topics related to primary processing and drying of lumber
Solid Wood Machining Forum
Discussing topics related to the machining of solid wood
Value Added Wood Products Forum
Learn how to improve your output, find new markets, and boost sales of your lumber products
Veneer Forum
Discussing topics related to veneer processing, manufacturing, and fabrication
WOODnetWORK
An electronic discussion group for woodworkers throughout the world
Galleries
Project Gallery
Where professional woodworkers can post examples of their work
Sawmill Gallery
Professional primary processing companies display and describe their sawmill facilities
Shop Gallery
Professional woodworkers display and describe their shop facilities, products and equipment
Shopbuilt Equipment Gallery
Professional woodworker's jigs, rigs, and shopbuilt equipment
Other Resources
Industry News
Late-breaking news from all sectors of the wood industry
Video Library
Index of industrial woodworking related digital videos on the web
Auctions, Sales and Special Offers
Advertisers offering woodworkers discounted prices on good and services, and announcements of upcoming auctions
FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)
WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
A valid email return address must be included with each message.
Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
Subject lines may be edited for length and clarity.
"Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
(return to top).
Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.
You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.
WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.
Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).
Libel: Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.
Improper Decorum: Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).
Advertising: The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).
Repeated Forum Abuse:
Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.
There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).
The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)
Forum Posting Form Guidelines
|
Your Name
|
The name you enter in this field will be the name that appears with your post or response (return to form).
|
Your Website
|
Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
|
E-Mail Address
|
Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
|
Subject
|
Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
|
Thread Related Link and Image Guidelines
|
Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
|
Thread Related File Uploads
|
Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .FLV .MP4 (Image Upload Tips) If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
|
|
|
|