Safety Speed Cut Thermwood Corporation ECabinet Systems

Cabinetmaking

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Wood movement-doors

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Wood movement-doors

4/1/15       
Russ Member

This is from a previous post, any advice would be great. A customer requested some folding closet doors, 3" wide styles/rails, flat panel, 2 panel doors per side 84" in height. total opening is about 7 feet. The doors will be painted white, frames will be poplar, and interior panel 1/2" MDF. Because of the vertical length of each door, Im concerned about the frames twisting a bit, is MDF the best choice for the panels and should I consider another species for the frames? Thanks.


View higher quality, full size image (519 X 433)

4/1/15       #2: Wood movement-doors ...
door shop guy

I make closet doors like that 1 1/8" thick

4/2/15       #3: Wood movement-doors ...
Russ

I was thinking 1" thick frame, but I can see going a bit thicker. If I use 1/2" MDF panel does weight become an issue for the outer panel sagging with time? My hardware supplier (Charles McMurray) only seems to have brass items in stock, any other reasonably priced supplier out there with satin finish hardware? Thanks.

4/2/15       #5: Wood movement-doors ...
David R Sochar Member

These are passage size doors, and the low end of the standards for that are 1-3/8" in the US, and the upper end suggests 1-3/4" thickness as a good door.

Use good wood, get it to rough length and ripped and let it acclimate in your properly heated/cooled shop for a few days, then joint straight and square before planing. Match your crowned stiles, and keep all your joints perfectly square at every step. As much as I hate MDF, it is good for flat, inexpensive panels.

Most small shop made doors do not 'warp' from wood movement as much as they deviate from flat - induced by non-jointed lumber, out of level or out of square joints, or other seemingly minor defects that have to do with joint mis-alignment.

Keep in mind that wood moves only in response to changes in moisture content.

4/2/15       #6: Wood movement-doors ...
Geoff

One inch stiles on a seven foot door??? Like David said, 1 3/4" thick stile and rail, 1/2" panel. If you are worried about the doors staying flat...

4/2/15       #7: Wood movement-doors ...
Mike Fuson

I think 1/2" mdf is over kill and to much weight. The thicker stiles and rails is a good idea, but I would go with 1/4" mdf.

4/3/15       #8: Wood movement-doors ...
Bill

Are you going to dowel the joints? Gravity is a bitch over time.

4/4/15       #9: Wood movement-doors ...
Geoff

If I was making those doors and they had a raised panel, the panel would be 1 1/4" mdf.

4/4/15       #10: Wood movement-doors ...
Larry

I'm not a fan of poplar for paint grade, Red maple paints much better. 1" is too thin like others have said. 1/2" MDF will be heavy! if you don't like 1/4" compromise @ 3/8".

4/4/15       #11: Wood movement-doors ...
Craig Gardner

Website: http://gardnerinteriors.com

You can always use ultra lite MDF, We use it all the time in our raised panel paint grade doors.

4/6/15       #12: Wood movement-doors ...
Russ

Thanks so much for the feedback. I'll go with the 1-3/8" thick doors and 3/8" mdf for the flat panels. I've used paint grade maple before too, I agree that the maple would be a much nicer finish.

4/14/15       #13: Wood movement-doors ...
GeneWengert-WoodDoc

David has already said the key points. I would add that the density of MDF is a key to its properties...strength especially. The lower the density, the greater the problem of fastening securely with screws, staples, nails and even glue. I would think that for a door, the low density material would not provide long service life.

4/15/15       #14: Wood movement-doors ...
antonio

Website: http://positivewoodworks.com

I think you are on the right track. The way i have done something like this in the past was: We would use soft maple @ 1 3/8" thick with a 1/4" mdf panel. Then, on the back of the door only we used 3/4" thick rails that were only seen when you opened the door. the client didnt want those rails to be seen from the front. This alone added great stability.

4/20/15       #15: Wood movement-doors ...
russ Member

Thanks Antonio, I like that option too.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Limtech Industries, Inc. Lamello