Safety Speed Cut Thermwood Corporation ECabinet Systems

Cabinetmaking

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Material for picnic table

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Material for picnic table

4/5/15       
picnictablebuilder

Need to make picnic table for a customer. First species that comes to mind is redwood 2 x 4s.

Any other species that would do this?

4/5/15       #2: Material for picnic table ...
Mike Fuson

The cheapest of the cheap would be treated. Cedar and Teak would be other options.

4/6/15       #3: Material for picnic table ...
rich c.

Redwood isn't what it used to be. Anything with sapwood rots just as fast as douglas fir. White oak works well. Personally, I would not want to eat off treated lumber. Also consider powder coated steel base if they want a longer term piece.

4/14/15       #4: Material for picnic table ...
GeneWengert-WoodDoc

If you use treated wood, rinse off the surface of the table to remove any excess chemical. Also, the sawdust and debris must be disposed of properly and the sawdust must not be breathed, must be washed off of clothes and skin, etc. is the surface now safe to eat off of...a kid drops a hot dog on the table for a minute, etc.? I would think not, but do not know of reliable technical info about this.

Now, redwood is probably too soft for a table and seat. And remember that there are chemicals (fungicides) in wood that make wood decay resistant. Are these natural chemicals safer than what we put in the wood when we treat? Plus, many species weather quickly to a grey color, due to aging of the wood and mildew. A finish or waterproofing has some chemical concerns too. So, maybe we need a table cloth? In any case, I would use in treated wood like eastern white pine and plan to replace the wood in 10 years or so. Watch for decay around the fasteners and brackets. I wonder of wood composite products would be stiff and strong enuf and safe?

4/14/15       #5: Material for picnic table ...
Kevin Jenness

Gene, what about torrified wood? It has been around long enough now that you must have some experience with it.

4/14/15       #6: Material for picnic table ...
Gene Wengert-WoodDoc

When wood as it comes from the tree is not exactly what we want, we modify it. Modification includes things like drying, sawing, gluing and so on. Further, there were some old processes for modifying wood (and a few new ones too) that changed the properties. We have wood that has acetic acid added (Accoya-TM), wood that is heated (torrified; Masonite is a heated product), wood that has chemicals added such as polyethylene glycol (PEG), monomers of styrene or other simple chemical that form a polymer within the wood (example is the hard wood-plastic knife handles), and wood that has various wood preservatives added to prevent rot (decay). Sometimes we add water repellants. Cement and wood are combined (HardiBoard-TM), and sometimes metal and wood are laminated or combined. And sometimes various wood species are combined (for example, plywood or laminated veneer lumber [LVL]). Certainly, there are other marriages of chemicals and materials.

Wood for years ago had natural decay resistance that is better than the wood grown and harvested today. Trees were larger and older, providing different material. Oftentimes, the structural use of wood was not considered to be for centuries, but rather for decades or even less (for example, log cabins were usually temporary, or short term, housing). So, today, the consumer demands have changed. (Example: I am changing four windows in my home that have rotted after 23 years.) Finally, I have seen architects and designers using wood and wood products in situations were other, wood or non-wood products could perform better (such as for house siding).

The bottom line is that if you can define the properties that you want in wood, there is a wood species or wood product that can furnish those properties.

Terrified wood is indeed one of those special products that has different properties and that may be a good substitute for "natural" wood.

4/15/15       #7: Material for picnic table ...
Kevin Jenness

"terrified wood"- I like it already.

My limited research tells me that terrified wood has had the s--t scared out of it, has lower strength properties, produces fine dust, glues poorly and is said by the sellers not to rot or move around. Accoya sounds somewhat more attractive as a possibility for painted exterior millwork (can we get a balsamic vinegar odor as an upgrade?). I am going to ask for a sample from the regional supplier, but I would like to hear more from folks who have a history of using it.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Limtech Industries, Inc. Lamello