Safety Speed Cut Thermwood Corporation ECabinet Systems

Cabinetmaking

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Edgebanding and frameless cabinets

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Edgebanding and frameless cabinets

11/3/16       
Lee

Website: http://www,legacywoodworking.net

I have a question regarding frameless cabinets. I'm doing a job now that has 3 different species of wood, plus some painted cabinets. All finished end panels and such will be installed on site. My question is, when you edgeband, do you match the finished exterior wood, or match your cabinets interior? I use prefinished maple for my boxes and was thinking of just using prefinished maple edgebanding for the boxes. In the past, I've matched the exterior wood, but was thinking that for ease of banding I'd do them all the same so as not to mix parts.

11/3/16       #2: Edgebanding and frameless cabinets ...
Leo G

I do exterior match.

11/3/16       #3: Edgebanding and frameless cabinets ...
rich c.

If you are doing an attached end panel, isn't the whole face showing? And you want to have a 3/4" wide natural maple stripe on a painted end panel? I'd match exterior.

11/3/16       #4: Edgebanding and frameless cabinets ...
Lee

The Face of the box will be behind the doors. The only thing seen on the exterior is the doors/drawer fronts, and the end panels with a solid piece of wood to look like a post.

11/3/16       #5: Edgebanding and frameless cabinets ...
JeffD

I've tried matching the exterior the hard way, by staining and finishing/painting, but it's far too time consuming. I personally would not want the banding to match the interior if it were different than the exterior, but it has been done. I think it was Thomasville that had a line of Euro cabinets done this way.....I did not like the look myself.

Nowadays I use PVC banding. I find a color/woodgrain that matches my doors as closely as possible and all is good.

good luck,
jeffD

11/4/16       #7: Edgebanding and frameless cabinets ...
Hen Bob Member

We match the exterior, As far as finishing goes we stack up 4-6 sides at once and spray. Clamp all stretchers together and spray as one piece. It actually goes pretty quick

11/4/16       #8: Edgebanding and frameless cabinets ...
Lee

Thanks guys. Up until now, everything has been a natural wood, so it was easy to find a matching band. I like the pvc idea.

11/4/16       #9: Edgebanding and frameless cabinets ...
jake mcgovern Member

Website: http://paramountwoodworking.com

we do a lot of euro boxes here and what we do is buy the matching raw wood and wrap it around some 4' long 12 round sono tubes. sand stain spray to match exterior then we roll it back up and run it on the edge bander. much easier then staining and spraying a bunch of random part sizes after its applied.

11/4/16       #10: Edgebanding and frameless cabinets ...
Tom C

We usually match exterior.
We try to do 1 MM when we can,
Like Henbob,we stack & clamp,but higher, run wrap & pack around the clamps for overspray, (dozen dedicated clamps)
and wide paper tape on some areas.
For all our white painted stuff, we use 1MM PVC. We have a couple colors that match most paints, Frosty, Designer,Ant. Wh.,Alabaster.....
Took 5 minutes to edge the boxes in the pic... bypass finishing to assembly
Greys,we use folkstone,fog,,,,
Custom colors ,Stack & we paint same CV.
All interior shelves I use 1 MM maple PVC
We have now a Brandt Ambition With Premill, very clean edges, Happy so far.
Been doing it this way for 20 years..
The only time I got a complaint was when I used prefin cherry on the boxes on a stained Budget cherry job. Go figure ....?


View higher quality, full size image (1080 X 1920)

11/6/16       #11: Edgebanding and frameless cabinets ...
aj

Tom C.. How do you go about getting the thicker end panel look? Is that 2 panels glued together then banded?

11/7/16       #12: Edgebanding and frameless cabinets ...
Tom C

The tall one is a 3/4" Door panel with a 3/4" MDF bottom section biscuted on & pocket screwed.
Joint is 1/8" Below the top that we stained to match floor.
The panel is then built-up on back side with 3" rip of MDF, Then 1/4" Solid stock glued on. Hoffman lip planed,sanded, 1/16" RO.
The 2 end panels we finished in shop, Conestoga finished all the other .
Crown & Base site painter.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Limtech Industries, Inc. Lamello