Labels
4/19/16
We're having trouble with the amount of time it takes to peel off our production labels on wood veneers, and some of our PLAM parts. What labels are you guys using? is there an easy release adhesive? Where are you buying them from? We currently use a dymo 450 at the router but cant seem to find an alternative adhesive that will release easy, any advice will help
4/19/16 #2: Labels ...
do a search using the label size or the label brand and number and the word removable.
dymo 450 (size or number) removable.
Should turn up many.
Richard
4/19/16 #3: Labels ...
Abel Label
http://www.ablelabel.com/
Get the DT Removable Adhesive label
Very friendly people and will help you pick the label you need.
4/20/16 #4: Labels ...
Use file folder labels and put them on the back edge. They come off pretty easy or you can just leave them on. They fit nicely on a 3/4" edge. Been doing it for 20 years with no problem. File folder labels just have regular glue, but they still come off pretty easy since it is on an edge rather than on the face. It also doesn't mess with your finishing.
4/21/16 #5: Labels ...
We buy the easy "repositional" stickers - Avery Knock-off You may need a different size.
Avery 8066 Compatible stickers:
http://www.desktoplabels.com/label-products/7330/3.4375_x_0.66_Labels_-_White_Pape
r_-_Repositionable_Adhesive