Total Finishing Supplies

Professional Finishing

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Paint buildup on spray nozzle.

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Paint buildup on spray nozzle.

3/20/15       
David  Member

Build up occurs on nozzle consistently where we have to clean the nozzle quite often. We spray precatalyzed lacquers clear and opaque. Use HVLP guns with spray pots. We've tried less air, material and fan and are still getting the above.

3/20/15       #2: Paint buildup on spray nozzle. ...
Nick

If your material flow and air pressure are suitable for the air-cap then build up on your air-cap is usually the result of either a dirty/clogged air passage in one of the horns of the air-cap or some solid gunk stuck in the nozzle giving you a angled stream out of the nozzle...give that baby a good cleaning and if that doesn't work then it sounds like time for new parts.

3/21/15       #3: Paint buildup on spray nozzle. ...
David  Member

Thank you for the tip Nick, we will try it out.

3/21/15       #4: Paint buildup on spray nozzle. ...
herb johnson

the other thing that will cause that issue is spraying too close to the part and bounce back is laying on fluid tips, the other reason is that if you are soaking your air cAPS, whic you should not do, any obstruction in the air cap holes or ports that can turn the pattern to a different angle, sometimes you have to change out an go to a no smoke air cap that is available for binks guns, seriously their is a cap designed just for that very issue

also did it just start happening, look at the fluid tip and make sure it is concentric, if not that can be a cause

good luck

herb j

3/21/15       #5: Paint buildup on spray nozzle. ...
Jim

Herb
Over the years I have learned much from your answers. So thank you!

You mentioned "not" soaking your air caps.

After cleaning , I take the gun apart and clean and soak the needle, nozzle and air horn. I use a 50/50 lacquer/aceatone.
Thoughts?

3/22/15       #6: Paint buildup on spray nozzle. ...
herb johnson

thanks for the very kind words, think of soaking your air cap like this

you place in a jar/can of solvent, over time the solvent breaks down any paint, or coating letting the sediment form on the bottom of the can, out of site out of mind, when you drop the air cap in, it is like stepping in mud in a creek, the bottom is disturbed, the problem with the air cap is that they are many holes which are small that small particles can land in and sometimes they are a pia to remove if at all, the extra big problems is teh horn of the air caps where it turns 90 degree, if you get a piece of sludge in their unless you have a ultrasonic cleaner, the air cap is toast and get ready to spend between 70-140 for a new one.

if the air cap is direct, hold it facing down, the horns facing down so the junk that you clean off falls down not back inside the aircap

again,

thx for the kind words

herb j.

3/22/15       #7: Paint buildup on spray nozzle. ...
herb johnson

also why take apart the gun, if its flushed and you leave it wet filled with solvent very rarely do you need to take it apart unless you are using a coating that has a very short pot lilfe, all you do is wear out the seals faster, always leave the gun full of solvent,

3/30/15       #8: Paint buildup on spray nozzle. ...
joe

Dave,

What type of HVLP gun are you spraying with, your fluid nozzle size, what is the fluid pressure set at going into the pot and your atomizing air setting to gun.

3/31/15       #9: Paint buildup on spray nozzle. ...
Shane

If material is collecting on your cap I would suspect your material is possibly too thick for your setup. Try reducing if a good cleaning doesn't fix you up...

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)