Subject: Re: Waterborne

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Waterborne

5/3/15       
Zoltan Member

Website: http://www.tortelicustomwoodworks.com

I am planing to improve my finishing system and the quality. Currently I use waterborne poly from General Finishes, which I am happy with,but I believe there is a better product. I spray with a pressure pot,which gives me a nice finish,but...
I'd like to go to the next level.
I'd like to hear some great suggestion on what waterborne product I should try and what equipment.
I mostly finish cabinets and do refinishing as well.

Thanks for all your help

5/3/15       #2: Waterborne ...
Brian T

Try out Sayerlack AF72. Used as clear as well as pigmented. Best water based product I have used in over 15 years of spraying them.

Also see if you can demo a kremlin or graco merkur AAA pump. It's the next logical progression in finishing equipment and quality.
Get the right tips for the finish.

5/4/15       #3: Waterborne ...
Bart

I've been using GF for over a decade and I'm really happy with them. One stop shop for dyes, stains, clears, pigmented, glaze etc... That being said it would be hard to get that commercial 2K euro/poly pigmented look with GF without lots and lots of coats. As someone who started in the solvent world theirs and other mfg's WB's I've used are really tough stuff now and unless it's a look thing you might be chasing your tale. Have you tried their new conversion varnish which is a two part euro style finish. It's got the nasty catalyst just like the euros.

As far as the AAA's you should search the data base. WB's and AAA don't always get along. You can get a "shearing" issue with the pump which can translate to micro bubbles. I considered it but at $2K +/- you better being spraying lots product. I just upgraded by guns for my pots and gravity apps.

my2cts

5/4/15       #5: Waterborne ...
Zoltan Member

Website: tortelicustomwoodworks.com

That was my first thought, trying their 2k varnish. The sales rep should bring samples this week.
Bart, have you tried ML Campbell's wb?What top coat do you use from GF?

5/4/15       #6: Waterborne ...
Nick

I agree with Bart...I like the pot & gun for WB's better than a AAA, I think you get a better finish and a lot less problems (micro bubbles). I did just buy a 1:1 diaphragm pump for spraying WB's but since it's on it's way I can't report if it's a worth while investment and an improvement over a pressure pot yet.

5/5/15       #7: Waterborne ...
Brian

I've been spraying waters for nearly 15 years with pumps and binks pots with devilbiss guns. After switching to AAA 13 years ago I would not go back to pots. Shearing is due to using a filter in the pump or the gun that is to fine for the material. The material separates as it goes through the filter not the pump. This is easily resolved by stepping up to the larger size filter.

We use 4 graco merkur pumps and 2 kremlin pumps as well as 4 cup guns for small job. The pots are no longer in use. We took the guns off them and set them up with pps for ease of use. We spray on average 20 gallons of chemcraft WB aquaprime per week with no issues.

We also spray 30 gallons per month of sayerlack WB finish with no issues.

2 of the pumps we have are dedicated for solvent top coats which we spray roughly 15 gallons per week of , 2 are for wb primer and the others for WB top coats.

I sprayed GF for nearly 10 years. They are great products but after switching to Sayerlack I would not go back.

That being said I have not sprayed any GF besides Exterior 450 in 3 years and I am not familiar with any of there newer products.

5/5/15       #8: Waterborne ...
Zoltan Member

Website: tortelicustomwoodworks.com

Thanks for all your advise

5/13/15       #9: Waterborne ...
Evan Member

Website: http://www.near-west.com

I've been spraying GF Enduro for several years, I liked it a lot but a recent project forced us to look for a faster local source for custom tints. Our SW rep pointed us to Sayerlack, it's incredible stuff. 1 coat of the pigmented over sanded primer, and it covered completely. It is absolutely dead flat, beautiful. That wasn't even using our good guns, just a $90 Porter Cable cup gun that we use for samples.

5/13/15       #10: Waterborne ...
Denny J

Sayerlack is probably one of the few I have not sprayed. We use mostly GF and Aqualente in WB due to availability.

If you are looking for an AAA and are open to a pre owned, I have a CAT AAA with a bobcat gun and lots of accessories that is cart mounted that I am thinking of selling. We have a Merkur that I am very happy with and can get replacement parts locally for.

5/14/15       #11: Waterborne ...
Zoltan

Evan, what product did you use from sayerlack ?

Denny, Could you tell me what difference you found between Aqualente and GF Enduro? pros and cons. Which one is better?

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)