Total Finishing Supplies

Professional Finishing

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Waterborne pigmented finishes

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Waterborne pigmented finishes

5/13/15       
JohnB Member

I have a good sized cabinet job coming up that calls for a low sheen white finish. I would prefer using a water based product but looking for some feedback. I have sprayed both Target and Agualente finishes in pigmented with better results from the Agualente but wonder if there's anything that might be a little better. SW has their Kem-aqua, and there are others but interested in opinions and what you like or dislike. I plan on shooting some test panels using my CA H20 aaa unit.
Also, do any of you topcoat with a clear such as Target's 9000 or just use the pigmented for final coat?

5/13/15       #2: Waterborne pigmented finishes ...
JP Member

I have used only waterborne for about 10 yrs. MLC Agualente and ValSpar Zenith.

I like the Zenith better. Especially the under Coat. Much easier to use.
If your using the CA Waterborne AAA (I use it with a bobcat Gun), Follow the recommendations MLC and CA Tech give for the settings. Thin as much as you can get away with (40 with #4 Ford cup).

If you use the 409F tip (their recommendation) it clogs very easy. watch and clean often. If you use the 411F, watch the fluid flow.

I use the 409F and set the fluid at 20. The air to tip at 16. Go from their.

Micro bubbles are unavoidable, so I use a retarder to reduce. Helps with the bubble pops. In fact I do not use moving air to help dry like MLC and CA Tech advise. Drys too fast.

One last thing comes to mind. When CA Tech shipped my AAA, they did not ship with a Stainless Steel fitting Fluid Supply hose. The fittings rusted almost immediately.

Good luck

5/13/15       #3: Waterborne pigmented finishes ...
JohnB Member

JP,
Thanks for the response. Do you do a clear over the Zenith or is it pretty durable on it's own? Any crosslinker to add? My CA rep gave me a small screen the other day that he says they have come out with that goes in the bobcat gun right behind the tip that is supposed to greatly reduce the micro bubbles. Have you tried one of these? I haven't had a chance to myself yet. The micro bubbles were the biggest problem with the Target finish although not as bad if I didn't add the optional crosslinker.

5/13/15       #4: Waterborne pigmented finishes ...
JP Member

John

I do not use a clear finish as a topcoat. So far it's been great. I'm using the 409F tip. It's for waterborne and has a pre-atomizer. It doesn't look like a screen though. It looks like a mini bullet casing with a tiny hole in it. It goes in the tip under the white ring. Is this what you were talking about?

5/13/15       #5: Waterborne pigmented finishes ...
Denny J

Different people will obviously have different opinions. We tried the Zenith and it was the thinnest and worst performing finish that we have tried and over the past 2 decades we sprayed most of them.

The Aqualente is a good product and we have used a lot of it. Currently I feel that the General Finishes Poly is a very solid product that ha great build, chemical resistance, sag resistance and appearance.

The best finishes that we have ever used were from a company North of Duluth Mn called Van Technologies. The owner is a Chemist and has an amazing mind when it comes to WB coatings and how they work It would be great to see him get crowd funded and become a major player because his product line and knowledge are second to none.

That being said, General Finishes has the most comprehensive line of domestic WB finishes IMHO in that price point and only imports like ICA have a wider offering and are much more costly.Becker Acroma is also outstanding but premium priced.

5/14/15       #6: Waterborne pigmented finishes ...
JohnB Member

JP,
After looking closer, I think that is what he gave me, but haven't tried it yet.

Denny,
Do you see issues with micro bubbles with the General product? I have tried some of their stain but nothing else. I would have to buy by internet as no dealer in our area. So far, MLC and SW are both locally available, with Mohawk also a possability. The Kem-aqua is another product I was thinking of trying.

5/21/15       #7: Waterborne pigmented finishes ...
Jeff Fleisher Member

Website: http://www.jeffswooddesigns.com

I build furniture and have used SW Kem-Aqua and it is very nice to use. I've used the pigmented version on some display cabinets. It goes on very nice and is extremely tough. Almost to the point where it is hard to scuff between coats.

5/24/15       #8: Waterborne pigmented finishes ...
Larry

Interesting takes on various finishes. We had used Hood finishing's w. b. urethane for several years. Great on maple & cherry, horrible on oak/ash. The most durable finish we've ever used. No tech support though. Switched to SW Kem-Agua. for several years. worked OK & had local support. Always did a wash coat, stain, and two tops. Had some complaints about durability. Went to MLC Agualente, lays down nicely and have gone to 3 top coats for better durability. Have been considering using their crosslinker additive. Anyone using it? Results?

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)