Total Finishing Supplies

Professional Finishing

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: ML Campbell euro-blid wetlook

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

ML Campbell euro-blid wetlook

9/11/15       
nick

I have a good size job spec-ed with this product and I have yet to use it. For those of you who have...any words of wisdom, tips would be appreciated...PI sheet says 92% sheen, no sanding between finish coats and 2 hour pot life,,,yikes
Job is typical euro cab; hard maple edge banded boxes, flat panel doors and drawers. color will be mostly white with a fair amount a deep red. Thank you

9/11/15       #2: ML Campbell euro-blid wetlook ...
Read

Nick,

I have used MLC Euro X for front doors, one satin and the other glossy, wet look.

Both doors have stood up well and look great after 4 years.

These glossy finishes are very unforgiving and will show every blemish. If you have a fussy owner, then you could be in for a lot of pain and suffering. You will need a clean environment and clean air. Be prepared to spend time sanding and filling to get a perfect finish.

Good luck.

9/12/15       #3: ML Campbell euro-blid wetlook ...
Jim

The last time my chemcraft rep was in we talked about this type of finish. He warned me to allow a lot time for wet sanding and rubbing the finish out. He told me I couldn't achieve an exceptable finish with just spraying like a satin sheen. I haven't tried this but thought I would pass this along.

9/12/15       #4: ML Campbell euro-blid wetlook ...
JeffA

In other words, you will need to practice. Alot. And don't do small panels as they are too easy. Do something rather big, at least 2x2.

9/14/15       #5: ML Campbell euro-blid wetlook ...
Max Neu

A few things to consider, use a very flat substrate like mdf,anything less than perfectly flat like plywood will look horrible! Also,plan on sanding and polishing to get the final finish, a flawless gloss finish right out of the gun is unlikely to happen. Use a finish that allows for heavier build do you can sand/polish without burning through the gloss coat.
Good luck!

9/14/15       #6: ML Campbell euro-blid wetlook ...
JeffD

I used it on a wine bar several years ago and agree with what the others have said. Lots of sanding and buffing after spraying. Also make sure you price out the finish before quoting. I don't remember exactly how much it cost but it seemed ridiculously expensive at the time.

good luck,
JeffD

9/14/15       #7: ML Campbell euro-blid wetlook ...
rich c.

Even mdf needs lots of work. There can be waves in the surface that show in high gloss.

9/15/15       #8: ML Campbell euro-blid wetlook ...
Dennis

I recently built a high gloss piece out of "balsa core", by Kerfcore, worked out quite well. As has been already mentioned, lots of sanding. Wet sand up to 4000 grit and than rubbing compound and a buffer up to 11,000 grit.

10/3/15       #9: ML Campbell euro-blid wetlook ...
Mike J.

I have used the MLC wetlok finish several times, all with good results and no buffing after the spray out. I use Kremlin spray equipment. I got good adv ice from a finisher in California quite some time ago and recommendations from the MLC rep in Canada. The finisher in California recommended only one coat of wet look finish per day, three coats total. I have found sanding between coats with 400 grit paper on a Porter cable electric sander to be the best scuffing technique. The wet look, as per the MLC rep should be catalyed with the red catalyst 1 to 1 as required and the reduced 30% with euro retarder. example , 10 ounces wet look , 10 ounces red catalyst, and then 6 ounces retarder. I spray two and one half passes off the gun , a half pass is twice as fast as a full pass, then let dry. The three coats of wet look go over 2 coats of euro primer. I am sure to wet down the spray booth and surrounding areas with gallons of water.

10/3/15       #10: ML Campbell euro-blid wetlook ...
nick

Thank you Mike J. that's the kind of info I was looking for.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)