Subject: Re: Small product, large quantities - finishing cherry

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Small product, large quantities - finishing cherry

9/13/15       
Ben Aroh Member

Hi everyone,

First post here, though I frequent the forums. I recently started a little woodworking company. Things are going great, but I have a finishing question that is outside my experience.

We manufacture a small product out of cherry - see the pictures attached. We make all 50 states, cutting them from cherry panels. Each state has a few magnets embedded in it- so it can hold paper clips, keys, etc. The shapes are fairly small and we stain them to a walnut brown color.

I would love to rub on a gel stain, seal them, glaze them & finish. But a finishing process that complicated is just out of the question- trying to minimize handling of the pieces & keep this operation as efficient as possible.

We are about to ship out an order of 1,600 units- and finishing is quite chore!

Currently we spray on a stain, and topcoat with two coats of urethane. I am in Louisville, and purchase my finishing materials from a small company called Jellico Chemicals.

Although our current finishing schedule is simple and quick, I'm not convinced its the best method. Cherry has its quirks, and some pieces get too blotchy and dark for my liking.

Water base materials have caught my eye. I was almost thinking a water based dye (maybe dipped) - followed by a tinted sanding sealer (to kill some grain for more uniformity) and a water based topcoat.

We are looking for a slightly rustic looking finish. Walnut / mahogany brown color. It needs some durability, because of the embedded magnets.

I would love your advice, b/c I simply do not know the best route to go from here!

Thank you so much,

Ben


View higher quality, full size image (600 X 600)


View higher quality, full size image (1000 X 1000)


View higher quality, full size image (1000 X 1000)

www.arohmade.com

9/14/15       #2: Small product, large quantities - f ...
Jim Member

Have you looked into a tumble finish?

It works great for large batches of small products.

9/14/15       #3: Small product, large quantities - f ...
Ben Aroh Member

Interesting! I hadn't thought of a tumble finish- but I'm concerned the states may actually be too big for that? Most end up around 12" long. Also many states have areas that may be prone to breaking off.

But I will do some research!

I wish I could tumble sand the edges somehow! The CNC leaves a decent edge most of the time- but still requires hand sanding. (at least we are able to edge sand groups of 20 states at a time)


View higher quality, full size image (2448 X 2448)


View higher quality, full size image (2448 X 2448)

9/14/15       #4: Small product, large quantities - f ...
Bart

I'm a big fan of WB I've used General Finish products for years. That being said WB stains/dyes will raise the grain which could be a problem when doing large batches. I'd stick to a solvent NGR (non grain raising) type of dye or stain and a dip/spray nitro lacquer finish (urethane seem a bit of overkill). Little or no sanding necessary and a decent finish. Mohawk has all sorts of NGR dyes and stains and lacquers.

9/14/15       #5: Small product, large quantities - f ...
joe

Ben,

As far as the color you should be using a spay stain not a wiping stain.Considering these parts are flat and your spraying a thousand plus pieces you should be looking into a small line spray something like the Cefla Mito K should be something to look into

9/14/15       #6: Small product, large quantities - f ...
Ben Aroh Member

That Mito K machine looks pretty amazing! I contacted them out of curiosity- but I have a feeling we can't afford it just yet. Definitely something for us to keep in mind! I wonder how it would do on the edges?

I do need to switch to a spray "no wipe" stain for color. That will likely be the best alternative. I've never used one actually!

Also, the urethane may be overkill. But I love how quickly it builds. Two coats seems to do the job.

I'll check prices on the Mohawk lacquers, and maybe give one of those a shot too.

9/14/15       #7: Small product, large quantities - f ...
Denny J

You might be a good candidate for a WB UV system. Do a google search for VanTechnologies.

9/16/15       #8: Small product, large quantities - f ...
JeffA

Those look samples look great. The detail is what will kill you, especially those edges. Once they are smooth it should go well. I wouldn't use water based until topcoat. Did you ease the edges? That will help with keeping the cut through's at a minimum. Looks like alot of hand work.

9/16/15       #9: Small product, large quantities - f ...
Ben Aroh Member

Thanks Jeff!
But I'm not quite sure what you mean by cut throughs?

9/17/15       #10: Small product, large quantities - f ...
JeffA

I should have said sealer sand cut through. When you sealer sand a sharp edge, you cut through all the way down to raw wood, taking off the stain and leaving a spot that needs touch up with stain. If the edges are eased or rounded a bit, the cut though's don't happen as much.

11/12/15       #11: Small product, large quantities - f ...
monty

"Splash Stain"!!!!
We use it on chairs, just dip, roll and dry. Easy to use and will work on anything.
Monty

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)