Subject: Re: removing grease and glaze from kitchen doors?

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

removing grease and glaze from kitchen doors?

8/18/16       
JeffD

So an odd question, I'm doing a favor for the MIL and trying to clean the grease off several kitchen doors, the ones directly over the stove. This woman cooks a LOT and the grease is absurdly thick. I tried the usual suspects like Simple Green and the grease just laughed at all of them. I'm now trying DNA and while it removes the grease, it's also removing some of the finish!

To my understanding the only solvent based finish that's susceptible to DNA is Shellac. These are 25 or so year old factory cabinets, (I think IIRC Schrock), so I can't imagine they used shellac, but it's definitely removing something! Almost seems like a glaze coat as the stain coat is still protected under a layer of dull finish, but there's a bit of color to the gunk coming off.

So my questions are....would they have used a softer finish as a glaze and left that as a topcoat? Alternatively could a finish degrade over 25 or so years to the point of being susceptible to DNA? The lower layer of finish seems impervious to the solvent. Also the rest of the doors away form the stove still look fine.

Would it be safe for me to spray a coat of catalyzed lacquer once I remove this gunk for a fresh topcoat? Or is there no way of knowing without trying it out?

Lastly...does anyone know of a good grease remover that's less potent than DNA but significantly more powerful than Simple Grean, 409, etc.? I still have the cabinet fronts to try and clean and don't want to deal with removing finish from them.

thanks,
JeffD

8/18/16       #2: removing grease and glaze from kitc ...
Leo G

Tri Sodium Phosphate is what is usually used to clean grease off cabinetry. If the finish is that soft it may take it off too.

Look for TSP.

8/18/16       #3: removing grease and glaze from kitc ...
Leo G

TSP... CLEANING FOR THE BIG DOGS!!

TSP... CLEANING FOR THE BIG DOGS!!

8/19/16       #4: removing grease and glaze from kitc ...
james G

Dawn dish detergent with a white scotch brite pad . The white scotch pad is soft enough to not typically harm existing finish . I usually will wipe down with VMP naphtha after that . Make sure to rotate and keep your rags somewhat clean so your not moving contamination around as well . Fish eyes can be a issue even after all your cleaning ... No matter what you use ...
As for going straight to a catalyzed lacquer after that, sounds like a disaster for finish crinkle issues . I like to shoot ML Campbell's vinyl ... Any vinyl sealer would most likely work . This should melt and adhere to existing finish , allowing to proceed to your more durable catalyzed product after .
I recommend that you do a couple light ... And I mean light ...dust coats of vinyl first . This will sit on top and not allow the fish eyes to form usually . After that has dry , you can come back and put your wet coats of vinyl for build .
Hope that helps .
Old finishes are weak . Heavy solvents for cleaning only break them down more and make them susceptible for finish failure when you put your solvent sear or top coats on top .

8/20/16       #5: removing grease and glaze from kitc ...
kevin

im a fan of automotive wax and grease remover.


View larger image

8/20/16       #6: removing grease and glaze from kitc ...
Mastercabman

TSP and then lightly scuff sanding
You can try a pre-cat lacquer but try it on a small area first
I wouldn't use post cat or CV if you don't know what's on those doors

8/21/16       #7: removing grease and glaze from kitc ...
Adam

Don't dilute the Simple Green more than 50% with water. It is better at removing motor oil and grease than anything I've ever seen.

The longer it sits the better it works. I would mix it 50/50 with water. Spray the cabinets. Let it sit for 1 hr. Then go back with a bucket of water and a sponge and wipe it all off.

8/21/16       #8: removing grease and glaze from kitc ...
Adam

TSP is amazing stuff. Besides taking the grease off, it will degloss any oil based finish. Which makes it great for painting ones house.

8/22/16       #9: removing grease and glaze from kitc ...
jonathan mahnken

TSP is the only thing that has impressed me besides the automotive type solvent stated above. And yes it does work on kitchen grease very well, just used it today on a kitchen refinish. I dont know about motor grease ect, but simple green has never impressed me, though I have never mixed it as strong as 50/50

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)