Total Finishing Supplies

Professional Finishing

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Spraying assembled drawers

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Spraying assembled drawers

9/26/16       
Jeremy

Hi there- wondering about some tips in spraying drawers that are assembled. I used to spray the parts individually with tape covering the joinery, but that made for many pieces to spray and tape and burned up a lot of valuable time. I turned down fluid coming out of gun so I don't get all the runs, but doesn't seem drawers are as smooth as I would like. Also, the tip of the gun keeps getting plugged with over spray since many of the drawers are seven to ten inches deep in a drawer base. The boxes are made out of the leftover wood from other parts of the kitchen making it nice since there is not much waste left at end of job. Depending on the specie of wood, using gf enduro-var or enduro poly and have been putting two coats on. I know gf says to put on three coats, but that seems overkill for a drawer. Any help/suggestions would be helpful in for future spraying. Thanks.

9/26/16       #2: Spraying assembled drawers ...
Mike Member

When i make drawers i cut the back short of the groove so i can slide the bottom in and nail the bottom to the back piece. I use the bottom to hold the drawers square with a couple of tacks in the bottom while the glue dries then remove the bottom to spray. When finished install the bottoms permanently. I also use prefinished ply for the bottoms.

9/26/16       #3: Spraying assembled drawers ...
Jeremy

The idea of taking the bottom out would sure help keep the gun and my face much cleaner. Never thought of trying that. I do apply three coats of finish on doors, face frames, end panels and such since they are exposed, but since they are laying flat I can spray a much thicker film on them. When doing the drawer sides and the gun is toned down so I don't get runs, is two lighter coats this way durable enough. Drawers arent really exposed to the exterior, but spoons and heavier items could ruin them eventually.

9/26/16       #4: Spraying assembled drawers ...
rich c.

Aren't you using an HVLP gun? Why all the bounce back? Turn the air and the fluid down if you have to. If the tip is getting clogged from the bounce back, you are holding the gun WAY TOO CLOSE! That's something I've never encountered, can't imagine how that happens. The bounce back can't be more pressure than what is coming out of the tip.

9/27/16       #5: Spraying assembled drawers ...
Pdub

Spray all of the inside pieces and their top edge's flat, assemble with prefin. bottoms then spray the assembly upside down.

9/27/16       #6: Spraying assembled drawers ...
jonathan mahnken

why arent you just using prefinished ply for the boxes?

9/27/16       #7: Spraying assembled drawers ...
nick

It's safe to say I spray over 1,000 drawer boxes a year (double that is more like it) and getting a off the gun smooth finish is no easy task...getting a off the gun smooth finish with 2 coats of wb...damn near impossible...as any sanding burn through on your first coat will give you some grain raise on your second. This can be alleviated the next day with a little rub-out with 0000 steel wool, 1500 grit wet/dry or white scotch-brite.
Don't get me wrong, I like/prefer finishing drawer boxes with wb as a solvent finish (CV) can out-gas for months in the confines of a drawer box but I always start with a coat of de-waxed shellac...dries quick, sands OK and keeps the grain raise down. I like sanding it with a new fine-grit sponge in the corners and 320/400 on a RO in the flats. Then I spray 2 coats of whatever WB I"m using (SW kem-Aqua at present)I sand with a fine grit sponge between wb coats, once again real focusing on the corners.
I prefer a pot/gun set-up for WB and for clears I use a Sata 1000k with a 1.3 needle/nozzle .
I'd be lying if I said it comes out perfect even after all of that effort as it is not uncommon for me to do a little rub-out in the corners just before the customer picks it up.

9/27/16       #8: Spraying assembled drawers ...
nick

PS; if you're building these thing save yourself some time (as has been mentioned by others) and build them out of pre-finished maple. It's lots easier to finish just the top edge...just brush on a couple of coats Target 2000 (that stuff is magic) keep a wet rag handy to keep the excess off the pre-finished material. Any roughness can be easily be alleviated with a little very fine abrasive the next day.

9/28/16       #9: Spraying assembled drawers ...
Jeremy

thanks for the input guys. I mainly use Blum soft close undercount slides, so it it easy to glue up leftover stock and sand/plane to 5/8" for the drawer parts. This kept my scrap pile to a minimum, but I will look into pre finished ply for the parts because a lot of effort seems to be doing into these boxes to achieve a good finish-more than is necessary I think. I will also work on gun to see how can get less bounce back. Thanks again

9/28/16       #10: Spraying assembled drawers ...
Mastercabman

Why not spray parts BEFORE assembly?
And use 1/4" prefinished plywood for the bottom?
Most cabinets manufacturer are doing it that way

9/28/16       #11: Spraying assembled drawers ...
D Brown

You could use the new clear edge banding material on prefinished plywood and be done.

9/28/16       #12: Spraying assembled drawers ...
Steve

Dried paint piugging the tip is not so much a result of blowback but rather an issue of air pressure drying the material too soon. Leaving the bottom out is convenient but for the commercial users here, they generally get their drawers from drawer box/door specialties so it is fully assembled. Proper distance from the surface should eliminate the clogging. Lastly, using offcuts from to build the drawers begs the question if you are spraying uniform surfaces. Using prefinished maple sides is usually only practical in the commercial environment since the suppliers sell them in case lots; buying them at WW stores is prohibitively expensive.

9/28/16       #13: Spraying assembled drawers ...
jonathan mahnken

gluing up boards to make drawers is a timely investment. How much is your time worth? I would be using pre finished baltic/russian birch ply, or apple ply for you snobs. But If you really want to carry on doing it this way then I would suggest spraying the parts flat. If you are doing butt joint drawers, Roo glue sticks very well to WB lacquer.

9/28/16       #14: Spraying assembled drawers ...
herb johonson

one other point if you dont buy they prefinnished

if you don't have one get a air assisted pump system will cut down overspray a lot reduce your sanding

good luck
herbj

9/28/16       #15: Spraying assembled drawers ...
Bart

Agree with others pre-finished is the way to go. I won't even take a job if they use unfinished drawers or boxes anymore. It's like analog and digital. Get with the times. At least pre finish your scraps after you size them. The price difference between raw and pre finished 1/4" and 3/4" is minimal. BTW the import pre-finish is a NO go.

9/29/16       #16: Spraying assembled drawers ...
Scott

I would agree with Herb, spraying the inside of cabinet boxes and drawer boxes requires an air assisted pump, you can dial the air way down and just lay the finish in place with very little overspray.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)