Total Finishing Supplies

Professional Finishing

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: setting up a new spray shop

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

setting up a new spray shop

11/30/16       
keith Member

I own a small finishing business, i mostly finish for local high-end millwork companies here in New York. In a few weeks i will move into a new work space (bigger, easier controlled environment), that gives me a clean slate to set up whatever way i want. i will have a 1,800sqft box room i plan to use for sanding, prepping wrapping etc..with a seperate room 600sqft where i plan to put an open face booth.

My question to all you finishers... what would you advise or do differently if you had a clean slate to work with when organizing you finishing shops? layout and equipment etc??

just curious, Thanks in advance.

11/30/16       #2: setting up a new spray shop ...
rich c.

Biggest deal this time of year is warm make up air. I also suggest you talk to your insurance agency and building/fire inspectors before shopping for a booth as well.

12/1/16       #3: setting up a new spray shop ...
Shane

Agree with Rich.. if you have the leisure of having a separate room just for finishing... clean it from floor to celing.... paint the walls high gloss white if you can.... invest in a heated air makeup and put your booth fan on a variable frequency drive... this way you can control your booth to have positive pressure pushing out of the room..... if you get junk in your finish its your practices inside the room... Also we put booth media on our air makeup intake to catch large debris... changed the aluminum mesh filters to merv8 pleated and had our ducting inside the room refitted with frames all along the ducting to hold 25x20 merv10 pleated filters.... its a pain to change them and we change every two months sometimes more but we have clean intake air coming into our room! Lighting lighting lighting... we have led bay fixtures hanging and man what a difference! no shadows!

12/1/16       #4: setting up a new spray shop ...
chris

your local fire inspector will want sprinklers especially in the booth.
I had to get a certified architect draw up plans for the spray room. had to use 5/8 and out and fireproof doors.
I would have been better off using an automotive style booth
search NFPA code 33. This gives you all the requirements to set up a booth.
I'm in orange county NY

12/1/16       #5: setting up a new spray shop ...
keith Member

Thanks for taking the time guys, i will speak to my landlord today about the alerting the fire inspector etc..

Painting the walls gloss white, i never would of thought of that, makes total sense... As far as the heated air make-up unit goes, obviously being a small business owner, my first reaction is....how much $$$? I have no experience with make up units and obviously they vary in size and quality like anything...but can anyone recommend a brand and estimate rough cost?

12/1/16       #6: setting up a new spray shop ...
chris

i can give you a name and number from where i got my air make up unit.
he services NY.

12/1/16       #7: setting up a new spray shop ...
keith Member

That would be great Chris, thank you.

12/1/16       #8: setting up a new spray shop ...
al

Shane,
Are the LED lights you have explosion proof? A friend gave me a LED shop light and the light is so much better. You do not replace the bulbs on this particular one, rather there is just a tiny little strip 48" long mounted to inside of housing. However it is just a general shop light and not for paint booth.

I tried LED replacement bulbs in a florescent fixture that are compatible as long as it's a rapid start ballast
which it is and the lighting is no better than florescent.

Larson brand explosion proof LED come with tubes like florescent but has no ballast. This is what I would like for my spray booth if I can get the light like the one my friend gave me but not interested if similar to
the LED bulbs I tried in florescent fixture. Anyone know about the Larson LED's? They are just under $1000
each for 4 foot (2) tube light. These are the type with glass tubes around the lighting tubes.

Thanks,
Al

12/1/16       #9: setting up a new spray shop ...
Arthur grudko

Website: http://primezall@gmail.com

RE: LED LIGHTS

If they are to be used for color evaluation, bear in mind that they wash out the red out of red mahogany. Make it look sorta like walnut.

12/2/16       #10: setting up a new spray shop ...
Shane

Our LED hanging lights are just bay lights hanging from our high celing wharehouse and are not explosion proof or located inside spray booth... All our booth are from global finishing and have the appropriate rating and color correction bulbs for color matching while your inside the booth area.... Our booths are about 21' foot wide 12' tall and 12' deep open face booths... I have four booths in one room with make up air and the same setup in another room...

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)