Total Finishing Supplies

Professional Finishing

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Thinning CV

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Thinning CV

12/19/16       
Ryan Member

Hi,
I have been using SW KEMVAR PLUS conversion varnish, I sometimes have trouble with sheen variations, sometimes not. It says thin up to 55% I am using aaa air assisted airless , I noticed when I thin more I have less problems , but I am going over the amount recommended. It seems that the spray pattern evens out and doesn't collect in thicker streams on the outside of the pattern which is causing sheen variations. Also keeping the tip cleaned out is easier as well, when it's not as thin it is always gunking up constantly. I'm probably thinning about 10% over recommended amount. Also this might be a stupid question but when it says thin let's say 50% does it 50/50 or 2 parts to 1 part?

12/19/16       #2: Thinning CV ...
kevin

Ryan, i would assume your talking about the Pigmented kemvar plus since your reducing it 50% .. the clear conversion varnish doesnt require reduction (ive been using SW products for over a decade with great results).
50% reduction would be 50% of volume. for example: for one gallon of cv you would add half a gallon of kemvar reducer.

If you're getting tails on your spray pattern (more material towards outside of fan) it would be on the spray equipment side. maybe you need to tweak your air/material outputs. Over thinning your material may help but its not ideal.
What size tip/nozzle are you using and what brand AAA?

12/19/16       #4: Thinning CV ...
Jim Clark

what are you using for thinner?
If you're using lacquer thinner, it may
be part of the problem.
Most lacquer thinners are reconstituted
and are junk.
I use auto grade Urethane Reducer.
It works much better and you can get
slower and faster grades.
I most always use the slow grade, it lets it
melt in real good.
I also thin my CV about 40%.
That's like 10 oz of CV to 4 oz reducer.

12/20/16       #5: Thinning CV ...
kevin

With the sherwin williams kemvar plus, lacquer thinner will give you spotty results. (Like jim said). They have Kemvar Reducer that is intended for use with this product and does the job well. I use it in any pigmented jobs that are not being topcoated with clear. If im clear coating over the pigmented cv then i just use lac thinner in the color coat

12/20/16       #6: Thinning CV ...
Brent

I also had this same problem with SW water white CV. After several long discussions with the SW coatings team we figured out I wasn't agitating good enough. Sounds dumb but it doesn't remix as well as lacquer, which I switched from. All coatings are high gloss and the part that settles out is the sheen inhibitor. No problems since I bought a mixing drill bit from SW. Maybe this is the problem. I also quit over thinning the CV, its a different animal than lacquer and I figured it out finally.

12/30/16       #7: Thinning CV ...
Steve Member

Use R7K310 reducer for Kemvar Plus

1/19/17       #8: Thinning CV ...
Eric Member

I use the Kemvar plus and you butyl acetate up to 40% without effecting sheen

Gives a much better lay down and Is a fraction of the price of the kemvar thinner blend..

I mix my own pigments using Phoenix and 844 colorant...

Darker colors require using a blending clr cv as well as white...much thicker and requires much more reduction

at which time I have a butyl acetate, xylene and high flash naphtha mix that still is a fraction of the price..

Tails are not necessarily due to equipment..but if product is to thick,,for your 1.4 then your going to have a dry spray.

Try using a larger tip if your afraid reducing will affect sheen 1.8

Binks 2100's have a 66SS fluid tip that's equal to a 1.7

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)