Subject: Re: White wash with sherwin williams cv system

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

White wash with sherwin williams cv system

2/11/17       
antonio

Website: http://positivewoodworks.com

about to get into a pretty good sized job involving white washing (or white pickling) of 2' x 8' maple panels. We haven't done this since we switched to CV years ago. We had a pretty good system before we knew about CV where we used a WB clear finish over a ragged on/off white WB paint. That was ok in its time before we knew about the durability of CV so we want to try this with white pigmented CV and water white clear CV preferably with sherwin williams products. My question is, can white pigmented cv be thinned enough to be a good white wash sprayed on? Or better yet, what methods are you guys using with CV to get a good white wash?

2/12/17       #2: White wash with sherwin williams cv ...
Sean Jackson Member

I've achieved this look a few times, here's how i go about it: under a clear CV finish i use white pigment (water) stain, maybe diluted 50/50, I think id be sealing off the maple with a thin 50/50 thinned sealer (thinned varnish) as maple might be uneven in absorbing any colour and finishing off in clear CV.
White coloured (milky) CV used to get a washed out/white look hasn't worked well for me in the past. Going with a thin white colour led me into warm and pink white hues as the base colour becomes more of a factor obviously. Plus 'coloured finish' is never going to look as good as a clear finish for wear and tear I think.

2/12/17       #3: White wash with sherwin williams cv ...
antonio

thanks sean, you used a wb stain under clear cv with no adhesion issues? or was there a cv clear sealer applied over the stain first as a barrier coat?

2/12/17       #4: White wash with sherwin williams cv ...
Sean Jackson Member

a water based stain that has dried is fine under a CV finish, use them all the time as well as light fast, it's generally oil based stains that are no go with CV (or AC lacquer here in UK). The sealer I talked about was just to ensure the maple is lightly sealed off and didn't go blotchy.

2/13/17       #5: White wash with sherwin williams cv ...
Shane

if you use all Sherwin based system I would do the following especially since you have a decent size run. Doing it this way would be very fast and very consistent:
Sherwood SB Stain colorant D59W85 White 200 grams with Wiping Stain concentrate clear base S64T28 200 grams. Naptha 500-1200 grams.

take this basic formula and play with the naptha ratio to use it as a spray stain... Put it in a pressure pot with a decent gun and spray several passes spraying just barely wet and overlapping strokes with gun pattern at pencil point just to where it starts to turn into a fan.. build the color to your desired opacity...... samples samples samples... come up with your formula and the approximate pass count for the panel and this will make very quick work of the whole run..
Use T67F7 Vinyl Sealer catalyzed with V66V26 at the correct rate and reduce with acetone 15% to keep the film build down, makes a quick flash to sand and topcoat with V84F90037 (What I prefer) or their kemvar water white stuff... One semi wet pass coat of topcoat... light flash and recoat within ten minutes and they will be perfect...

2/13/17       #6: White wash with sherwin williams cv ...
antonio

thank you shane, in your response you answered one of my main questions -- whether i could use the white sw sb stain. Thanks will give that a shot!

2/15/17       #7: White wash with sherwin williams cv ...
Shane

Follow up and post some results and photos!

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)