Subject: Re: Conventional vs HVLP

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Conventional vs HVLP

2/23/17       
rob

I started spraying lacquer in the early 80's in my millwork business through the mid 90/s, both opaque and clears, some pre cat and conversion. From the beginning, this was a no brainer, it was intuitive, fast, easy and unscientific. Sprayed miles of the stuff with excellent results. I used a Binks 2001 in both pressure and siphon configurations, I still have both these guns. A decade later and now doing furniture in a one man shop I invested in a HVLP setup in both pressure and gravity gun, both C.A. Tech., the gravity is a Jaguar. I haven't used either in a couple of years, but am now wanting to get back into spraying lacquer. My hvlp setup is a follows: C.A. T. Jaguar with a 1.2 tip, material is Behlen’s laquer and sanding sealer 15sec through a ford 4 cup (Right out of the can). Painfully slow with fluid wide open for a large area such as a case side or table top. I have a 1.5 tip but this seems a bit large for the viscosity. I don’t seem to be able to get the same quality of atomization and speed from the HVLP as the conventional guns. They also seem to require more fine-tuning for a given application. I do this on such a small scale I could care less about transfer efficiency among other things, just interested in ease of use and quality of finish. I am close to ditching the HVLP guns and dusting off the old Binks 2001’s… Any advice here would be appreciated.

2/23/17       #2: Conventional vs HVLP ...
Leo G

I'd use a 1.7 tip. You need to have hi flo fittings and make sure you enough CFM to use that particular gun.

2/24/17       #3: Conventional vs HVLP ...
kevin

i personally would never use a 1.2 tip for anything. I always go with 1.8 and dial it back if needed.
Why use a small nozzle that cant be opened up instead of a larger nozzle that can always be restricted?

2/24/17       #4: Conventional vs HVLP ...
rob

Thanks for the advice, I will try the larger tip. The 1.2 was recommended by the manufacturer based on the viscosity of the lacquer I am spraying. Based on what I am experiencing I'd say you two are correct. Thank you.

2/24/17       #5: Conventional vs HVLP ...
Jim Clark

Most HVLP guns spray better if you crank
up the PSI a little.

If you run higher pressure, like 70 PSI
to the gun and then regulate down with a
pressure regulator at the gun, you can
overcome the small fittings pressure
loss issues.

2/24/17       #6: Conventional vs HVLP ...
Nick

The Jaguar is a gravity gun right? when compared to a pressure set-up a gravity gun's fluid flow is slow...very slow. so if you used a 1.2 on your 2001 use a 1.7 on the jaguar to get comprable results. even at that it could still be a bit slower.
air volume is the key to good results with hvlp. so change out your connection fittings to high flow and make sure your compressor has the cfm to match or exceed the needs of your gun. Or just go back to the 2001. The 2001 is a great spray gun; pretty fast and a flawless finish.

2/24/17       #7: Conventional vs HVLP ...
Arthur grudko

Be aware that the transfer efficiency of the average HVLP sprayer is greater than 90%, and your Binks guns is around 20%. If you can afford the waste of finish and the more rapid changing of filters of the spray booth, then go with the Binks. If saving money is important, then it's worth climbing the learning curve for HVLP. If properly adjusted, the HVLP system will put out as fine a spray as the conventional.

2/24/17       #8: Conventional vs HVLP ...
Nick

To my understanding Arthur is both overstating and understating.
my understanding is most HVLP spray guns have a transfer rate in the 70-75% area and to meet the HVLP standard need to have at least a 65% transfer rate and have no more than 10 psi of air pressure at the cap. Many HVLP spray guns end up compromising speed and quality to achieve this standard. also it is my understanding conventional spray guns have a transfer rate around 30- 40%. that is still close to 1/2 as good and a good reason to go with something with a better rate. Of course it still depends on how you use either one. crank up the pressure on either one and you'll produce more overspray and of course use more compressed air.

2/24/17       #9: Conventional vs HVLP ...
rob

Your post, Nick, came in as I was beginning this reply. The research I have done on conventional vs HVLP transfer efficiency is more in line with your numbers. When I owned and operated a small custom millwork and cabined shop this would have been an important issue. As I now have the luxury of a one man well equipped shop building mostly one off furniture, not so much. Speed, ease of use and quality of finish are primary at this late stage of my career. It just seems that to get the same results, the tuning of the HVLP guns is a bit more dicey. By the way , my compressor capacity is not an issue.
I have at this point four quality guns, 1 pressure and 1 gravity HVLP (C.A. Technologies). And 2 Binks 2001’s one gravity and one pressure. So I will continue to work the learning curve as Arthur suggested to see if I can obtain the same results with the modern guns, but will put the older Binks back into use as well.
With that said. Thanks to all for the professional and useful advice I have received so far. Any further examples of setups by those experienced with this equipment is much appreciated.
Couple more questions.
I get the impression that exceeding the rated air pressure on the HVLP guns is pretty common to get better atomization. Is this the case in the field?
I work mostly in Cherry and go to great lengths to select for grain and color to avoid coloring the wood. Lately though, I have been playing with transtint dyes to shift the color slightly to blend everything in and to warm the piece up a bit until the natural aging takes over. A total of 1 teaspoon of dye combination in 12 oz thinner and 2 oz of lacquer sprayed over a washcoat of de-waxed shellac seemed to work. What would be the ideal gun setup for this.

Regards
Rob

2/24/17       #10: Conventional vs HVLP ...
Arthur grudko

Nick, I stand corrected. The savings/efficiency differences are likely not as pronounced as I thought. They are more in line with your figures.

Is there a difference between a compressor driven HVLP conversion gun and a turbine system? I have both, and seem to get more efficiency and better spray results from a turbine sprayer.

When I had a Binks Mach 1 HVLP setup with separate air pressure for the cup and the gun, I got excellent flow and leveling with minimum overspray. The set was so heavy, I gave it up for a turbine system and got the same results.

2/25/17       #11: Conventional vs HVLP ...
afinisher

I use 2 pressure pots for lacquer work. I fought with conversion hvlp guns starting in the early 90s and it wasn't till high efficiency guns came out around Y2K that I was finally ready to retire my binks 62.

High Efficiency or Reduced Pressure technology gives you the speed/material flow and atomization comparable with conventional with much less overspray. I've been very happy with this Devilbiss gun. If you look into it be sure to note you are looking for high efficiency air cap- not HVLP. The HVLP version is the same gun but with a different air cap.

Devilbiss Transtech High Efficiency Gun

2/25/17       #12: Conventional vs HVLP ...
kevin

Rob, to spray a toner such as your describing i use a gravity feed hvlp. Easy to dial in a small stripe if needed to blend in problem areas. Once you get tuned in with your equipment, it becomes an extension of your arm.

2/25/17       #13: Conventional vs HVLP ...
nick

I agree with afinisher on both counts; the devilbiss compact with the reduced pressure/transtech air cap is a is a very good spray gun ( the Binks Trophy LVMP is very similar) and I prefer reduced pressure aircaps/spray guns over HVLP ones; they are usually faster with better atomization, use less air and still deliver very good transfer rates...what's not to like?

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)