Subject: Re: Refinishing a natural lacquer job

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Refinishing a natural lacquer job

4/17/17       
Andy H

I made a bedroom suit for a customer in red oak with only a CAB acrylic lacquer finish about 15 years ago. They have decided that they would like me to tint it a medium to dark brown...or paint it.

I have used dye in lacquer before, but it was just to fine tune already stained pieces. Has anyone ever tried to tint a lightly stained (or unstained) sealed piece?

Any suggestions appreciated. There really isn't a budget for stripping down to bare wood and starting over, so I was hoping for a light sanding and going from there.

4/18/17       #2: Refinishing a natural lacquer job ...
Shane

it can be done...... clean it well with vm&P naptha first. Scuff it down with 320-400 grit. get some Mohawk M520- dyes of your choice. Mix 4 oz. of your colors/color of dye into 28 oz. of acetone. put the bed and rails together and tone it lightly and slowly build up the color with a cup gun with round pattern and low air pressure. bring the color into about half the intensity needed. Shoot a topcoat on it with your cab or nitro topcoat and begin bringing the color to it's final intensity. shoot final topcoat right over with a nice wet pass or two.... done. It takes some skill to get the gun settings right and to overlap your patterns correctly without getting odd streaks & stripes... you can do it just be even & thorough. That dye formula is pretty safe to build slowly without throwing too much color at one time down...

4/18/17       #3: Refinishing a natural lacquer job ...
Vince Member

"build up the color with a cup gun with round pattern and low air pressure"

I am working on learning a good toning technique lately..

Do you use a round pattern for most or all of your toning? Do you prefer that over a standard "oval" pattern? I have only experimented with oval so far. Could round be better?

4/19/17       #4: Refinishing a natural lacquer job ...
rich c.

You'll need to learn some new skills as well. Practice on a piece of junk furniture from Goodwill. There won't be an opportunity to "work" the color. What you spray is what you get. Overlap one surface a little more and you will see streaking. Especially difficult around moldings, legs, and small surfaces. It's way more difficult than spraying clear!

4/19/17       #5: Refinishing a natural lacquer job ...
JR

I would over glaze.

4/19/17       #6: Refinishing a natural lacquer job ...
Andy H

Shane,

Thanks for the info. I've used the Mohawk dyes before, and it definitely is pretty tricky getting an even finish. That's why I only like to use it in lacquer to do fine tuning. I'm nervous about attempt a color change to this extent.

I'm also a bit concerned about the chances of scratches peeling off the color, and exposing the light natural finish too easily. Is that reasonable?

JR,

I've never tried glaze over a lacquered finish. What kind do you suggest?

4/19/17       #7: Refinishing a natural lacquer job ...
Shane

That's why I suggest toning the color onto the piece and then locking it into the topcoats.... much less chance of the scratches/wear showing the natural color than when just adding the color straight to your clear and using it as a toner....Obviously the best way is having color laid down on raw wood but you said no money in it for full refinish... You can bring the color in evenly with mouldings and radiused areas.... the trick is not going to far too fast... multiple passes with weak color is the answer..... I work for a full custom commercial millwork company. I have eight open faced booths shooting ten hours a day adjusting with dyes to get everything they shoot spot on with their control samples...We have all different shapes and sizes.. trim.. flat wall panels.. cabinet doors, entry doors, reception desk... low walls..Entry doors you name it. In the end it all has to match the approved color we have signed off... by the time we buy and lay up skids and stacks and stacks of veneer to make panels it all varies in color a bit and the basic finish recipe is only a starting point.... the end result is a control sample in that finishers hand and his ability to see color and make changes. does it need red, green, yellow,, more brown green, more red green.. a blue black, a green black
?It's all about knowing your colors and their strength.. if it's wrong or too dark it gets washed down and we start over.... period. you just have to approach it cautiously and without guns a blazin'....

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)