Total Finishing Supplies

Professional Finishing

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Off Gas

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Off Gas

8/9/17       
WCW Chris Member

Website: http://waukeecabinetworks.com

We have been spraying in a building bay for over a year but we just recently got our spray booth and exhaust fan functional. It's a booth with a wall of (35) 20"x 20" filters. We have about a 24" diameter exhaust fan. We spray SW conversion varnish. Now that we are fully functional we have a lot more off gas when open the bay in the morning. It's almost like tear gas walking in there. We suspect it may be coming from the filters? Do we need to concerned that it's flammable? We plan to add heaters for winter.

8/9/17       #3: Off Gas ...
Leo G

Ya, the filters will hold the smell. It's just the solids that get caught in the filter.

I'm sure it's flammable, the filters themselves are flammable.

8/9/17       #4: Off Gas ...
al

This is somewhat relevant to your post. I have an outbuilding that after I spray I let parts sit in there for a few days until everything off gases. Seems to work fine
in spring, summer, fall. The building has no heat. If I spray and let parts cure for 4 to 6 hours at 70 degrees will it hurt putting parts in outbuilding in lets say January? Located in North NJ.
I know what you mean when you say CV is like tear gas, my eyes water when I'm around the parts that have been sprayed the day before.
Thank you,
Al

8/9/17       #5: Off Gas ...
Leo G

CV needs to be above 65º for the whole cure period or it won't cross link properly.

8/9/17       #6: Off Gas ...
rich c.

You sprayed conversion varnish for a year with no spray booth? Holy crap! Good luck with your health in the future.

8/9/17       #7: Off Gas ...
nick

chances are what's making your eyes burn is the formaldehyde out gassing, which means your using SW's waterwhite CV or using catalyzed fast dry vinyl sealer or both. If so you may want to try SW's F3 formaldehyde free CV; it dries faster, sands better and feels smoother than the waterwhite and of course has no formaldehyde for you or your customers to breath...that said on the down side it's a little less tough and it still out-gases something noxious for 24 hours or so...but it's not near so bad as the waterwhite.
And Leo is right above 65 degrees for the full cure period which I believe 24 hours for both of SW's CV products.

8/10/17       #8: Off Gas ...
Adam

24" fan is small for most booths unless its high volume. You may not be pulling the last remaining fumes out of the booth. I like to let it run for atleast 10 minutes after I stop spraying. I think it helps with drying, keeps the dust off the product.

Also notice the overspray that is hitting the walls of the booth. Without enough fan it may tend to collect on the walls.

8/10/17       #9: Off Gas ...
JM

We have an 8x10 open face booth and we ordered it with a VFD so we have speed control. When done for the day, we turn it down to low and leave it running for the night. Next morning, cant tell anything was sprayed. The smell is not just from the filters, its off gas from all the sprayed parts that are curing.

Sounds like its a home made spray booth. If so, in addition to the 24" fan. add another smaller fan that you could leave running all night to continue to evacuate fumes from curing, or if possible add a speed control to your 24" fan so you can just turn it down for the night.

8/10/17       #10: Off Gas ...
chris

buy yourself a dwyer vaneometer. about $35
you can measure the air speed in your booth.
You want 100 feet per second.
i think your fan and ducting is too small.
my booth has 16 20x20 filters with a 24" fan and duct.

8/10/17       #11: Off Gas ...
Leo G Member

100 feet a second? He'd be sucked up to the filter wall LOL

100 feet a minute.

8/10/17       #12: Off Gas ...
Bart

Nothing like a face full of formaldehyde in the morning. I like JM's idea of a low speed exhaust fan overnight. And store in a well ventilated area until you deliver to the jobsite. Switching to WB was the best thing I ever did.

8/11/17       #13: Off Gas ...
Adam

The only thing worse than wearing a respirator when spraying cv, would be sanding cv the next morning wearing a respirator.

The 36" belt driven fans allows you to control the speed of air much better. It pulls more air at a lower fan speed from a larger wall area so you get much better ventilation. Its adjustable by simply changing the pulley's.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)