Total Finishing Supplies

Professional Finishing

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: white stain on oak

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

white stain on oak

9/3/17       
dar

doing a white stain on oak, usually use mohawk stain, but need a recommendation for a heavy stain that covers more, the mohawk white is too thin , also must be fast dry thanks

9/3/17       #2: white stain on oak ...
Robert Member

Have you considered making up your own stain ? Some Titanium Dioxide and paint thinner is all it takes. You can make it as strong as you like. If you want it to dry faster you could use Naphtha instead of Paint Thinner.

Are you staining White Oak ? Red Oak will end up looking Pink with a White stain.

9/3/17       #3: white stain on oak ...
rich c.

M L Campbell Woodsong II

9/3/17       #4: white stain on oak ...
Robert Member

" ML Campbell Wood Song II " is no doubt a decent product. A brief look at the M.S.D.S shows it contains some solvent....some Titanium Dioxide.... some Linseed Oil....some other solvents.

In other words, nothing special, except of course the price. Those ingredients can easily bought at any Hardware Store, Paint Store and will cost wayyyyyyyy less than any brand name of stain.

9/3/17       #5: white stain on oak ...
JeffA

I agree with rich c. It's one of the best ones I have used. And you get what you pay for. Sometimes. ;.)

9/4/17       #6: white stain on oak ...
Tyler

Chemcraft Frost 825-9101 is a pretty heavy white, I use it pretty often

9/5/17       #7: white stain on oak ...
dar

it is white oak, not interested in making my own, it is a large job and saving a couple bucks is not worth it, does chemcraft stain dry fast and can you spray shade with it. thanks

9/5/17       #8: white stain on oak ...
Tyler

It dries quickly, im not sure what you mean by shade? do you mean toner?

9/5/17       #9: white stain on oak ...
Bart

You'll probably need to do at least a couple of coats to get to where you want to get to. I use GF's water base RTM.

9/5/17       #10: white stain on oak ...
rich c.

I'm trying to make money Robert. It's very easy to add the cost of a gallon of stain to a job. It's not easy to calculate how long it would take to mix up a product and experiment with the amount of pigment and percentages of solvent. It might save the customer $50 on a $10,000 job, it won't save me anything.

9/5/17       #11: white stain on oak ...
Robert Member

Hi rich c, after 35+ years as a finisher I retired in 2015. Making money has always been a major priority be it as the Proprietor or as an Employee. Ive never bought any type of pre - mixed stain, always mixed my own and kept a formula.

Not knocking any store bought stain but I have complete control by mixing my own.
An issue I can see with a store bought stain is what if isn't as "strong in depth " as I would like it to be ?

Gallons of pre-mixed stain can cost upwards of $ 70.00. dar is staining White Oak with a White stain, its not rocket science to mix up a home brew if one is inclined to.

The major suppliers spec sheet for a White Stain, all contain pretty much the same ingredients. Their MSDS indicates... a Solvent or two, a Color and some Linseed Oil.

Since dar has expressed an interest in purchasing a pre-mixed White Stain; lets wish him the best ,and look forward to seeing some photos of the completed project.

9/5/17       #12: white stain on oak ...
dar

Tyler, a shader is when you spray stain after you have stained and sealed, I cut stain with lac thinner and spray with a good touch up gun then lacquer. On this project you can barely see wood, i have to do 45 doors and frames so doing this has to do be very production like in order to make money

9/5/17       #13: white stain on oak ...
Tyler

Oh, well if I was doing it, I'd do a clear seal.coat, then two washcoats of white topcoat. Reduce it 50% and you get the effect you look for. Hit it with a clear topcoat and you're in business. More consistent color than stain anyways

9/6/17       #14: white stain on oak ...
kevin

i agree with tyler. in this situation i would use reduced paint. you can add a little clear coat to the white paint to give it slight transparency.
Using wiping stain reduced with lacquer thinner as a "shader" over sealer is begging for finish failures. The oil in the stain will prevent the adhesion between coats.
You may have gotten away with it a time or 2, but definitely bad practice.

9/6/17       #15: white stain on oak ...
Matt Calnen

Sound to me like you might want to try a coat of white vinyl sealer. Then clear topcoat. It lets some of the color of the wood through, and doesn't fill the grain. Just a thought

9/7/17       #16: white stain on oak ...
dar

kevin i have been using shaders for 30 + yrs
without any problem, you have to use quick dry stains like mohawk, kitchen cabinet factories and furniture manufacturers use this process

9/7/17       #17: white stain on oak ...
Robert Member

Hi dar, since the look your after is rather Opaque than transparent, would it be more productive to go a different route similar to the ones mentioned by Tyler/kevin/Matt ?

I see the possibility of eliminating that shading step you would be using to intensify/deepen the overall color by switching to a White Vinyl, White topcoat, etc...

Any chance you could post a picture of the look your after ?

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)