Total Finishing Supplies

Professional Finishing

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Exterior Door Stain

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Exterior Door Stain

10/3/17       
John Member

What brand/type of stains are you all using for an exterior front door? I've never had to stain/clearcoat an exterior door - until now, so I'm interested in your experience and recommendations. If it matters, the wood is probably going to be rift sawn white oak for the frame with plain sawn panels. And my preference is a waterborne topcoat, something like Target Coating EM9300. Thanks.

John

10/3/17       #2: Exterior Door Stain ...
rich c.

I am no fan of clear film coatings on exterior doors. Just ask any wood boat guy, it takes a ton of maintenance. Likely to be sanded and refinished every 3 to 5 years based on locale and sun exposure. I'd wager, you will be the first person they call when the film starts to crack and let moisture get under it. Personally, they couldn't pay me enough to do that job.

10/3/17       #3: Exterior Door Stain ...
John Member

This door is behind a storm door on a covered porch. It gets direct sun for a couple of hours some days on the bottom third. The existing flat veneered wood door was last refinished by an amateur using BORG stain/varnish about 15 years ago and shows only minor degradation where the sun hits it.

John

10/4/17       #4: Exterior Door Stain ...
Leo G

I've used the EM9300 on an exterior door and it performed very well. You need to put it on thin and many coats. It calls for 2-3 wet mils or it'll go blue on you. The door I did I put on 5 coats. As for stain, you probably want something with a metallic pigment, stable and reflects UV

10/4/17       #5: Exterior Door Stain ...
RobertJ

A word of caution. A Wooden door behind a Storm door( I assume a full view glass door) is not a perfect scenario for keeping the door from feeling the effects of heat during the summer months. Tell your client to remove the Storm door.

10/4/17       #6: Exterior Door Stain ...
John Member

Thanks Robert. I'm aware of problems that occur with a storm door over a wood door. In this case, the storm door was installed 8 - 10 years ago. The finish was last redone about 15 years ago with low end products and still looks pretty good other than the degradation (oxidation) where the sun hits it directly. The door is still flat, with no evidence of the veneer splitting or cracking. I think the new door will be OK with higher end finishing products. If I'm wrong we can always remove the storm door.

John

10/5/17       #7: Exterior Door Stain ...
Jonathan Mahnken

General finishes has a complete water based exterior stain/clear coat system for this. I did a mahogany entry that is east facing with an overhanging porch and its still looking good five years later.

10/5/17       #8: Exterior Door Stain ...
John Member

Thanks Leo. That gives me some confidence the EM9300 will stand up well.

John

10/5/17       #9: Exterior Door Stain ...
John Member

Thanks Jonathan. From what I saw in their literature, GF's line of exterior stains is pretty limited, although I'm sure I could custom blend them to extend the range. Normally, I use mostly GF products, and I might this time as well, but I'm looking to see what other systems people are using and how they have performed.

John

10/5/17       #10: Exterior Door Stain ...
Jonathan Mahnken

You can call them and or send a sample and they can make a custom color in their exterior formula

11/3/17       #11: Exterior Door Stain ...
John Member

What a disaster the EM-9300 was. Bubbles large and small, even when I dripped some off the stirrer onto a clean piece of glass and spread it out with a razor blade. And it bridged around the pores in the sealed white oak and looked terrible whether I sprayed light, medium, or heavy coats. Lots of correspondence with Jeff Weiss at Target Coatings, who was very nice and very helpful. He refunded my purchase and replaced the product, which was very generous (except it can't cover the lost time and rework), but I asked for EM-6000 instead. I doubt I'll ever give EM-9300 another look. I ordered some GF Exterior 450 and just sprayed the first coat today. What a difference. Flat, smooth, no issues at all.

The EM-6000 arrived today and I sent the remainder of the EM-9300 back so they can hopefully find out what was wrong with it.

John

11/15/17       #12: Exterior Door Stain ...
Ed Arthur Member

Website: http://doorsbyinvision.com

The main thing to consider when doing an exterior stain is not to us dye stain that will fade easily. I’ve never heard of metallic based pigment. I use linear polyurethane on the doors I refinish and it works great.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)