Total Finishing Supplies

Professional Finishing

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Fisheye question

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Fisheye question

8/14/18       
Kevin Member

Wondering if anyone has ever come across this. Looks like fisheye but with a tiny dust spec that may be causing it. Happened in two colors of CV over primer, so maybe its pump/hose related? Or something airborne?


View higher quality, full size image (1512 X 2016)

8/15/18       #2: Fisheye question ...
Jon Member

Interested in this as well. We are seeing this from time to time.

What material are you using? We are are using Matador and Innovat for clear. Colors show it worse than clears, but I believe it is present in the clears as well.

My thought is something coming from the inside of the pump, or falling off the outside of the gun/hose. We have a line heater that could be holding some contaminants.

8/15/18       #3: Fisheye question ...
Shane

Many a finisher has lost sleep racking his brain on exactly why this happens.... Sometimes I have found the answer but 90% of the time you never really know what causes it... Do your inner well being a favor. Lick your wounds and move on. Best thing to do is just clean/flush your equipment well... check your regulator filter bowls from your main air supply line for rust/oil/contaminants. If you've introduced new grooming products to your own personal routine go back to what you were using. Most deodorants contain silicone for that nice smooth feeling when you apply it.... On hot sweaty days those lotions and deodorants will multiply like bacteria and work their way all over your skin and equipment... I have a long story about how I eliminated a fisheye problem in one of my operators booths... short story we had the problem for days and after process of elimination we found he had been using his old ladies deodorant all week.

8/15/18       #4: Fisheye question ...
Kevin Member

Thanks. Using chemlife 24 primer and topcoat. Happens with two pumps. I checked my first stage of filters and the oil coalescer is trashed. Hopefully replacing that may help. Also somewhat recently purchased a new to me compressor, really hoping its not piston rings or something. Bought new fluid lines and still happening.

8/16/18       #5: Fisheye question ...
Adam

If its from the system(gun, hose, filter) its usually more consistent and frequent.

The random bit of garbage that ends up occasionally in one coat is simply something one deals with from time to time.

If it happens with any kind of consistency its time to have a complete look at all possibilities.

I would guess its a particle of something the finish didn't like. Surface tension collapses.

8/16/18       #6: Fisheye question ...
Jim Clark  Member

I have found straining the finish with a
really fine strainer catches a lot of stuff
the paint strainers miss. And that fine
dirt can cause that.
I got a metal fine strainer off Ebay that I pour
all my finishes through and it has made a
huge difference.
It cost me a dollar and I just rinse and reuse it.

8/17/18       #7: Fisheye question ...
jmace

looks a speck of oil, likely from a worn seal. It'll get worse.

9/14/18       #8: Fisheye question ...
Scott

The cause of fish eyes is usually some kind of contamination, it can be like finding a needle in a hay stack as others have mentioned.
I ran into a guy many years ago who had his own finishing shop for ever and then the supplier hired him because he knew so much. He worked for ever with that company and learned a ton more from the suppliers.
He said the biggest culprits of fish eyes, are dirty fingers and dirty air. Cleaning dirty fingers is fairly easy, dirty air not as easy. You need a good supply system, preferably without using black pipe as it is full of rust and oil. You need good filters and dryers, to clean your air. He said one shop they tried everything and still had some contamination, it turned out it was coming from one of there $5 air blowers that they blew off their parts after they sanded. It had some silicone or oil or something in it.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)