Total Finishing Supplies

Professional Finishing

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: quilted maple

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

quilted maple

1/20/19       
Eric Smith

I am making a 42" x 84" wood penninsula counter out of some very nice 8/4 quilted / curly maple. To pop the figure I'd normally sand to a high grit, put on BLO and then a high gloss finish. But would like it to have a soft warm bit of distressed / antique look. In more of an antique pine color, or at least more warm than the clear. And maybe more of a satin gloss?

Is it possible to have the best of both on this? Pop the grain and color with some technique with dye and BLO? Ding it up a bit for the distressed look and use some dark brown glaze in the dings and edge detail? Will the satin gloss still show the pop on the grain?

Do any of you experts have any suggestions or comments?

Thanks!

Eric
eric@woodsmiths.biz

1/20/19       #2: quilted maple ...
rich c.

I'd check, there may be a law against distressing quilted maple by "dinging it up a bit". There would be around my place!

1/21/19       #3: quilted maple ...
Shane

agreed......Figured maple distressed would be an abomination...lol

1/21/19       #4: quilted maple ...
David R Sochar Member

Agreed, but there is nothing like an older piece of wood that one examined, shows exceptional grain or other characteristic. A smooth, satiny piece of Quilted invites touching. Even rubbing. Watch people interact with it if you get a chance.
Glossy wood things look like plastic and are so shiny that people are afraid to use them.

1/21/19       #5: quilted maple ...
Eric Smith

My thought exactly. This is not a showpiece but a kitchen peninsula counter. Wants to be warm, friendly and inviting.

1/21/19       #6: quilted maple ...
David R Sochar Member

The nice part about low tech finishes (none?) is that they are easy to renew. If you watch, people will always gravitate to the table with the old wood showing - rings, dents, gouges, lack of obvious color and coating. The high tech table may get the wows, but the obvious natural wood gets the use. It makes people comfortable.

1/21/19       #7: quilted maple ...
John L

Try hand scraping which should provide enough character, treat with Aqua Fortis, then pop color with BLO, and clear finish of choice. For a more authentic clear finish you could even use a beeswax infused tung oil such as Millie’s All Purpose Oil by Sutherland Wells.

1/23/19       #8: quilted maple ...
Mat

I've done this before on curly maple, basically the same process you are talking about.

I prepped the wood surface with an orbital sander up to 220 grit.

Over the course of a week, I'd apply 1 coat of thinned boiled linseed oil (thinned with mineral spirits about 30%) and use that solution to wet-sand, by hand, in the direction of the grain.

Each day I'd step up in grit, 220/320/400/600.

In all honesty it may be overkill but it was fun, and the final product had a more vibrant curl than anything I've ever seen.

I cured the linseed for a good week after that, scuffed GENTLY with the grain with 320, and put two light coats of satin-sheen polyurethane on it.

By the way, you referred to "satin gloss"--- those are two different terms. It's either satin, or it's gloss.

Gloss is forbidden on nearly anything I make--- it turns everything it touches into cheap plastic looking sillyness. Satin is the highest sheen I would normally use.

1/23/19       #9: quilted maple ...
Shane

Please post pics when your done or during the process as well..... It does sound like a fun project your working on. The bulk of us don't see center pieces with nice tops as often as we'd like... Gets old with working with the same old stuff all the time... Sometimes I see mahogany for months and months on end with large commercial projects.

1/23/19       #10: quilted maple ...
rich c.

Mat, must be tough getting the customer to wait that long and accept the cost for a countertop. Two weeks and all that labor for the finish?

1/31/19       #11: quilted maple ...
Matt

Rich, it all depends on the market you're in and you client, and how you run your shop.

When I did the finish listed above, I was at a shop that had no trouble doing that sort of thing (although it was NOT the norm), and it isn't as laborious as it sounds reading it on paper. On a 26X96 countertop, it would take maybe an hour each morning (max) to wet sand it and leave a slight linseed slick on it. The worst part is having it sitting around.

You are right, it is tricky, you could drown yourself in it if that's the only sort of project you took on.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)