11/27/16       
Norm

Help! I just completed remodeling a stair case for a customer, He was responsible for the hiring and execution of the finishing process. The painter he hired came in and stained the treads and then proceeded to apply a topcoat without ever sanding other than to hit them with a sponge sander. Obviously, the treads look awful and the homeowner is blaming me for not sanding the treads. In over 50 jobs like this, it's always been the painter/finishers job to do the final sanding. Also, my understanding has been that once he applies any finish, he's responsible for any issues. can anyone lead me to a written code or ethics guide that will clear this up?

11/27/16       #2: finishing dispute ...
Dan

Painter is responsible. He is in charge for the next steps to complete the job.
If you took a dirty car to get painted and the body shop just painted without cleaning or prepping it, it would be his problem. I'm sure we'd all agree it's the body shops responsibility. Same as in your case.

11/27/16       #3: finishing dispute ...
nick

once the painter applies any coating they have accepted the surface as ready for finishing and the responsibility for the outcome.
That said in my neck of the woods (So.Oregon/No. California) the woodworker is responsible for the white wood finish sanding, so if it's rough or full of RO swirls I'm on the phone to inform them of the condition of the project and the cost of getting it right before I start any finishing.

11/28/16       #4: finishing dispute ...
Norm

Nick...what is the "whitewood" that you refer to? The stairs in question are red oak.

11/28/16       #5: finishing dispute ...
Nick

It's my understanding that 'white wood' just refers to any wood after fabrication but before finishing.

11/28/16       #6: finishing dispute ...
rich c.

If there is nothing in writing between you, the owner, or the painter, then no one is wrong or right. The history and your explanation is just based on assumptions. So it will be purely negotiations now. Depends on who flinches first, and if no one does, get a lawyer.

11/28/16       #7: finishing dispute ...
Robert Member

In the Cabinet Shops I have worked in, the Cabinetmaker does a sanding of the completed cabinets. Some do a real fine job and others would just do a belt sanding with 100 grit and call it a day.

Also, in the Cabinet Shops I am referring to, the Foreman in those various shops would make sure the Cabinets were presented to the Finisher in a ready to finish condition, OR they would say that the Cabinet Makers do a quick sanding and the Finisher does the final sanding.

Its pretty normal for the Finisher to do some raw wood sanding, the product may have been scuffed/marred/scratched or dinged as it was being moved from point A to point B.

With that said, if a product came to the Finisher with badly cross grain scratches left over from a belt sander or giant swirl marks left by an orbital, its wise to ask the Foreman if they wanted the Cabinet Maker to re-sand them OR would they prefer that the Finisher stop what their doing,slow down the work flow and sand the Cabinets themselves.

In the case of finishing stair parts, I think the builder should do a careful sanding with say..100 grit, maybe following it up by sanding with the grain with 120 grit. The painter should then do a final sanding to get the parts ready to stain/clear coat.

On a side note Norm, a Wood Finisher approaches the finishing of a piece of wood differently than say a Painter does.
Some Painters go the extra mile and some just geterdone no matter what.

Any way you can post some photos ?

11/28/16       #8: finishing dispute ...
Leo G

The finisher is responsible to assess the wood before they apply any stains or coatings. If they find them unacceptable then they either need to stop immediately and report or never start in the first place.

Sometimes it's difficult to see a not great sanding job until the stain is applied. But you don't go and stain the whole stair system knowing that it looks like crap and then expect to blame the guy before you. It's absolutely your responsibility to stop the work if there is a problem.

11/29/16       #9: finishing dispute ...
RobertJ

Agree with Leo! The Finisher is now responsible for the final product. Once he/she accepted to commence the work, they own it and end of story.

11/29/16       #10: finishing dispute ...
dean c

agree with Leo.
the finisher has an obligation to insure the wood surface is ready for finish before any stain or sealer goes on.
if the finisher sees that the wood surface is not ready for finish, he/she should kick it back to the woodworker, or get it ready himself.
Ideally the woodworker/cabinet maker hands off to the finisher in a fully prepped state- meaning no machine marks, no glue spread, no puttying required etc.
Still, the finisher cannot proceed with an inferior/unprepped surface and blame the woodworker.
once they start on it, they own it.

11/29/16       #11: finishing dispute ...
doug mclaren  Member

happens all the time. your shop gives a realistic quote for finishing including sanding thru the grits ,cleaning , staining , seal, clear. customer freaks and says hell my painter will do it for 1/3. and of course you say well, i will remove machine marks, and prep before finishing is on you. they get what they paid for, and blame you . partly because they dont want to admit they re the ones to blame. but, your position should have been stipulated in contract.

11/29/16       #12: finishing dispute ...
Norm

To all the great responders here. thank you for your input! Yes, I agree that I should have been clearer in my quote about the sanding issue. My problem is that I used to contract the trim in high end homes in Tennessee & Florida, and this never came up as an issue. In fact, all the painters that I worked with preferred to do all of their own prep thereby ensuring that they had control of the quality of the finish.This is the first job of this sort I've taken since moving to Alabama, and boy do I regret taking it! From now on, I'm staying in my shop doing what I love, building custom furnishings and working with reclaimed wood!

11/29/16       #13: finishing dispute ...
rich c.

I'm thinking prep of stair treads and risers is way easier before installation. With all the inside corners, getting a good preliminary sanding job is almost impossible after installation.

11/30/16       #14: finishing dispute ...
John B Member

As a custom builder/contractor for over 30 years, while also operating a small cabinet shop, I'll chime in. I've built my share of custom stairs along with a host of other built-ins and I would always leave the product sanded to the point of being ready to accept a finish. That being said, I would also expect that my painter would touch up sand any part once installed as even the best situation, during installation and the time until painting, it is exposed to the jobsite full of other workers and installers. Once the painter noticed a problem in this case I think he is absolutely required to either bring it to the attention of someone or stop until further notice. What exactly is the issue, cross grain scratching, etc.?

11/30/16       #15: finishing dispute ...
Norm

John B. I think the main problem is that the customer hired a lousy finisher. I sanded all the treads as I installed them. What I saw in my brief look was splotchy spots, many looking like the stain was applied unevenly and left to sit too long. They were using a dark walnut MinWax, which in my opinion, is a terrible stain and should only be used with a conditioner. But, I've hired a lawyer and we'll see how it all pans out. If I was the homeowner, I'd make him pay to have a professional hardwood floor finisher come and do a complete refinishing job.

11/30/16       #16: finishing dispute ...
Robert Member

Hi Norm, can you post some photos ?

12/5/16       #17: finishing dispute ...
John

Yep, same old story. Builder is responsible for handing over a sanded product, but the finisher is responsible for making it look good. If I were installing primed baseboards, I wouldn't sand them afterwards. That's the finishers job.

12/5/16       #18: finishing dispute ...
dean c

Norm:
Just wondering...what wood were the treads fabricated from?

12/5/16       #19: finishing dispute ...
Robert Member

I'm not Norm,dean c, but the wood in question, according to Norms reply on 11-28-2016 is Red Oak.

12/5/16       #20: finishing dispute ...
dean c

Thanks Robert. I missed that!


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)