pigmented cv over raised panel doors

3/9/17       
antonio

Website: http://positivewoodworks.com

We have been doing shaker doors for so long now using a 1/4'' mdf center panel that its been so long since being asked to build raised panel doors. Any of you finishers had any issues with your pigmented cv where the raised panel planks are joined together? Im thinking of using 5/8'' mdf for this but just incase the client insists on using solid maple.

3/9/17       #2: pigmented cv over raised panel door ...
Shane

My $.2 cents An Mdf raised center panel out of medex will yield a better finished product for paint... no telegraphing from solid glue up and it's going to move a lot less with temp/humidity changes.... Cut your centers to size and prime them very well first to seal the panels edges. you can even tint your primer close to the final color will help if the panel shifts a bit later. build your stiles and rails and sand your doors flat.... Reprime the whole door to prep for topcoat... bam.... sand that bad boy and bondo/spot fill imperfections and hang them for topcoat... Perfection. Only trouble spot is the groove for the panel is the only spot not sealed but most don't dig that far into quality. but if all areas were sealed with a catalyzed primer it would be darn near perfect moisture barrier.

3/9/17       #3: pigmented cv over raised panel door ...
antonio

thanks shane, so your suggestion would be center panel mdf but stiles/rails solid wood correct?

3/9/17       #4: pigmented cv over raised panel door ...
Bart

I've done finish work for a cabinet shop that used MDF raised panels. They primered the cove detail etc where it exposed the more porous interior. Then sent it through their wide belt to clean up the face before gluing up and then delivered to me for finishing.

3/10/17       #5: pigmented cv over raised panel door ...
Adam

We've built a couple of thousand raised panel cabinet doors. We have been using mdf panels exclusively since the early 1990's. They make better doors.

The trick to finishing mdf is to use ultra refined(less porosity). Sand the raised edge to 240. Use a brush to spot prime the edge with a sealing primer. BIN shellac works well in most cases. It drys in 15 minutes. Some people use cat. primer to spot under cat primer. Let the edge cure. Sand it smooth with 320. Spray the whole panel or door with primer.

We use soft maple for stile/rails 5/8" ultra refined mdf for panels.

3/12/17       #6: pigmented cv over raised panel door ...
Alessio

Not sure if they have them in your area, but we get two piece mdf doors here, and even for shaker they can do a 5/8" thick center panel if you want that solid/heavy feel to the door.

However, the frame is one piece (but inside corners are square), which means there will never be any joint movement/hairline cracks, and the center panel gets glued from behind and creates a tight seal to the frame. beautiful doors, and we are here in Canada where humidity goes from 10-90% and no issues

3/13/17       #7: pigmented cv over raised panel door ...
Mike Fuson

We do it like Shane, done a bunch today matter of fact. Stiles and rails are soft maple, 5/8 mdf for the panel. Get a good door quality mdf, the porous stuff is crap. Raised panels are taken straight from the shaper and get a coat of primer on the profile. Then scuffed with 220. We use space balls in all our doors.

3/14/17       #8: pigmented cv over raised panel door ...
antonio

thanks shane do you use medex mdf or another type of water resistant one?

3/14/17       #9: pigmented cv over raised panel door ...
antonio

sorry my last msg was for mike, i see shane uses medex but was also curious if mike does.

3/14/17       #10: pigmented cv over raised panel door ...
Mike Fuson

To be honest I don't know what it's called. I can tell you that the porous mdf is dark brown and the good door quality stuff that I use is light brown.


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)