11/8/17       
Matt

We have a job coming up that we need to replicate the look of "old white painted stuff that was stripped and clearcoated"

Part of that process will involve using a 2-4" wide brush with white conversion varnish applied to the face, in THIN streaky brush strokes. Somewhat to replicate paint "in the grain".

I can do this easily with common chip brushes but they donate their bristles too easily to the substrate.

Since these brushes will quickly foul up from dried material, I'm looking for what you folks suggest for affordable disposable brushes that won't lose it's bristles into the paint.

Basic process will be the brush on the light coat of white over "most" of the wood surface. Scuff gently and topcoat with 3 coats of clear (sprayed as usual).

Thoughts?

11/8/17       #2: Best brush for conversion varnish? ...
Robert Member

Hi Matt, sounds like an interesting project. Have you considered a rubber graining comb for the application?
Can you post some photos of the look your after?

11/8/17       #3: Best brush for conversion varnish? ...
Rick Mosher

You might consider a metal graining comb.

11/8/17       #4: Best brush for conversion varnish? ...
Matt

I did think of a graining tool and it's on my short list of other things to try, but I'm not sure I can get a graining tool properly into the profiles (this job has a huge amount of profiles, carvings, etc) and we'll end up needing to do at least some brushing.

However, since you guys are suggesting it, I'll pick one up and try.

11/8/17       #5: Best brush for conversion varnish? ...
Matt

Rick, I haven't used the metal graining combs but those do look useful. Thanks for suggesting it. I just looked them up and like what I see.

11/8/17       #6: Best brush for conversion varnish? ...
Leo G

I would do it with the primer myself. Thin it out and use lots of retarder. Brush it on quick and have a pot of retarder to dip the brush in occasionally to clean it out.

You can keep brushing until you get the desired texture, keeping it a bit rougher than you'd like the finish product to be. Then you can spray coat the topcoat.

11/8/17       #7: Best brush for conversion varnish? ...
Matt

Good idea Leo.

Can anyone recommend a brush? I really like the coarse texture of the wood handled chip brush throw-aways but I'm hoping to find something that wont' tear apart so fast but also isn't $15 each.

11/8/17       #8: Best brush for conversion varnish? ...
Leo G

I was using a Rembrandt 2 1/2" sash brush which has PBT Filaments for bristles. Some kind of synthetic. It did very well with the 2K poly I was slathering into Oak to try to grain fill more effectively.

Don't remember how much it was, under $20 I think. But I've cleaned it up many many times and it's still in good condition.

Just remember to clean while using so the CV doesn't get packed into the bristles.

You get what you pay for. And those disposable brushes are worth exactly what you pay for them.

11/8/17       #9: Best brush for conversion varnish? ...
chris

are you concerned about total thickness?
3 coats and the white?

11/8/17       #10: Best brush for conversion varnish? ...
Matt

Yes, you should always be concerned about thickness with conversion varnish.

The three coats of clear we spray will be thinned enough to avoid exceeding the maximum dry mil, which I believe to be 4-5 mil on our product.

11/8/17       #11: Best brush for conversion varnish? ...
Mike

Maybe try putting thin CA glue in the heel of the brush. I do this with cheep acid brushes for glue and it keeps most of the bristles intact. Add a second coat for safety on a finish job like yours.

11/8/17       #12: Best brush for conversion varnish? ...
Robert Member

I suggested a rubber comb for a couple of reasons. They have a chiseled tip. They come in a variety of grain sizes and can be used on round or irregular surfaces. You can easily slit each comb to create finer brush marks. They wont scratch a finish. The rubber ones are easy to manipulate to achieve various looks.

11/9/17       #13: Best brush for conversion varnish? ...
Matt

Mike, funny you should say that. In experimenting, I found that the chip brushes work a lot better if you actually DO cake them up with some dried conversion varnish. They don't dump bristles as much. The CA glue would be a great way to hit the ground running.

Robert, I'm going to order some of these graining brushes, even if we don't use them on this job, I think they could be a really useful tool for some other stuff we do.


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)