Finish Adhesion using hand planes

10/1/18       
Gordon Fowler Member

I would appreciate references on the use of hand planes and finish adhesion.

I build custom furniture and teach furniture finishing. At a recent workshop a nationally known woodworker stated that a hand-planed surface provide good surface adhesion without resorting to sandpaper. The research and the opinion of most professional finisher does not support his position but when I re-review the literature I could not find any studies that tested adhesion using hand planes; mechanized planers yes but no hand planes.

10/1/18       #2: Finish Adhesion using hand planes ...
Matt

You're probably not going to find many tests on this because it's going to vary a lot--- so many variables here.

People vary significantly in their ability to keep a plane sharp, used at the proper angles/methods, etc. Those all are going to effect the adhesion of finishes, and that's going to vary from one finish to the other.

And obviously that will also vary from one wood to another, and one grain pattern to the other.

Personally I would not have any problem at all making a gentle pass with some 180 grit just to give a tiny scuff to the raw wood surface for finishing.

If this is an oil finish, there shouldn't be any trouble at all.

10/2/18       #3: Finish Adhesion using hand planes ...
rich c.

A properly sharpened hand plane leaves a surface with very clean, open pores. Sandpaper will give tooth to the hard grain, but also leave slightly closed pores since it was not as cleanly cut with the abrasive. I vote for good adhesion after a hand plane. I doubt if all the finish fell off hand planed furniture before sandpaper was commonly available.

10/2/18       #4: Finish Adhesion using hand planes ...
CWWOODWORKING

Gordon, where do you teach at?

10/2/18       #5: Finish Adhesion using hand planes ...
Adam

Depends on the finish. Penetrating oil finishes require no abrasion. They soak into the wood.

You will be hard pressed to find any company that makes film finishes which would say its ok. Most finishes require 240 grit at the very least for mechanical bonding to a substrate(typically 120-240). Even between coats the manufacturers recommend 240-320 grit. Some of the waterborne finishes can get away with 400-800 grit between coats.

In other words the vast majority of experienced finishers would say no.

10/2/18       #6: Finish Adhesion using hand planes ...
DannyB Member

I think there are a lot of factors here - the wetting characteristics of the finish, etc.

I was gonna pull out my little 300x microscope, and see what i would see, but it turns someone did one better:

If you look, you'll see they put drops of water on it, and also examine it under a powerful microscope.

While it's true that a handplaned surface leaves very clean, open pores (and this is obvious) , you can also see what happens when they put a drop on it: The smoothness and cleanliness of the surface causes it to become hydrophobic.

This is not entirely surprising given the relative size of the pores in most wood vs finish molecules/etc.

I think the conclusion is pretty obvious:

1. Closed grain wood - handplaned is a really bad idea.

2. Open grained wood - Still seems like a bad idea given what the video shows, but maybe an okay idea with big enough pores.

I think the TL;DR is also: This is not going to provide surface adhesion, the person is pretty wrong (and doing a little science would have shown them this).

10/2/18       #7: Finish Adhesion using hand planes ...
mauricio poli Member

Fantastic video, DannyB
Thanks a lot, very good to teach our people here.
Hugs for everyone

10/3/18       #8: Finish Adhesion using hand planes ...
Gordon Fowler Member

DannyB, thank you! What a perfect teaching video.

Gordon


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)