We aren't yet committed to switching to post-cat polyurethane but it has several advantages over conversion varnish that we like (low/no odor to the client, exceptional durability, very elegant look/feel).

My main concern is safety and health. Obviously we provide our spray team with vapor masks and optional disposable plastic suits, and the whole spray booth area has plenty of fresh air flow.

I'm aware of the offgassing of isocyanates with post cat Poly. I'm aware that a lot of companies require their employees to wear the disposable suits, and we want to stay as safety minded as possible here.
However, our climate is also much hotter than it is cold. We're deep southeast, and coastal, so it's hot and humid MOST months of the year.

I want to be realistic. If I switch over to a finish that requires wearing a tyvek/plastic suit just to spray it and stay healthy, there's a pretty strong chance I'm going to have a hard time finding anyone willing to deal with that.

So here's my question for you guys that spray post-cat poly for cabinetry and similar high production--- what is your manufacturer saying you need to do for safety? What have you found your finish team prefers doing? What are you offering as "optional" equipment, and what are you requiring they use?

1/28/19       #2: Any safety tips on switching to pos ...
mauricio poli Member

Hello ! With all those equipaments you already have there will be no problem for your workers. If you read all the MSDS you will find out that Pre-Cat or CV are also dangerous, in my opinion using masks and cabin is ok.
The PU system is the best to apply in your city, humidity is good for them. And you will use less material and get better results. Make a 3 month trial , take notes, and you will check by yourself. Have a nice day!

1/28/19       #3: Any safety tips on switching to pos ...
Mat

I am not sure what you mean by "cabin", can you clarify what you are calling a "cabin"?

I do appreciate your advice though, very helpful.

1/28/19       #4: Any safety tips on switching to pos ...
rich c.

If I was working in your spray booth 8 to 10 hours a day, I would require an air supplied full hood in the booth. Too many finishers don't think they will be the ones for organ damage from chemical exposure, until they are diagnosed with it in their late 50s. Too late then!

1/28/19       #5: Any safety tips on switching to pos ...
chris

I agree with the supplied air hood which I find way more comfortable than a half face mask.Especially in hot weather having cool air flowing over your face.
isocyanates have no smell so it’s hard to tell if a regular mask’s filters are good

1/28/19       #6: Any safety tips on switching to pos ...
Bob Niemeyer  Member

Website: niemeyerrestoration.com

Mat, 2k urethanes that use isocyanates as a hardener do not "off gas" as you state.
The isocyanate binds with the resin, it does not "off gas".
The finishers are only exposed to free isocyanates in the wet film or wet overspray.
I have been using it for over 30 years and when I spray I wear a mask. Yes you can not smell iso's, but when you start to smell the coating in your mask it is time to change cartridges. I just wear a long sleeve T-shirt and gloves. No need for Tyvek, complete over kill, car painters wear them as they are spraying colors and don't want to ruin clothes.
I vary rarely spray CV or precat, Can't stand the smell in the shop from all the off gassing.
Spraying PU's you will not have that weeks of off gassing either on cabinet insides that customers complain about.

1/28/19       #7: Any safety tips on switching to pos ...
mauricio poli Member

Hi Mat ! I am sorry about my poor english. I wanted to say Spray Booth.
I would like to say that nowadays PU chemistry is more safety than in the past. A long time ago one could have a lot of free isocianate in the hardener, because of poor chemical reaction inside the reactor. But today so many reaction problems was solved, and there is almost zero of this free isocianate. This is the chemical which cause a lot of desease on the guys. If I were you, I would ask for your supplier samples of self sealer PU/Acrylic water based 2K. This is the future for us. Good Luck !!

1/29/19       #8: Any safety tips on switching to pos ...
dar

bob I know you are a ICA guy which product do you use for kitchens and baths thanks

1/29/19       #9: Any safety tips on switching to pos ...
the google

bob,

i, too, spray mostly 2k. i was told the iso's are most harmful in aerosol form, but these can be absorbed by humidity in the air (so maybe not that big of a deal). i wasn't under the impression they were any more harmful in the can or dried finish on the ground. is this not your understanding?

i have a fresh air mask and wear a spray suit. hot and more problematic to get around the booth, but very nice protection against harmful chemicals.

1/29/19       #10: Any safety tips on switching to pos ...
Mat

This has been very helpful! Thank you all for contributing.

I had been told before (and, I had forgotten) that the isocyanates weren't offgassed but rather present in the fluid and overspray. Thank you gents for clarifying that.

1/29/19       #11: Any safety tips on switching to pos ...
Bob Niemeyer  Member

Website: niemeyerrestoration.com

For Kitchens I like Acrylic Urethane finish systems. The trend is a nice open pore right now and Acrylics provide very good distension, a non yellowing film and long pot life. I use the ICA OAC363 topcoats and FAC241 Sealer most often.
The isocyanates are only a big deal when they are still wet. Dry film is not a problem. Wet overspray in the air is an issue, but with a good spray booth and spraying in the same direction of your air flow will help minimize exposure.
We need to remember that the isocyanate levels in our 2k urethanes made today have very low levels of actual isocyanate compared to the products of 20 years ago.
I will take a few parts per million of Iso rather than p-Toluenesulfonic acid used in CV or a Polyfunctional Aziridine Crosslinker used in many waterbased coatings.
Everything has it's dangers, we as finishers just need to be smart and protect ourselves as needed.

1/29/19       #12: Any safety tips on switching to pos ...
DannyB

Isocyanate is *only* harmful in two situations:
1. In the air, and only in fast moving overspray that has a chance to be inhaled before reacting

2. Contact exposure.

Isocyanates react *very* quickly with moisture in the air. They are also heavier than air.

When i say "reacts fast", that means that studies done by the various health orgs find that brushing/rolling 2k urethanes generates no detectable amount of isocyanate in breathing air[1], even in spaces with *no ventilation*[2].

That is, whatever amount is so small we don't have anything that can even measure it.

So it's basically "whatever gets on your skin/in your lungs before it can react with the air".

See:

http://www.hse.gov.uk/research/hsl_pdf/2005/hsl0560.pdf

h
ttps://www.ncbi.nlm.nih.gov/pubmed/26833099

You should use supplied air, and be very careful, but as the last post said, it's actually probably a lot better for you than spraying CV (in part because people take much better precautions).

1/29/19       #13: Any safety tips on switching to pos ...
dar

thanks bob , have used those products before, I should have ask about pigmented finishes because thats all I seem to do lately do them come in mixable bases?

1/30/19       #14: Any safety tips on switching to pos ...
JM

Take a look at Alcea Coatings. They have an iso free catalyst. We switched to it about 6 months ago from CV and are very happy.

The iso free catalyst is part number 9981/A699

https://www.alcea.com/en/

1/30/19       #15: Any safety tips on switching to pos ...
Bob Niemeyer  Member

Website: niemeyerrestoration.com

Dar, Yes there are tint controlled whites and intermix clears for making any colors. Tint pastes and other tinting options are available.


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)