Furniture Making

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: "Soft Spots" - a hardwood problem that's difficult to describe

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

"Soft Spots" - a hardwood problem that's difficult to describe

8/13/13       
Sam R Member

I'm doing a job which includes making table tops from premanufactured IKEA-style wood countertop slabs. These are edge-grain with finger-jointed blocks about 2ft long glued up to form 25"d countertop blanks. I've been told that returning the slabs to the manufacturer isn't an option and that I need to find a solution. The problem as best as I can describe it is that some of the components are face-grain-up rather than edge-grain-up, and although everything seems in order in the early stages, after sanding down we occasionally find an end of a block within the table top face that is "lifting". It's almost like the wood is stratifying, like a head of lettuce. Sorry I don't know how to describe it better than that. So there's a portion of the wood that is "loose" as my coworker describes it. Although I'm curious to know what cause this, I'm much more concerned with finding a solution to finish the job. We tried saturating the "soft" are with super glue which works marvelously except that it forms a slick that stands out from the surrounding oil-finished surface. Is there an adhesive or hardener that can be used to "cement" these areas that isn't so glossy when dry? Any other suggestions? The clock is ticking.


View higher quality, full size image (1024 X 768)

8/14/13       #2: "Soft Spots" - a hardwood ...
JeffD

Regardless of what kind of glue you use to glue it down you'll need to sand it off the surface of the wood before finishing.

As for the cause it's not b/c of face grain vs edge grain. It's a problem with the wood itself. May be b/c it was improperly dried or possibly stresses that were within the tree. being that it's from Ikea I'd hazard a guess there's not a whole lot of QC going into slamming as many of these wood tops as as quickly as they can. You can glue it down to do a band-aid fix and get it out the door.....I just wouldn't be too surprised to get phone calls down the road!

good luck,
JeffD

8/15/13       #3: "Soft Spots" - a hardwood ...
David R Sochar Member

Website: http://www.acornwoodworks.com

If you bought the tops, you are stuck. If they were given to you, give them back with a clear and simple explanation. If the owner will not take them back, then explain what you are up against and how it has already cost you more than anticipated. It is not unusual to see costs go up in one area as a result of lower costs in another. You do not have to absorb that difference.

It sounds to me as if pieces of punk or shaky wood were used. Sometimes it is hard to train those 12 yr old kids.

If the glue will not consolidate the bad wood, you can route them out about 3/8" deep and inlay good wood. This will still increase the costs, but should yield a quality result/product.

I refused to cut or work with Ikea or other tops years ago, with the phrase "I prefer to see local woodworkers employed."

8/15/13       #4: "Soft Spots" - a hardwood ...
Sam R Member

I did get some photos. These particular ones are in a different wood but they illustrate the problem more clearly.

The wood is cracking horizontally at intermediate stave ends. In this case the woodworker had cut a trough into the surface, revealing the issue. The problem is that after finishing this thin top piece will sometimes raise up, or "peel".


View higher quality, full size image (1024 X 768)


View higher quality, full size image (1024 X 768)

8/15/13       #5: "Soft Spots" - a hardwood ...
David R Sochar Member

Website: http://www.acornwoodworks.com

That is low quality wood. The heart of the log can be seen. This is avoided in better construction since it often splits in drying and has reaction wood in it.

This can be repaired by injecting a thin epoxy into the cracks, but you have to find them first - nearly impossible. The epoxy soaking into the wood may make the oil finish difficult.

The tops should be returned for a full refund. You will need to increase your fees to cover the unknown amount of work that you will encounter. This could go on for a while. You could get a call in a year about your tops 'falling apart'.

Oil finishes are reserved for the finest woods since that quality shows better with the oil. This is 'rustic' wood at best, and will not tolerate an oil finish, and would require a typical surface film, or barrier coat.

8/15/13       #6: "Soft Spots" - a hardwood ...
the google

sam -

we specialize in custom wood countertops and have rarely encountered this problem. unfortunately, this is most directly related to the quality of product you are working with. i'll leave it there because this isn't going to help your situation.

typically, we do as you have with epoxy and the like to keep cracks from lifting and feeling soft. sanding an oil finish is difficult at best so i would encourage you to tape everything but the cracks to limit your sanding and refinish work.

one question for you - are the tops finished on both sides?

the few times we had a similar problem it seems like we'd finished one side and let the other side sit for a day or two unfinished. this has been due to unexpected situations as we typically finish the other side the next day (as soon as we can with our finish system). anyways, that seems to be the constant when we get situations like you have described.

8/15/13       #7: "Soft Spots" - a hardwood ...
rich

If the wood has finish on it, I don't think anything will work. If you have raw wood, use a clear coat thin epozy finish, then scrape and sand back to wood. Oil finish after that. That is some really crap wood, wonder why it was the cheapest option for them?

8/15/13       #8: "Soft Spots" - a hardwood ...
mark

Don't be silly, Sam R. Give them what they'll pay for, and move on to the next job. Some people are just programed to purchase temporary things multiple times. There's nothing that you can do about it.

8/16/13       #9: "Soft Spots" - a hardwood ...
Chaim Gottesman

It has been my unfortunate pleasure to come across this problem as well.
You can use shellac to stiffen the wood fibers to allow for sanding but the epoxy or super glue is the only solution that wont allow the "grain" to pop up again and fill for finishing.
Try the shellac thing first.
Chaim

10/1/13       #10: "Soft Spots" - a hardwood ...
Jim Lewis

You'll be chasing this monkey for years before you fix it.

You are showing the heart of the tree. It's the part that moves most with changes in moisture. You can perhaps overpower it with epoxy, but it could easily check elsewhere, and you never know how far the splitting goes.

My experience with stabilizing wood like this with epoxy is that it sounds so much easier than it is: it takes at least 5x as much as you'd think possible, both in materials and in time.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)