Furniture Making

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: wood movement

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

wood movement

9/8/14       
Dan

I make limited production hardwood lamps. One lamp is essentially a milled block of hard maple 7 1/2"W x 2"D x 11"high. A 1/4" thick piece of walnut is glued to the top of the block as a decorative cap. The grain of the 7 1/2" face of the maple block runs up and down. The cap's face grain runs left to right, i.e. perpendicular relative to the maple grain. Since wood movement occurs mostly from edge to edge I am worried that the walnut cap will eventually be split by the movement of the maple left to right. Could a solution be to saw the walnut in half prior to gluing? A clean cut could be hidden quite well by careful gluing and clamping. My theory is that each half of the walnut would then be free move with the maple as the maple expands and contracts from it's center. I'd appreciate any ideas you have.

9/9/14       #2: wood movement ...
Huang Dai

The shrinkage calculator on this site can help you calculate the amount of movement one would expect in a block of maple that wide.

There are a variety of design approaches that would eliminate this issue - saw the cap out of a piece with the grain oriented the same direction.

Anchor the cap only in the center, leaving the ends free to float.

Mill a recess in the cap so that it fits over the maple, then glue it down in the center.

Build a test example then cycle it through humidity changes to see whether this is even an issue.

9/9/14       #3: wood movement ...
rich c.

A glue seam does not reduce the movement in half. Not gluing the seam will provide the half movement you want, but not the look. Huang has given good options.

9/9/14       #4: wood movement ...
mark

The stress will be on the maple block, not the cap. Rather, the cap won't split across the grain, but a long-grain crack might show up in the middle of the maple piece, or more likely, the glue will fail prematurely at the cap ends. Look up "bread board ends" for a traditional solution to a similar problem, then design a joint that accomplishes the same function while working within the limitations of your lamp design.

9/10/14       #5: wood movement ...
Dan

Thanks for all the input. I'd never considered that the block might crack instead of the cap! I like Huang's idea of anchoring the cap only in the center but unfortunately that wouldn't give the permanently tight (no gaps) interface I need between the flush-trimmed edges of the cap and the face and sides of the block. I'll continue to monitor the effect of seasonal changes on the lamp and alter the design if necessary.

9/11/14       #6: wood movement ...
Huang Dai

I have seen objects built with classic cross grain construction - they have remained sound for years. There are a lot of variables involved in whether or not any particular design or joint fails.

9/12/14       #7: wood movement ...
rich c.

The thing is, you won't have flush edges between the cap and the block very long. Something is going to give with the seasonal change, and they won't be flush.

9/12/14       #8: wood movement ...
Dan

You're right Rich. Actually it's the reason I submitted the question. I've had a finished version of this lamp for about a year now and noticed this summer that the sides of the block had moved 1/32 or 3/64 past the edge of the cape. The glue seal still looks fine (the glue moved?) and no cracks have developed. I'm assuming with dryer winter air they will move flush again. Visually it's OK because it's only perceptible when you rub a finger across the edges. Time will reveal the real consequences of this joint.

9/12/14       #9: wood movement ...
mark

Dan, time has revealed the real consequences of this joint. You're getting some good advise above from folks who have put this knowledge into practice.
Consider the projected lifespan of one of your lamps. What should it be? 5 years? 10 years? 50 years without abuse?
How many variables of material selection, construction environment, use environment, etc. are you willing to test with your, "wait and see?"

9/13/14       #10: wood movement ...
David R Sochar Member

Observations on cross grain construction:

I have made cross grain construction items for 40 years with very few problems. The most extreme example are many bread boards (for making bread) with breadboard ends. Most of these are about 18" wide, with quartersawn hard maple in 1-3/4" wide strips. Most had 3/16" wide Walnut strips between the Maple. This board is surfaced to about 7/16" and then tenoned on each end (about 3/16" thick by 5/8" long) and a Walnut end cap is fitted, about 1" x 1", plowed for the tenon.

These have been made with resorcinol, TB3, TB1 and TB2 as well as epoxy. They get a mineral oil finish, and little maintenance over the years. That means these are very prone to environmental changes in humidity, therefore wood movement.

I have had no joint failures, or even movement, period. 18" wide. I attribute this to the Q/S Maple and the surface area of the tenon. As well as the fact that these are almost never soaked in a sink or get more water than the occasional rinsing and drying.

So....if you were to increase the surface area of the joint on your two parts - splines, tenons, even rabbets - this should reduce or eliminate the movement, or the appearance of movement. A step between the two parts will also disguise any movement.

If absolute flush is required, then man-made core and veneers should be used.

9/13/14       #11: wood movement ...
Dan

Thanks David. So it looks like the easiest solution may be to use quartersawn or rifsawn boards for the maple block. I've been using 6/4 plainsawn wood milled into two pieces each 1 3/16 thick. Those pieces are then glued (face to face) creating a block 2 3/8" thick. But plainsawn gives me maximum movement across the 7 1/2" width. Qtrsawn or rifsawn will reduce and maybe eliminate noticeable movement. The question is whether I can find those boards in the retail barn where I purchase my stock. I'm not into large volume wholesale purchases or custom orders yet.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)