Furniture Making

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Fir coffee table

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Fir coffee table

11/7/14       
Jesse Andreini Member

I need to gray the exterior and am planning on using shop-made (table vinegar and stew wool) iron acetate to do so. Also, the clamp is holding the doors shut as they are on self-opening hinges. I need a positive hold latch that isn't the cheap looking plastic crap. If anyone has a source for well-made catches I'd love to buy some; otherwise I'll be building them so let me know if anyone has a shop-made solution they're proud of.
Regarding the graying: I have done this on oak but the fir (and maybe some cedar snuck in there, too) is more liable to soak up the vinegar and I'm wondering if I can remove the vinegar smell easily, short of pressure washing the whole thing. I'll do a clear topcoat, probably poly or OSMO polyx.

11/7/14       #2: Fir coffee table ...
Jesse Andreini Member

Here are the pictures.


View higher quality, full size image (1632 X 918)


View higher quality, full size image (1632 X 918)

11/10/14       #3: Fir coffee table ...
mark

I don't have any experience with aging fir. Iron oxide reacts with the tannins in oak, (white especially) to turn it black. Perhaps, fir has some available tannins, but it's a drastically different species, so I wouldn't expect the same results. Around here, some woods age brown, some grey, and some silver. Perhaps, the color difference is due to species, perhaps it's due to oxidation vs. UV degradation. The makers of hard wax oil floor finishing systems have figured some of this chemistry out: check there first. At any rate, I like your block of 2 x 4's.
I'd prefer not to think that there are euro hinges in there, but if so, I'm pretty sure that Salice, Grass, and Blum all make a push release hinge.

11/11/14       #4: Fir coffee table ...
Jesse Andreini Member

Thanks for your response. This is the fir sample with the chemical solution, whatever it is. It was done a few weeks ago, so it's been knocking around the shop a bit, but the tone is pretty close to what I got when it was fresh. The bench it's sitting on is untreated old fir; not sure how well the colors come through from a camera phone. I also noticed there is no vinegar smell on the sample, so maybe time will take care of that problem. It was still somewhat present 4-5 days after application.
The hinges are concealed 35mm cup hinges, an amazing engineering marvel! These are push by salice, but they're all marvels. I've never used these before; I usually stick to blum products, and these do feel like a slight step down, fit and finish-wise.
I don't really have qualms about using this type of hinge in modern furniture. I know I am supposed to feel like it is too pedestrian or something, but I think that is mostly because they're inexpensive.
I guess I draw the line at using their latches, though; I am considering the ives cl11, but would have to order it. Anyone have thoughts on the quality of those latches? Can't find anyone locally with a sample to put my hands on.
I think the solution is iron acetate(II) which is not depositing color on the wood but reacting with the tannins, few as they may be. It goes on basically clear, starts to darken, and then dries to the color you see in the pictures. It reacted much more quickly on the white oak. The topcoat does change the look quite a bit so it takes a lot of experimenting.


View higher quality, full size image (1632 X 918)


View higher quality, full size image (1632 X 918)


View higher quality, full size image (1632 X 918)

11/11/14       #5: Fir coffee table ...
mark

Yeah, ok: I've made my fair share of euro cabinets, so I won't give you too much of a hard time, regardless of your preferred mode of transportation...
For some reason I thought that the Salice push had a push-release catch within the hinge. Marketing. I have one of those Ives kicking around the shop that I didn't use for it's intended project. Fit and finish wise, it'd be ok, if you can mortise the box into the side of the cabinet, or the top, whatever's more appropriate. It's no good for surface-mounting, but that may just be my aversion to big wads of unnecessarily complicated gagetry poking through. It's got a good amount of power, and needs 1/8" to 3/16" at the mechanism for the push release to work. As I recall, it seemed more suited to a passage or closet door than to a cabinet door.
The vinegar and rusty nails seems to do the trick. On white oak, the effect is cumulative, so multiple applications can yield a nearly black color. It is interesting to note that texture has quite a lot to do with the appearance of age. Not that you expressed aging as your goal; just looking at your pictures.

11/18/14       #6: Fir coffee table ...
Joe Knobbe

Salice makes a drill in catch to use with push. See attached

Click the link below to download the file included with this post.

Push_Ed08_04_2013_ENG.pdf

11/25/14       #7: Fir coffee table ...
Rob

Rare earth magnets work well. They are available in different sizes. Drill the appropriate hole in the edge of the door and the rail, a little deeper than the length of the magnet glue it in with a wood plug at the top and it is hidden.

http://www.kjmagnetics.com

12/20/14       #8: Fir coffee table ...
Jeff

Jesse,
Try some Monocoat "Rubio Smoke". It is a reactive stain. I used it on some fresh end cuts in wormy Chestnut to match the weathered grey of the original surface and it worked well. You can control the intensity of the color with the amount you put on.
Jeff

2/23/15       #9: Fir coffee table ...
markbattles Member

Website: http://v-dubfurniture.com

Iron oxide reacts with the tannins in oak, (white especially) to turn it black. Perhaps, fir has some available tannins, but it's a drastically different species, so I wouldn't expect the same results.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)