Furniture Making

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Limitations re: tabletop size

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Limitations re: tabletop size

2/6/16       
Doug Member

Website: http://DougGunn.com

A potential customer has asked for a stow-leaf dining table like the one on my website. He wants the stationary top to be 60"x60". I've convinced him to reduce that to 54"x54". Leaves would be 18" each. I would make the top at least 1-1/8" thick. There can be no battens other than breadboard ends because of the mechanism under the top. My instinct is to refuse this commission because I'd have so little control over cupping in the top, which must remain flat. In addition to all of this, the table would travel to arid Nevada after being built in Pennsylvania. I'd appreciate opinions and advise.

Stow-leaf dining table

2/6/16       #2: Limitations re: tabletop size ...
Tom Diel

I understand your concerns. I finished up reception presentation station in Oct (no good pics yet) that has a 92" x 72"top. Long grain edging and breadboard are 1 7/8"th and infill panel approx1"th. This allowed the panel tenon to be a heavy 7/16"sq with the top of the dado in the bread board to match being 7/16"+ w/ btm tongue 1" in rift white oak.

I also had a large subtop to help span the load so sagging won't be much of a concern as in your condition being supported from four legs. My suggestion maximize you size of breadboard, tenon and mortise.

If I understand won't your leg footprint be a problem unless the length of the leaf is shorter to nest leaves under the legs? I.e. leaf to be 50"L? It could be a nice setback feature to allow across the table conversation?

Still working on web redirect, time to change web hosting!!!


View higher quality, full size image (3205 X 2455)

2/6/16       #3: Limitations re: tabletop size ...
Gene Wengert-WoodDoc

Cupping of a top results because of mositure change--100%.--but with a glued up top, there is enough variation in natural wood behavior that moisture change alone will not create a big difference in shrinkage too create much cupping. This assumes that you are making a table top at a moisture content that is very close to the MC in use. NOTE: In my dealings with these sorts of issues, almost always the problem occurs the first year and then no further problems after that. This means that the initial moisture coming from the manufacturing is not close enough to the in-use environment causing the problem, and that the yearly changes in humidity are not that much of an issue.

So, what must also be happening to create cupping is that the bottom side is being held from moving freely...the top can move, but the bottom is restricted.

And then, perhaps there is a different finish on the bottom than on the top, which means moisture changes from month to month. The bottom responds quickly, while the top's response is delayed due to the buffering of the finish.

I suggest that you avoid this job because not dies sound like the bottom is quite a bit different than the top.

2/7/16       #4: Limitations re: tabletop size ...
rich c.

I keep getting the feeling that no one wants to glue two pieces of solid stock together on here anymore because it can cup. Using quarter sawn is a start, but with good quality stock this is not an impossibility.

2/7/16       #6: Limitations re: tabletop size ...
Doug Member

The potential problem with moisture content is that the piece would travel from a humid to an arid environment. Seasonal changes in Nevada, once the table is there, would cause minimal movement.

Top and bottom finish are identical, and each has equal number of coats. MC of lumber and shop are plus or minus 2%. Top is attached to base in slotted screw holes, and only though a structure in the center 18" of the table.

A major challenge, and perhaps the single reason I'd turn down the commission, is that the table top "floats" above the leaves on a stow-leaf table. On a 54" top with an 18" leaf on each end, the table top is attached only to an 18" fixed structure in the center.

This means that when closed, the table top rests on the closed leaf, which rests on the table base. when the leaf is open, the slides rise up and support the top. (This is why the leaf can be (and must be) the exact width of the table top). This floating isn't a problem on a 42" wide top.

The one thing that might save this job is breadboard ends, which I would maximize. Also, quartered stock would influence my decision if I can get the customer to agree to it.

2/8/16       #7: Limitations re: tabletop size ...
Doug Member

The question for me (which I see I forgot to ask) is whether a 1+" x 54" x 28" quarter-sawn hardwood top will lay flat for 100 years (roughly 28" long because it would be anchored to the base structure at one end, breadboard at other end). I'm attaching a picture of the base of one of these tables without the top, hoping it might clarify some of this. One leaf is closed and one is extended but not yet lifted up and locked into brackets. The top would sit on all of this. When I put the quesiton like this, it seems do-able.


View higher quality, full size image (3264 X 2448)

2/12/16       #8: Limitations re: tabletop size ...
Jason

I just finished a 72x72" table and was worried about cupping, but if you find good stock that has been dried correctly, it should be fine. If you're really worried about it being Nevada, I would go with quarter sawn stock and price accordingly. The way you describe the table, I don't see why cupping should be an issue with quarter sawn stock that was dried well.
If you're still concerned, maybe do a veneer top???

2/19/16       #9: Limitations re: tabletop size ...
Doug Member

Website: http://DougGunn.com

Yes, I think quartersawn stock is the answer. The customer has agreed to it, without reservation. Not sure he really understands why I insist on using it, but he likes the look of it and doesn't mind the cost. Having thought and talked all this through, I feel confident that this top will be fine, anchored in the center and with breadboard ends. It's not a done deal because we still haven't settled on a design or agreed to a price. But if we can, I'll be happy to take this commission.

2/19/16       #10: Limitations re: tabletop size ...
Gene Wengert-WoodDoc

To be safe, indicate that the table is designed and constructed to function between 30% to 50%RH (6 to 9% MC). When the table leaves your shop, measure the MC at several spots with a painless meter and mark the spots and record the data. If an issue arises later, remeasure the MC to determine if it is outside the 6-9%.

2/20/16       #11: Limitations re: tabletop size ...
Paul Downs

The problem you are going to run into is when the humidity changes, and the exposed top of the top and bottom of the leaf expand faster than the two surfaces that are touching each other. Tell your client to be sure to leave the leaves extended for a couple of weeks after delivery, otherwise the change in climate could well cause cupping. How do I know this? I've made lots of this type of table, both in solids and with veneered top and leaves. If you can do it, a veneered top and leaf is much better for this design.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)