Subject: Re: console table structure/ makeup

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

console table structure/ makeup

11/3/17       
brant ritter Member

Website: http://brantritter.com

need some advice on the best way to approach building the attached console table. Anigre veneer, ~5' long x 2' deep
the bases are brass plate welded that slip into the grooves.
The center of the tabletop is 3" high, the ends are 1.25"

I'm debating using solid anigre for the apron and some cross members underneath. The top will be classic core with veneer.
Does this approach make sense? I'm concerned about the top veneer and sides matching.
Would using the same flitch to veneer the apron be appropriate?
(I'm showing two images, one with the drawer open, one closed.)


View higher quality, full size image (3260 X 1902)

11/3/17       #2: console table structure/ makeup ...
rich c.

I'd be mostly worried about the brass and wood notches matching up. Fabricated metal is not as precise as machined wood. You're expecting the brass to counterbalance the tops? Have you tested the forces required to tip the tables? Looks like too much overhang to me.

11/4/17       #3: console table structure/ makeup ...
Tom Gardiner

I would think it better to make the top a full torsion box with anigre all around. Build the box core with the drawer opening in mind.
I too would be concerned with the base/pedestal connection. I think I would just have the end tips of the brass let into the wood apron and design a solid steel connection for the pedestal that is bedded into the torsion box.

11/5/17       #4: console table structure/ makeup ...
David R Sochar Member

If these are Art Tables and all the people concerned understand there will be no rock collection out at the ends, then it may be OK to build. Any weight not directly above the leg(s?) will tip the table easily.

If the legs are not cast solid bronze, I would put about 150 lbs of steel in the very bottom of the legs. I have done this with 1/4" steel sheets, drilled to lag bolt into a recess in the wood structure.

Once that is accomplished, then you have to attach the legs to the tops. I'll leave that one up to you. The drawing shows a wedge penetrating the top, giving the illusion that this supports the table, but I would only think of it as illusory, not as a real point of attachment.

11/5/17       #5: console table structure/ makeup ...
brant ritter Member

thanks for the thoughtful responses. I do plan on pinning the legs to the table top as well as adding some weight to the bottom of the legs, The legs are made up of 1/8" brass plate.
The table will end up in the corner of a 3000 sf foyer with a telephone and lamp on it. Daily use is not in it's future.

11/6/17       #6: console table structure/ makeup ...
Tom Diel

Website: http://thomasdiel.com

Brant,
Nice project, the foyer comment qualifies the scope & expectations that helps us know the intent.
So many questions and ways to go but I would:
1. Sequenced book-matched qtr or ribbon stripe veneer would look good.
2. Miterfold laid up panels if you have access to a good slider & if bottom shows as a solid plane. Btm could be 1/4"th balanced construction access panels if reveals could be worked through.
3. Waterfall the end grain over the ends with that look would be my first design driver. This also begs the aprons to matched from the same flitch maybe over solid anigre so the draw front read as solid end grain when exposed.
4. Size your veneer flitch width to match the width of the top w trim allowance.
5. I agree w/ Tom about the bronze tips being decorative in the apron w/ steel plate up under.
6. You said welding, so if TIG welding C260 1/8"th with SIB filler the alloys are differing which you will have to be patient with any patination w/ multiple applications w knock back between and don't rush.
7. Wear a mask + fume extractor when welding but I am sure you have this experience from seeing you website.

You will get it,
TD

11/6/17       #7: console table structure/ makeup ...
Tom Diel

After a reread the C260 could be out to solid silicone bronze plate if budget allows (expensive and harder to get). The silicone bronze plate TIG welds like butter, and almost zero boil out of zinc. Then if you have to use 260 or other close alloy you might flame-braze so you don't have have darker patination problems associated w zinc and lower copper content brasses.

TD

11/6/17       #8: console table structure/ makeup ...
rich c.

Make sure you have a qualified welder who is fully aware of heat control during the welding. 1/8" plate of that size will very likely warp or oil can.

11/7/17       #9: console table structure/ makeup ...
brant ritter Member

I have an excellent metal fabricator who has extensive experience with brass.

One of my biggest concerns is the mitred edge on the tabletop that is exposed when the small pencil drawer is opened.

One option would be to simply glue in a small piece of veneer. I'm not too excited about this option.

I was considering edgebanding the table with 1" solid anigre prior to veneering of course. Then cutting my mitres. If I went with this method, I think that I will also use solid stock to make up the aprons and veneer them with the same veneer flitch as the top.

I'm reluctant to waterfall the veneer on the short sides of the table because I would be running it perpendicular to the grain of the apron.

Would I need to add a balance sheet to the back sides of the aprons, or are they stable/short enough to stay flat?

Thanks for everyone's feedback


View higher quality, full size image (1400 X 1017)

11/8/17       #10: console table structure/ makeup ...
Tom Gardiner

With a large 1" edge under the veneer of the top you risk print through of the joint between solid and substrate. Seasonal humidity change and the different reactions of the two might show a slight line. Anigre is busy enough that it might not be an issue but the quality of your work shown on your website suggests you would be bothered by it. A solution is to counter veneer the anigre before pressing to the substrate.
For the apron I am a bit of a heretic about balanced veneering. I have had no problems with veneering only one side of solid and I live in Ontario Canada where winter RH is 6 percent and summer is 75. Use urethane glue so as to add no moisture in the veneering.
On the other hand what is the cost of veneering the back?

Good luck.
Tom

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)