Home » Forums » Professional Furniture Making » Message | Login | |||
|
||||
![]() You are not logged in. Consider these WOODWEB Member advantages:
Curly Maple Top9/18
![]() Have a beautiful curly maple plank that I was able to plane down to 5/8" to get rid of saw marks. However it was plain sawn so am concern about it bowing. It is 14" wide and I really would like to not cut the plank. So any suggestions? 9/19
![]() Breadboard ends? 9/19
![]() Is it bowed now? Was it kiln dried, and kiln dried by someone that knows what he is doing? Is it acclimated to your shop? What is the current moisture level of the wood? Top top? Table design? Are you shipping it across the country to some weather extreme? I don't know why everyone is so afraid of wood these days. Start out with good material, follow the rules of proper furniture construction and proper finishing techniques to balance moisture absorbtion, and go to the next peice. 9/19
![]() Kiln dried by company that knows how to kiln dry wood. It is acclimated to my shop and all, does have a slit bow in it, do not have a moisture content meter. It will be a top without "aprons" for the top nor will it be shipped else where in the country. Do have good material and this is a great piece of wood. 9/19
![]() Breadboard ends, had not thought about it but it would work due to having enough ot the same wood from the same board. 9/19
![]() I'm no fan of bread board ends on a modern design. Are you just going to fasten the legs to a 5/8 thick top, or run the legs through the top and wedge them? You sure won't have much for screw engagement if you use them to fasten on the legs. 9/19
![]() Well the big issue for me is keeping the 5/8" maple plank flat since it is sawn flat. Have any suggestions? 9/20
![]() Battens on the underside, screwed near the center with tight pilot holes and near the edges with slotted holes and pan head screws. 9/20
![]() Okay I know battens are strips of wood. So the middle batten would be tightly screwed while the end battens would have slots in the battens to allow movement in the curly maple plank if I understand you right? 9/20
![]() Here's a hall table that is similar to what I am making. So tell me a little more about the battens
9/21
![]() One of the hallmarks of a professional furniture maker is problem solving. One of the first tasks of problem solving is to determine the goals of a solution, and the parameters within which the solution will be workable. All of this requires knowledge, much more so than can be acquired in a few paragraphs online. If this knowledge is beyond your ability, then it is time to up your contribution to your efforts. Attend a class, do research, visit museums, look at furniture and develop strategies that will work for what you want to make. Or work with a professional that is willing to let you learn while you work. Or, you may be better off shopping for plans. Beyond that, here is your first question for you to answer: Why will the flat sawn board warp? 9/21
![]() The flat sawn plank is similar to the attached pic and this would general mean some bowing at some point. Over the last few years I've attempted to learn new techniques here and there, but classes that would interest me are expensive. Am saving some funds for next year for a week long class in Philly that takes teaches Nakashima's work. Classes are expensive. So if the good wood workers would offer classes at a more reasonable rate I would be taking them. Am just a forester -- not the doctor that's into wood working or retired engineer or the successful businessman, etc. They have the professional Grizzlies, Delta Unisaws, etc. So if they would have the classes then I'd take more. The one in Philly is $1100.
9/21
![]() I have a four week furlough that lasts from mid January to mid February and I do try to connect with a woodworker that building style I like. And ask if I can visit his workshop and learn from them while working free with them. Once almost ended up with a Master Japanese Woodworker during my furlough but his cancer came back so that did not work out. Other reasons involve insurance. 9/21
![]() that table design in your picture would definitely look good with bread board ends.
9/22
![]() Why will the flat sawn board warp? 9/22
![]()
Or should each person complete the school of hard knocks with little help ? Or should we only give tips and advice to those who seem to know what they are doing ? Part of the issue here is to be in business and call yourself a professional has little to do with ability or skills so the field , since no degrees are usually required is open to all . I would do much better on a test now then 35 years ago , how bout you ? 9/22
![]() The most simple method for milling a log into planks, plain sawing, involves making a series of parallel cuts through the log. This method is quick and leaves the least amount of waste. Because of the directional tension across the grain as the wood dries, ages and wears, flat sawn boards can be subject to cupping, twisting and bowing. Often, dry boards will absorb moisture from the atmosphere and will become distorted. Plain sawn lumber has a large variety of appearances based on the angle of the growth rings relative to the surface of the board. Often, these rings can be nearly parallel to the board, creating large, open patterns. When the angle of the growth rings nears perpendicular to the surface of the board, there are tighter stripes across the face of the plank. 9/22
![]() As a forester one of the areas of my study was wood technology not the building of furniture. 9/22
![]() Just out of curiosity, since I see that you're from PA, did you go to Penn State? I studied forestry at Penn State in the seventies. 9/22
![]() Ken , a couple of things , were you a Silviculturist when you were with the forest service ? I did a kitchen for one , like you he told me he engineered the species geneticly to be the board he wanted . When he looked at one of the large glued up drawer faces he asked me if that was one piece of wood . It became obvious to me that he may know how to grow the trees but he did not know what he was looking at .
" Knowledge without experience is simply information " MT
9/22
![]() No, did not go to Penn State, went to University of Tennessee and now work with the NPS at the Great Smoky Mountains national park. 9/22
![]() D. Brown, this is just such a nice piece of wood and that was the reason to make a hall table out of it. Regular I would rip the boards and glue them together to make the top, but really did not want to do this. Besides I do not think I have the ability to slice a veneer out of this board. So was looking for a way to ensure good movement minus any bowing and such. 9/23
![]() Oh the suspense is killing me. Will Ken ever ring in with the correct answer to Kilgore's question? Will seasonal or moisture swelling of wood ever get mentioned? Will anyone ever tell Ken the proper slotting of cleats? Will anyone ever suggest that Ken reads Hoadley's book Understanding Wood? Will anyone ever tell Ken that the wood must be finished top an bottom to allow equal moisture absorbtion? These questions and more on "As Wood Moves". 9/23
![]() I'm not sure how many master craftsmen this website has on board, but there's no shortage of master wise asses. 9/23
![]() I think Ken already knows that but is looking for an solution to his unforgiving design . Where the cleats going to go with the design as it is ? After a degree and a career in forestry he knows little about wood movement or design but the table pictured looks nice . 9/23
![]() It's called humor Dave. 9/23
![]() Sorry, I haven't followed this thread since my earlier post, didn't think it needed elaboration. By battens I mean solid wood strips thick enough to restrain the panel's tendency to cup (say 3/4" to 1" in this case) screwed to the panel's underside with their grain direction at right angles to that of the panel in such a way that the screws do not restrict the panel's movement in width due to varying humidity levels. Thus the battens would be screwed tight at the panel's center, and the screws at the ends of the battens would run through slots, allowing the solid wood panel to grow and shrink while remaining flat. A breadboard end might accomplish the same thing, although if only as thick as the panel it's doubtful, and the relative movement of the two pieces would be apparent at various seasons. The panel could be restrained by a frame, but its movement would still have to be designed into the system. The most common system for harnessing table top cupping is to use metal s-clips or cabinetmaker's buttons (L-shaped wooden clips) screwed to the underside of the top and their tongues caught in a groove or pockets in the apron of a leg and apron frame, or the stretchers of a trestle frame. It's not clear how large your panel is, you may need intermediate cross stretchers between the ends of your frame depending on the length. It would pay you to get a copy of Joyce's "Encyclopedia of Furnituremaking". It will answer most questions of this nature, as they have been dealt with for centuries. 9/27
![]() Kevin I've gone with the cleat idea which sounds best and can add it to my design as some contrast to the maple and cherry. Just did get back from a week long backcountry trip at work. Enjoyed the humor and discussion guys, 9/27
![]() "The most simple method for milling a log into planks, plain sawing, ..." http://www.northendhardwoods.com/2010/09/quarter-sawn-vs-plain-sawn-v ...not that this is an answer to Mr. Trout's question, but here's my best guess citation for you anyway. Here's two more really easy questions to point you in the right direction:
9/27
![]() I asked the question because the OP is concerned about the board 'bowing' - apparently since it was plain sawn. He continues by mentioning he does 'not want to cut the plank'. This confuses things, because he proposes that cutting the plank will somehow prevent bowing. Not a good linkage of cause and effect. His OP in fact has two statements that utilize defective cause and effect. This is the reason for all the confusion that follows. His statements presuppose conditions that are faulty, or at least unclear, and the conclusions are based on that, as well as many of the responses. I asked why he is concerned about it bowing (whatever is meant by that could be another discussion...). Does plain sawing affect its proclivity to bow? -- as an attempt to explore the faulty (in my opinion) connection. >> Answer: Why does wood move (assumed to include 'bowing')? Wood moves in response to changes in Moisture Content (MC). This is normally caused by changes in the Relative Humidity (RH) in the environment of the board. A reading of Hoadley or any basic book on wood technology, or even here on Woodweb, will get that basic bit of info. So, is the piece going to be in an area where MC is likely to change from changes in RH? What will be the parameters of that change in RH > MC? Then, how will that affect the board? "Bowing" is one response. Cupping, twisting, cracking, moving, winding, splitting, or more are other responses. Battens, assumed to be cross grain, can prevent cupping. I'm unsure about preventing bowing since I don't know what is meant by that term. The battens (cleats, sticks, things) placed cross grain will do nothing to prevent most of the other defects that can happen. Natural curiosity is good thing, but must be countered by logical and rational thought, generating a sound line of reasoning. Without those simple basics, we would have a planet full of religious wars and hatred. 9/28
![]() There you go! 9/29
![]() Well, technically bowing refers to curvature of a board throughout its length, i.e. "rocker", whereas cupping refers to rounding across its width and crook to a bend in the edge direction. I addressed the issue of cupping as that is the most common problem with a wide plainsawn board, and seemed to be what the O.P. was concerned with. Bowing would be addressed with the same technique for a tabletop, pulling the board down onto a frame with clips. On the issue of free advice, it's worth every penny. If the questioner brings nothing to the fray but uninformed curiosity, perhaps he will exit with some useful information, and may actually be able to put it to good use. Perhaps he will be inspired to do some research before asking again, or maybe he will be sufficiently rebuked by the gadflies that he will never return. I am willing to share my experience, such as it is, with anyone who cares enough to ask,but it is only reasonable to expect an informed question on a "professional" forum. 4/1
![]() One of the first tasks of problem solving is to determine the goals of a solution, and the parameters within which the solution will be workable.
|