Sawing and Drying

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject:

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Cooking green wood in linseed oil

2/12/15       
Heinrich Spillmann Member

Website: http://www.heinrichspillmann.com

not sure if this is the right Forum to talk about this, but yesterday I stumbled over a Russian online article which I translated with Google Translate. The Russian wood worker talked about curing his chairs, carved from green logs by “cooking” them for several days in linseed oil. He further mentioned that this is a historic method used in Russia a long time ago. I have never heard of such a process and was wondering if anybody heard of this or has an experience with it on this side of the ocean. I similarly to the Russian wood worker carve chairs from green logs but then go to elaborate processes to dry and then reassemble them as I have talked about here before.

2/12/15       #2: Cooking green wood in linseed oil ...
Keith Newton

Well, I will say that I like carving green wood much better than KD.

I started my woodworking career about 50 years ago as a carver for a Frenchman interior designer down in Dallas. Besides what we custom made, he was importing a lot of wonderful carved antiques from Europe, that to my eye appeared to have been carved green, just judging by the way the cuts were made relative to the grain, and would hole the detail without the tendency split down the grain the way it would have if it were dry.

But, I just assumed that if they were doing that, they were also being very careful about how they dried these parts, like I do now when I carve green things.

There are a lot of turners who turn green, then boil, claiming that it helps prevent a lot of splitting. I've never tried that, nor felt a need to.

One thing that I would question, if what effect this oil soaked wood would have on gluing?

I think if I were going to experiment with something else after the carving was complete, would be to let the work dry naturally inside a paper sack, or cardboard box, which slows down the surface loss closer to what the moisture can come up from the inside to replace it, preventing surface checking. I would then soak it good with CPES, Clear Penetrating Epoxy Sealer.

I've not been using this product long, but I'm favorably impress with the results, especially in some soft woods. It isn't cheap, but then again, I wouldn't be too fond of having a flammable liquid boiling in my shop for several days.

If you try the boiling, I'd sure like to hear back from you. Otherwise, try this, and welcome to a new century. ha

I like your chairs. And while I don't know if there were any insects already living in your wood, if the CEPS would keep them from chewing out, but I'll bet it would keep them out in the future better than linseed oil. It is slow curing, so you can keep flowing it on as long as it will absorb.

After it has cured, a single coat of wipe on finish will look like 10 coats, but feel much harder.

2/12/15       #3: Cooking green wood in linseed oil ...
Gene Wengert-Wood Doc

This technique is called boiling in oil. It is in the literature here in the U.S.

2/13/15       #4: Cooking green wood in linseed oil ...
Heinrich Spillmann Member

Website: http://www.heinrichspillmann.com

Thanks Gene, I found the report by J.M.McMillen from 1961 (and a later one together with you?) and it doesn't doesn't
sound too promising for my needs. But it explains some of what I saw in the on-line photos from the Russian woodworker, checking and grey weathered look of the finished oak piece. I am still hoping to somehow find a way to stabilize the large carved oak bench, so it could be used in a controlled indoor environment

2/13/15       #5: Cooking green wood in linseed oil ...
EC Aumiller Member

PEG will stabilize it if you soak it... see this link from the Knowledge Base

Stabilizing Wood with PEG

2/13/15       #6: Cooking green wood in linseed oil ...
Heinrich Spillmann Member

Website: http://www.heinrichspillmann.com

Keith, thank you for you comments. I love your wild life and nature photography, beautiful. (Luckily I don’t have to decide which one I like better, your wood work or your photography, both stunning! Plus it looks like you live in a beautiful part of this country which I am sure helps with both) I know the comparison to turners and their processes keeps coming up with my stuff, but my stuff is harder to handle because of the size and so some of the turner’s experiences are harder to apply. Insects of course are an issue. With the chairs, I managed them by drying the quartered chairs in a kiln at temps over 130 degrees and afterwards I reassemble the pieces to the finished chair. But for the large bench, I am still searching for methods to control the processes. And large pieces are what I am drawn too……

2/13/15       #7: Cooking green wood in linseed oil ...
Heinrich Spillmann Member

Thanks EC Aumiller, looks like I missed that post from last July. That thread might be very helpful

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)