Sawing and Drying

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject:

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Flooring made from poplar that's not been tongue and groove

10/4/15       
rod hays

Kiln dired poplar that is glued and scred down. which I think tured out great. I put filler over the screw heads in in between the boards to fill in the cracks.


View higher quality, full size image (2048 X 1152)


View higher quality, full size image (2048 X 1152)

10/5/15       #2: Flooring made from poplar that's no ...
Scred Dird

Very nice - be sure to post a picture in a year - I, for one, would be interested in seeing how well that installation method and materials choice hold up in that environment.

10/5/15       #3: Flooring made from poplar that's no ...
Iswhatitis Member

The filler will never stay in the gaps/joints at the floor expands and contracts through the seasons. It will become loose when the floor shrinks, and then will be crushed/pulverized when it swells. It will then either be vacuumed out or fall through leaving the gap you were trying to hide. The filled screw holes will also shrink and be sucked out by the vacuum or sweeper.

Very pretty though.

10/6/15       #4: Flooring made from poplar that's no ...
rod hays

I got the idea of using filler from videos like this.

''Gap filling wooden pine floor with filler and sawdust mix''

YouTube video

10/6/15       #5: Flooring made from poplar that's no ...
Iswhatitis Member

It may definitely get the check, but better have a very short warranty. Those floors simply move too much to be sealed up tight light that.

The video is funny, many of the screws are not even counter bored. They are just barely below the surface and you can see the cross pattern of the phillips head in the filler.

All you can do is try it and see what 5-10 years brings. There will be little to no filler at that point. More than likely far earlier. The filler will dry rock hard. It will not accommodate the slightest movement.

Still, pretty when first finished.

10/6/15       #6: Flooring made from poplar that's no ...
rod hays

You more then liekly are right,but it's an old house with unlevel flooring. The boards made the floor level. So in 10 years this floor could be used as a sub floor for a new floor if a person wanted a new floor. I'm 66 years old,so I'll give an up date in ten years if I'm still alive at 76 on how the floor lasted. I've decided to do the whole 1890's 1000 sq ft house with this flooring.

10/6/15       #7: Flooring made from poplar that's no ...
rich c.

You probably won't have to wait 10 years to see the problems. One winter and one spring should do it. Might be earlier if a lot of water comes out of the shower or sink.

10/6/15       #8: Flooring made from poplar that's no ...
Gene Wengert-WoodDoc

The moisture content of a floor will typically change from 5 to 6 % MC in the wintertime up to 9% MC (maybe 10% MC) in the summertime. A 4% MC change results in 1% width change. So, we can expect the floor to shrink at least 1/16" between each piece. If this crack is filled with putty, caulk, etc. in the winter, then when the floor swells 1/16" in the summer, the pressure will cause the filler to pop out, or a ridge to develop between each piece. The ridge does not go away the next winter. If the filler is hard, traffic will cause it to crack and come out.

The video referenced shows a process similar to spreading filler on a tile floor, but tile does not shrink or swell, so this is an acceptable process. Also, the swelling amount is less with narrow wood flooring pieces.

Although it may not have worked in this case, there are a products (sheets of Hardi Board is one) that are designed to level a floor prior to installing wood flooring.

10/7/15       #9: Flooring made from poplar that's no ...
rod hays

Well I guess I'll get my router out and tongue and groove ...the rest of the flooring. Below is what the floor looked like as it was laied out before it was screwed and glued down.Most liked it best with the cracks showing.


View higher quality, full size image (2048 X 1152)

10/7/15       #10: Flooring made from poplar that's no ...
goracle

The additional flooring laid on top of the original flooring will increase the fuel load, thereby enhancing the combustibility of the structure when the inevitable urban renewal comes to that address.

Keep gluing and screwing - in the long run it's all good.

10/7/15       #11: Flooring made from poplar that's no ...
Iswhatitis Member

I think the statement "most liked it best when the cracks were showing" is where the money is.

People want the romance of these old floors but they somehow want to force them to comply with modern consumer demands (smooth, easy to clean, dont trap trash, and so on). But thats simply not possible. When you see someone build a three quarter of a million dollar tibmer frame home and they want old world, wide board floors (meaning face nailed wide16"-30" floors) they actually DO want the old world look. That means that in the summer your floors will likely have a gap between boards that you can look down in and see a tic tac down there that you dropped. There will be all sorts of trash in those gaps that will have to be cleaned out, vac'd out, or lived with.

In the old world days these gaps never filled with trash. Why? Because the floor was the floor! There was no subfloor. So trash that was on the second floor, fell through to the first floor, then fell through to the basement.

It was not uncommon in colonial times to have light peeking through from floor to floor. I even remember as a child, kids who lived in very old homes being able to lay down on the floor and peek through to the floor below and we are talking way way after colonial times.

The problem we face nowadays trying to recreate these floors with modern subfloors is that there is no where for the trash to go. So the gaps fill with trash, the floor expands in the summer, and jacks itself wider. It then shrinks in winter, re-fills with trash, and summer comes and it jacks again. If this process continues until the floor has no more room for expansion (hits the exterior wall) it buckles.

It is a very very difficult thing to incorporate these old world, rustic details, in to modern homes. They can most definitely work, but they have to be accommodated and tended to.

Unfortunately, most people who think they are fine with whatever misconceived cost savings they think they may be getting by using "old world" building practices in modern time soon come to the realization that it was a mistake.

There is no reason what so ever not to build like they did 200 years ago but you gotta take it the whole way.

There is a simple reason why we dont build that way any longer. You cant fight it.

10/7/15       #12: Flooring made from poplar that's no ...
Iswhatitis Member

PS. In that photo of the floor with the cracks, you've got what looks like an unvented full S trap sticking through the floor (good you put a cleanout there cause you'll likely need it or want to install a mechanical vent in the future).

Full S traps were banned perhaps 25 years ago.

10/9/15       #13: Flooring made from poplar that's no ...
Woodie

I really don't think you will have any problem. I used some poplar on a floor in an old house a couple years ago. I face nailed it with 16ga finish nailer and you have to really look to find the nails. Only thing I hope you used some type moisture barrier. Roofing felt will better than nothing.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)