when can we use white oak? -- 1 -- 
12/14

Just purchased 4 slabs of quarter-sawn white oak, 1.5" thick approx 20" wide, 10' long. Bought from a sawmill, it was cut days ago. We would like use it to make a top for our kitchen island. A local furniture maker that makes a ton of farm tables, mostly from pine, told me it needed to dry ( inside a building away from moisture) for 30 days. Does this sound right? I know nothing about this and am learning the hard way that i may have made a mistake in this purchase...that i can't return. Thank you in advance for any help.
12/15 #2: when can we use white oak? ...

30 days? More like a couple of years. No species of wood will be ready to be used by air drying for 30 days. 6/4 white oak could hardly be ready in 30 days in a kiln.
12/15 #3: when can we use white oak? ...

You could use the oak but you would have to allow for the wood shrinking in mostly width. They build cabins out of green logs. They do this by building in ajustment. Your counter top would have to be free floating.
12/15 #4: when can we use white oak? ...

read this and than you will know, that it will be a while before you can use inside , go to this link
Link
12/15 #5: when can we use white oak? ...

Thank you all for responding but I guess i'm just as confused as i was before. Can use it...can't use it....
Rod, you indicated it would shrink mostly in width, but everything I've read about quartersawn is that it will shrink mostly in thickness, not width.
Again, I have no experience and am way out of my realm of knowledge, but from what I'm reading online is there may be problems with cracking as it dries but with quartersawn it should have minimal cupping and minimal shrinkage in width. This is quartersawn white oak.
Any more thoughts? Anyone?
12/15 #6: when can we use white oak? ...

I made a bar top made out of 7 different types of wood. They were all 4/4 air dried for 2 years and planed down to 7/8". Moisture was 7 to15% depending on the type of wood. They were glued to a 3/4" piece of plywood and sealed on all surfaces. After that I put the final 3 coats on the top. So far no cracks or splits.
12/15 #8: when can we use white oak? ...

My mistake, it would shrink the most in thichens
12/15 #9: when can we use white oak? ...

It will shrink proportionally more in thickness but will actually shrink way more in total width because it is way wider to start with. There is a shrinkage calculator here on Woodweb that will tell you how much it will shrink but I didn't look at it.
As stated earlier the wood needs to be dry before using. I personally would never try to build a counter top of all things out of green lumber, quartersawn or not.
12/15 #10: when can we use white oak? ...

Website: http://www.tsmfarms.com
KP...This craze of using the beautiful woods for all these fabulous projects has gotten the truths and correctness out of line by all the so called "we know what we're doing" unprofessionals doing shoddy cut throat work. MOST don't even have business liscense much less morals and ethics of being masters ( that is anyone who can do a trade on their own in a professional and ethical manor AND provide leadership in seeing trade is being taught correctly). I'm sorry if this sounds like a rant....IT IS!!! BUT I hope it's an eye opener and gives you good guidance. I'm seeing SO MANY people that are getting bad info and are going to be disappointed when their tops (or whatever) warp and twist and the bugs start coming out.
Let's start with your issue/question. 1) YES it needs to be dry.....the correct MC (this is what the interior of the wood should be NOT the outside!!!) Interiors of the average "USA" home is 7-10% and most use 9% as the ideal average. AD ,depending on your location, average in USA is 12% and this can be used IF all the stars are lined up and the project is made to "float".
2) AD vs KD...MANY arguments on this but the truth is both have their pros and cons.....I personally do both...long term ADing is good on stress relieving in the wood but once below 25% MC it's not as critical but I dry on down to the 12-14% range, then I KD on down to 7% MC, then sterilize....
3) Sterilizing/debugging.....THERE IS so much wood being reclaimed, regenerated...whatever the name they use this week LOL....that is NOT being sterilized/debugged and being introduced into homes and businesses that could cause future problems when they decide to come out......YES you need to do this step also AFTER drying.
I just talked to a lady this week and she was "doing" her own workmanship. She is planning to build walnut countertops BUT running the grain front to back instead of lengthwise....for 15-18'...I didn't have the walnut to fill the order BUT I thought I misunderstood the direction...after calling her back and inquiring, I asked her IF she knew how much it was possibly going to move that way....her reply if it's KD'd it won't move...WRONG!! I guessed and informed her possibly 2+" from winter to summer on a unregulated humidity home.
KP, you have a great vision and can be very self rewarding if done correctly. Gene the Wood Dr. here can give better specs than I recall from memory. Check out my website to see wood from start to finish.
Have a Blessed day,
Tim
12/15 #11: when can we use white oak? ...

Thank you everyone for your responses! Shame on me for jumping on what i thought might be a "deal" without doing more research first. Shame on the guy that sold me the slabs, knowing what we were buying them for. Hopefully we can sell them, and move forward with something else.
Thanks again!
12/16 #12: when can we use white oak? ...

I will throw my two cents in on this issue. I am in western Oregon and mill and dry Oregon white oak.
The white oaks as a group are difficult to dry properly. This is because they have a fairly high radial to tangential shrinkage ratio, are very dense and contain plugs in the conductive cells called tyloses which impede the movement of water out of the cells. Because of these considerations, green lumber must be dried very slowly at first to avoid internal checking known as honeycombing and then dried aggressively after the wood is below 20% moisture content to drive the last bit of water out of the wood. So, with 6/4" "slabs", the best strategy would be to air dry for a good 6 months to a year (depending on the local conditions) followed by kiln drying to get down to the desired moisture content for internal usage (usually 6-10%). Then, as previously stated, the wood should be heated to 130 F for at least 4 hours to kill any insects or larvae which might be in the wood. It should be noted that with Oregon white oak, the high tannic acid content of the heart wood confers resistance to insect problems, but the sap wood is susceptible to boring insects.
You can build with much wetter wood than kiln dried, but it should be understood that the wood WILL move and shrink as it drys and you must allow for this movement both in the overall dimensions and in how you attach the wood to the counter.(Trapped wood will split or crack at the points of attachment).
In the final analysis, quartersawn white oak is an excellent choice as a wood for counter tops, but it must be both properly dried and properly installed. The installer should understand that the wood will move AFTER INSTALLATION as the humidity conditions change (both with wet kitchen situations AND seasonal humidity variation). It is true that quartersawn wood changes more proportionately in thickness than in width when compared to flatsawn wood, but it will still move a bit...
Good luck with your project. I hope you will takre the time to locate properly dried QS white oak as it is beautiful material which gives a beautiful style and is very durable.
View higher quality, full size image (2240 X 1488)
12/16 #13: when can we use white oak? ...

I should note that the table in my last post was built by Zach Malcolm from Portland Oregon...
http://www.zachmalcolmfurniture.com
12/17 #14: when can we use white oak? ...

Website: http://www.tsmfarms.com
KP If you have a little bit of time,especially if you really like your slabs, a option might be a vacuum kiln. Also yours can be KD'd soon if special care is taken in the drying process. I think there's a link on here to find local kilns in your area.
Have a Blessed evening.
12/18 #15: when can we use white oak? ...

I agree with Tenn. that the QS white oak could be dried from green in the kiln, but you need to be ABSOLUTELY sure that the kiln operator has experience not just with drying hardwoods, but with drying thicker green white oak. If the dry rate is too fast, (even for a few hours) the wood will be destroyed.
I have a dehumidification kiln (Nyle) and 6/4 Oregon white oak takes around 9 to 10 weeks in the kiln to dry.This assumes that you have a full kiln load of material (around 1500 board feet in my case). It is difficult to properly dry just a few pieces, as the relative humidity around the wood of a partial load may not be high enough and the wood will dry too fast and cause honeycomb defect.
I do not have any experience with vacuum kilns, but it is my understanding that there is not much advantage to this method with most white oak species because the tyloses in the cells impede the movement of water, thereby reducing the efficiency... Perhaps someone with experience with these systems can add their comments..
1 -- 
Buy & Sell Exchanges | Forums | Galleries | Other Resources | Site Map
Buy and Sell Exchanges
Job Opportunities and Services Exchange
Employment opportunities and services within the woodworking industry
Lumber Exchange
A worldwide buy/sell exchange for lumber and wood products
Machinery Exchange
A worldwide buyer and seller exchange for woodworking machinery and equipment.
Classified Ad Exchange
Classified advertising for the woodworking industry (for advertisements that do not include machinery, lumber products and employment listings)
Forums
Adhesives Forum
Discussing topics related to adhesives within the woodworking industry
Architectural Woodworking Forum
Discussing quality standards and production of architectural wood products
Business and Management Forum
A forum for the discussion of business topics: from sales and marketing to dealing with difficult customers.
Cabinet and Millwork Installation Forum
Discussing all aspects of installation issues encountered by cabinet and millwork installers.
Cabinetmaking Forum
Discussing 32mm and face frame cabinet construction including fabrication, casegoods design, and installation.
CAD Forum
Shedding light on the all-too-often shadowy world of CAD.
CNC Forum
Discussing CNC (computer numerically controlled) woodworking equipment, software, and automated product manufacturing.
Dust Collection, Safety and Plant Operation Forum
Discussing topics related to maintaining a safe and productive working environment.
Professional Finishing Forum
Finishing issues for the production environment
Forestry Forum
The science and art of forest cultivation and timber management, planting, surveying, tree diseases, silviculture and timber harvesting
Professional Furniture Making Forum
Helping professional furniture makers improve quality, save time, and increase profits
Laminating and Solid Surfacing Forum
Issues related to laminating and solid surface materials and processes
Commercial Kiln Drying Forum
Discussions covering issues faced be commercial drying operations that process at least 750,000 bd. ft. of lumber per year
Sawing and Drying Forum
Discussing topics related to primary processing and drying of lumber
Solid Wood Machining Forum
Discussing topics related to the machining of solid wood
Value Added Wood Products Forum
Learn how to improve your output, find new markets, and boost sales of your lumber products
Veneer Forum
Discussing topics related to veneer processing, manufacturing, and fabrication
WOODnetWORK
An electronic discussion group for woodworkers throughout the world
Galleries
Project Gallery
Where professional woodworkers can post examples of their work
Sawmill Gallery
Professional primary processing companies display and describe their sawmill facilities
Shop Gallery
Professional woodworkers display and describe their shop facilities, products and equipment
Shopbuilt Equipment Gallery
Professional woodworker's jigs, rigs, and shopbuilt equipment
Other Resources
Industry News
Late-breaking news from all sectors of the wood industry
Video Library
Index of industrial woodworking related digital videos on the web
Auctions, Sales and Special Offers
Advertisers offering woodworkers discounted prices on good and services, and announcements of upcoming auctions
FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)
WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
A valid email return address must be included with each message.
Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
Subject lines may be edited for length and clarity.
"Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
(return to top).
Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.
You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.
WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.
Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).
Libel: Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.
Improper Decorum: Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).
Advertising: The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).
Repeated Forum Abuse:
Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.
There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).
The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)
Forum Posting Form Guidelines
|
Your Name
|
The name you enter in this field will be the name that appears with your post or response (return to form).
|
Your Website
|
Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
|
E-Mail Address
|
Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
|
Subject
|
Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
|
Thread Related Link and Image Guidelines
|
Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
|
Thread Related File Uploads
|
Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .FLV .MP4 (Image Upload Tips) If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
|
|
|
|