Solid Wood Machining

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Grinding to Axial Constant System for 5 head molder

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Grinding to Axial Constant System for 5 head molder

3/19/16       
Scott

Using a few DIAGRAMS, can someone give me the simple explanation of the Weinig Axial Constant system for grinding profile knives?

I want to know WHERE on the knives am I keeping things constant?

How do the side knives fit into the axial constant system?

I understand the concept and benefits of the system - so I don't need explanations of why its a good idea - I just need to know HOW to implement it.

If there is a document out there that explains all this, pls post it or post a link.

Thanks!

3/19/16       #2: Grinding to Axial Constant System f ...
shaner

Go to Mirror Reflections Website. Russ wrote a bunch of articles about moulder and grinder setup,operation and troubleshooting. Very informative and always go back to them if I need to check something. He has a ton of knowledge and has helped me be more successful since I started.

3/20/16       #3: Grinding to Axial Constant System f ...
Russ

Website: http://www.mr-moulding-knives.com

Scott
The Weinig axial constant system is built off of a 10mm or .394" starting point on all moulding knives and 20mm .787" on all moulding templates so you don't fall off the template the same time you end the knife.

It is also based off of the stops on the template carrier installed on the profile grinder and size of the arbor that the cutter head is placed on.

I have placed a link below that may help you, if you have any questions or concerns please just give me a call, contact information is on my website.

Thanks Shane for the mention.

All the best
Russ

https://www.mr-moulding-knives.com/information/axial-constant-alignment

3/20/16       #4: Grinding to Axial Constant System f ...
Russ

Scott
Here is an article on how to set up your moulder axial constant after your have ground the knives axial constant.

I hope you have a better understanding on how the system is setup to save you up to 50% of your setup time.

Good Luck
Russ

https://www.mr-moulding-knives.com/information/axial-spindle-calibration

3/21/16       #5: Grinding to Axial Constant System f ...
Scott

ok, i'm a newbie and I think I'm missing something here... it would seem that the axial constant would need to relate to the EDGE of the FINISHED PRODUCT. I did not see anything in Russ's diagrams showing where the finished product is in relation to things - the drawings don't even show a finished product. Even if the head had the 10mm spacer below, if I ground the finished edge of the molding in 15mm from the edge one time and 7 another then we'd still have to line things up with the particular knife when it is set up.

My question - in my drawing - which color 10mm axial constant is correct?

1. is it Blue - 10mm from edge of head to edge of fence
2. is it green - 10mm from edge of finished product profile edge to the fence?
3. is it red - 10mm from the edge of the finished product profile to the edge of the head?


View higher quality, full size image (1042 X 984)

3/21/16       #6: Grinding to Axial Constant System f ...
Russ

Scott Green The below article may help you. Keep in mind these few things Profile Template begins 20mm from edge Profile Knife begins 10mm from edge Distance between template stop pins is 260mm using a 240 mm arbor with spindle nut installed. Please call if you need further help.

Article

3/21/16       #7: Grinding to Axial Constant System f ...
Russ

Green Is the best picture but not entirely correct, the 10mm mm built in to the knife is always behind the fixed fence or below the bed plate by 10 mm. .000" or 0 mm is where the cutter head come in contact with the spindle base. Therefore you counter on the spindle would read .394" or 10mm.
Let's say for instance you own a Weining P23, the number stand for 230 mm or 9.062" of finished width, you could mill a 8.625" profile and if you move the counters to 000" you can get 9.062" s4s.
I hope that helps
Russ

3/21/16       #8: Grinding to Axial Constant System f ...
Rob Scaffe  Member

Hey Russ
I didn't review your articles which I am sure are excellent, so my apologies if this is redundant. But if not maybe it will help.

I am assuming we are talking about a Weinig grinder and molder.


View higher quality, full size image (816 X 1056)

3/21/16       #9: Grinding to Axial Constant System f ...
Russ

Rob
Perfect,
I did not have time to draw a sketch to illustrate, slammed here.

Nice Craftmanship on the Grandfather Clocks by the way, absolutely gorgeous

Russ

3/22/16       #10: Grinding to Axial Constant System f ...
Scott

YESSSS! Thanks Rob. Your drawing was perfect to bring clarity.

Now that I see your drawing when I read Russ' nice explanation I understand it but your putting the profile drawing on there nailed it. Thanks! Basic stuff, but first time around I want to make sure I am setting things up right.

Russ - yours are excellent articles - why don't you clip Rob's drawing and drop it in? That would help visual learners like myself to more quickly grasp the written content.

3/22/16       #11: Grinding to Axial Constant System f ...
Russ

Yeh
When Rob and I work together we make a pretty great team :)

3/22/16       #12: Grinding to Axial Constant System f ...
Scott

another question - IN GENERAL is it better with a profile like I've sketched it above to have the thin side on the left and the straight thicker side on the right next to the fence? or does it make any difference?

3/29/16       #13: Grinding to Axial Constant System f ...
David Waldmann  Member

Website: vermonthardwoods.com

For the profile type you drew, in general it's better to have the thickest part at the outside. The reason is that the thinnest part is where the most wood must be removed, which means higher stress on the knives/head/spindle. The spindle is strongest nearest the bearings.

However, there are many times when this is not feasible, and I'm not really sure just how much difference it actually makes. It may be like the straw that broke the camel's back.

3/29/16       #14: Grinding to Axial Constant System f ...
Scott

Thanks David, that makes sense.

What about some of the rest of you that run molders -how do you decide which side goes to the fence?

3/29/16       #15: Grinding to Axial Constant System f ...
Russ

Scott
I use the the same theory as Dave mentioned, as time goes on you will realize from layout mistakes a lot comes into play when deciding which way to orient the moulding in the machinery, hold down issues, is the knife gonna mill away wood from the feed system, will the knife design hit the rollers, etc.
I can't speak for everyone but my experience in your question above comes from making many mistakes over the years, you learn what works best and what to stay away from.
All the best
Russ @ MR

3/29/16       #16: Grinding to Axial Constant System f ...
Scott

Speaking of creep - wouldn't having the deep part on the outside (left) tend to push the profile toward the fence and conversely the thin side to the right push it away from the fence?

Trying to drink from the experience of the molder community here before I grind a bunch of knives wrong.

3/29/16       #17: Grinding to Axial Constant System f ...
Russ

Depends on the profile, if it was a beveled casing I would agree with you and reverse the detail with the small side toward the outside and simply use a reverse profile pressure shoe. But David's comment above is generally what I use as a starting point then I look for other issues from that point that might detour me from that decision.
Russ

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)