Solid Wood Machining

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Straight line rip saw personal safety solutions

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Straight line rip saw personal safety solutions

9/9/16       
Justin Member

I'm looking for some information regarding the safety practices/PPE (personal protection equipment) for the operator of a straight line rip saw. I have attached a picture. The saw we have is a older cantek SRS 12.

We recently had the owner of the businesse injured by a 1/8" thick by 2" high off cut that tapers down to a point. i won't go to much into detail but basically the off cut shot back and went into the side of a finger and towards the knuckles.

There has been 4 accidents similar in nature involving different operators on the same saw over the span many years (maybe 15years or more) it's not a common accident. In all cases the machine is looked over and inspected for faults but always found in proper working order.

Normal practice is for the operator to feed the machine from the side of the line of cut and when the saw grabs the board to step aside. The person catching normally holds onto the board along with the off cut until clear from the saw.

My question is what is everyone else in industry doing to prevent these freak accidents and what kind of PPE, if any are company's using to protect their employees?

During the safety meeting, the accident was discussed and a few ideas was suggested to protect the operator in case of a freak accident.

For example kevlar gloves but that may create a risk of the feeding belt catching the fabric and pulling your hands in if your ripping short lengths if your hands get to close.

The other issue is we've been lucky to only have accidents involving the hands, not to downgrade the importance of any injuries but if you get struck in the core with a off cut then it becomes life threatening. So a leather vest/Kevlar vest was also suggested.

Are any of these ideas common practice is other shops or what else can one do to increase safety.

Thanks


View higher quality, full size image (2711 X 2355)

9/10/16       #2: Straight line rip saw personal safe ...
David R Sochar

I have seen a heavy leather apron of sorts worn by people infeeding a ripsaw. This was usually double thick, covered well the "combat zone" that is at risk. Hands should be kept out of the path of potential kick backs. The operator also needs to be able to step aside and have the next board in place to go thru the saw. This put wood in the position needEd to help block those narrow pieces reversing direction.

9/11/16       #3: Straight line rip saw personal safe ...
Mark Elliott Member

Justin,

If your Cantek has a one piece chain with the blade running in a grove, the grove needs to have rubber inserts glued in there.

Contact Cantek over this, it's a regular maintenance item.

They create a zero clearance insert that the blade runs in and goes a very long way cutting back on those types of kickbacks.

I suspect this might be the case. I keep lots of extras on hand and have to re-do them when they come out of the grove.

You can use 3M contact adhesive that comes in the aerosol cans to glue them in place.

They are absolutely essential for the over arm blade import saws.

Mark

9/11/16       #4: Straight line rip saw personal safe ...
Justin Member

A thick leather apron is along the lines of what we were thinking. would a thick apron be enough to stop a off cut if it were to kickback?

The feeding chain is in segments with a grove in it, similar to the picture but not as deep maybe 3/16". Is that the same kind of feeding belt your thinking of that needs a rubber insert? There is very little extra room in the slot to try and glue something in.


View higher quality, full size image (500 X 500)

9/11/16       #5: Straight line rip saw personal safe ...
Mark Elliott Member

Justin,

The rubber inserts are are meant to be glued into that slot.

I think you'll find they'll come in the exact size to be glued in there.

Raise the blade, glue them in, then lower the blade back into them with the chain running.

You'll be pleasantly surprised how it will help to eliminate that kind of kickback. Those pieces get caught between the blade and chain in that slot, hence the need for the rubber inserts.

Mark

9/12/16       #6: Straight line rip saw personal safe ...
Ryan Akhurst

Website: http://www.cantekamerica.com

Hello Justin, I am one of the owners of Cantek. Over the years we have developed additional safety devices for this saw (now C12RSH). We have an add-on bottom kickback device (yours only has top kickback fingers) and a side safety guard assembly. Please email me your serial number and we can provide you with photos and pricing on these items. In addition we have the rubber inserts in stock which Mark has already mentioned. Email: sales@cantekamerica.com

9/12/16       #7: Straight line rip saw personal safe ...
Justin Member

I check the machine today and we actually already have the rubber inserts installed.

Thanks for all the response

9/12/16       #8: Straight line rip saw personal safe ...
Mark Elliott Member

Justin,

That's good, just make sure you're not missing any.

I'm going to ask one of my guys tomorrow how many kickbacks he's getting off of a similar saw and report back. I do have the second row of anti-kickback fingers that Ryan referred to.

But having said all this, what David said is still 100% true and worth taking to heart.

Mark

9/14/16       #9: Straight line rip saw personal safe ...
Bill

Just a point of information we have a relatively new Diehl saw and never get kickbacks.

9/14/16       #10: Straight line rip saw personal safe ...
Fred

Website: http://www.rivercity.ca

Hi Justin,
We have a 10 year old model of that saw.
2 rows of fingers on top,
1 row of fingers on table at the start of the track. We never had any problems with kickbacks. We do replace missing and bent fingers as needed.
If you lower your top without running the track it can happen that the top fingers get jammed in the track. as soon as the track gets started they break or bend.

9/14/16       #11: Straight line rip saw personal safe ...
Mark Elliott Member

Justin,

Not trying to beat a dead horse to death, but I did ask my guy who runs that saw the most, and he said he wasn't getting any kickbacks from it.

Hope all this help outs,

Mark

9/15/16       #12: Straight line rip saw personal safe ...
Joe Calhoon

Our import Oliver has the 3 sets of anti kickback also. We have had no issues with kickback in 10 years. The set in front of the feed belt takes a little getting used to but I think a good safety feature.

Thanks for pointing out the plastic inserts Mark. I checked mine and thought they were all in but upon further inspection several were missing. The missing ones were packed with oily sawdust and looked the same.


View higher quality, full size image (2016 X 1512)


View higher quality, full size image (2016 X 1512)

9/15/16       #13: Straight line rip saw personal safe ...
Mark Elliott Member

Joe and Justin,

I tend rip shorter pieces and those are the ones that are going to kick back, not the longer rips.

When I started to have some of the shorter pieces kicking back a long time ago, that's when I recognized the importance of the rubber inserts in the chain.

Since keeping a close eye on those we just don't have kickbacks anymore.

I too have a newer Diehl along with the Northtech rip saw and have had some kickbacks on the Diehl with some shorter pieces. The anti-kickback fingers has stopped them.

David has offered the best piece of advice that can't be over looked.

Step aside until the piece has cleared the blade. When those pieces come back, it's scary the force they come back with. I have had to replace some of the fingers on my saws.

Mark

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)