Subject: Re: Should I add a brush sander to the back of my wide belt sander?

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Should I add a brush sander to the back of my wide belt sander?

8/7/17       
Jeremiah Nielson  Member

Website: jeremiahcolleciton.com

I have an SCM 42” double head sander. One option that was available for the sander from the factory was a brush sander/buffing wheel on the back if the machine. The unit has its own motor and looks like it would just bolt on the back of the sander. I’m wondering is anyone out there can tell me if this type of sanding wheel will cut down or eliminate our orbital sanding. I use a 120g / 220g belt sequence and orbit sand by hand after. The only thing we sand is edge glued solid wood panels. No doors or anything with crossgrain scratches. The flap or brush will be sanding with the grain. We use rubio monocoat for finish. No stain so blotchiness isn’t a issue. Thanks!


View higher quality, full size image (1872 X 1196)


View higher quality, full size image (1872 X 1196)

8/8/17       #2: Should I add a brush sander to the ...
Bill

I don't think the brush would help. Why do you need to use an orbital sander after the wide belt?

8/8/17       #4: Should I add a brush sander to the ...
Jeremiah Nielson  Member

Website: jeremiahcolleciton.com

You can see the long scratches in areas where the grain curves. Do people recommend not sanding after the wide belt? I feel like it’s required. The 220 belt does a good job but not hand orbital good.

8/8/17       #5: Should I add a brush sander to the ...
Bill

Get with your abrasive person. I would think you could get a finish that would be acceptable with the right abrasive. You might have to work on belt speed and conveyor speed to get the right combination.

Worth a shot before you begin to modify/replace the machine.

8/8/17       #6: Should I add a brush sander to the ...
rich c.

A wide belt is not a finishing sander, and I don't try to treat it like one. A brush sander will not sand the hard grain as well as the soft and you will not have a flat surface after using it. Not popular for this generation of woodworker's, but I love a good stroke sander. 150 off a stroke sander is like 220 everywhere else. You can feather out any tear out on hardwood, and really put on a fine job. Hardly ever see them these days!

8/8/17       #7: Should I add a brush sander to the ...
B

We still use our stroke sander! Great for curved/concave work too.

Have you thought about a gang orbital sander? I see them sell for fairly cheap on the used market. Might be worth it if your sanding a lot.

8/9/17       #8: Should I add a brush sander to the ...
Bill

Might not translate but our segmented platen sander is a finish sander. We are sanding plywood but I think there are the same challenges. We run it through twice opposite directions so it cuts the raised fibers from the prior pass. In testing the finish is the most uniform straight out of the wide belt.

Jeremiah can you describe how you are sanding and what abrasive you are using. Drum Drum, Drum Platten.....

8/10/17       #9: Should I add a brush sander to the ...
Kevin Jenness

Another vote for stroke sanders. I would love to have a feed through sander that produces a finish ready surface. I am willing to believe they exist, but I would guess quite costly. Bill, can you give some specifics?

All the shops I am familiar with do further sanding after the wide belt, usually with hand-held random orbital sanders. A stroke sander used skillfully is far faster.

8/10/17       #10: Should I add a brush sander to the ...
Bill

We have a Butfering widebelt. Two head, Drum, combination head. For finish we use silicon carbide abrasive off the platen only. As I said we run it both directions to cut the raised fibers from the prior pass.

The sander new several years ago was $60 +/-. Paid for itself many times over.

You can't just pick any abrasive and speed. There is some science there. We took a Stiles training course on sanding and maintaining the machine. Again that course has paid for itself many times over.

8/10/17       #11: Should I add a brush sander to the ...
Mark B Member

Without some type of oscillating head or finish sander beyond even going to 220 (which is crazy for us, 180 max) I cant see how you could NOT finish sand. Even with no cross grain the sanding scratches are brutally obvious.

8/14/17       #12: Should I add a brush sander to the ...
Bill

I am not an expert by any stretch but there are a lot of things at play here.

Size of the platen, how hard is the platen? Abrasive, what is the abrasive they are not all the same? What is the conveyor speed, what is the belt speed? What sequence of belts are you using, what is the abrasive of the belts leading to the final sanding?

I'll bet SCM has a wide belt expert that would be willing to help. I would call SCM and find him or her. If you said their wide belt could not produce finish quality I bet they would disagree. We had tons of samples from abrasive companies to get the right abrasive. We sand to 180 by the way. Do you think a cabinet company that produces 1,000's of cabinets a day is RO sanding them all, not a chance. It can be done.

8/14/17       #13: Should I add a brush sander to the ...
Ryan

One issue I see here is the sequence of your belts. You are likely putting too deep scratch with a 120 grit to take out with the 220 grit. You could consider two passes and have two grits (go 120 / 150 grit, then 180 / 220) in between. This should greatly minimize your need to orbital sand after.

11/27/17       #14: Should I add a brush sander to the ...
Adam West  Member

Website: http://www.surfprepsanding.com

I travel the country as a technician for SurfPrep abrasives, teaching folks how to work through issues like this.

If the grain is all straight and homogenous then staining right out of the wide belt is easy. Once you add in knots, burls, and curls things get a bit more complicated.

Hand sanding is often the best option. They key is teaching the hand sanders how not to over sand.

Color consistency is also a major issue going from the wide belt to hand orbital sanding. It is extremelyimportant that both operations work together.

I would be happy to talk to you about your options. PM me and we can talk it through.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)