20mil vs 10mil

4/23/13       
Leo G  Member

Website: http://www.lrgwood.com

Pretty inexperienced with veneering but have been in the woodworking field for 20 years with my own shop.

I am making a curved wall desk, I will be using FlexBoard for the front of the desk which I will be using a vertically aligned ribbon striped Sapele'. I am using paper backed and have a choice between 10 mil and 20 mil. The curves are very gradual. One of the desks is somewhat an "S" shape and the other is a "C" shape with radius's on the order of greater than 9'.

I would prefer to lay up the veneer flat and then bend the FlexBoard, but that isn't set in stone.
This is a desk that will be used in the commercial world so it should be more durable than a residential project.

So, which would be the better choice for the thickness of the veneer for me?

Also as a side question. If it's listed as a 20mil paper backed veneer is the whole thickness 20 mil or is the veneer thickness 20 mil.

Thanks.

I'm sure I'll be in here a bit more often as this job progresses. :smile:

4/24/13       #2: 20mil vs 10mil ...
Wyatt

The mil thickness refers to the paper not the veneer. The veneer is the same thickness on both. I would use wood on wood aka 2 ply rather than paper backed if you need to use sheet veneer. I personally feel the bond is better. What method do you plan to use to adhere the veneer?

4/24/13       #3: 20mil vs 10mil ...
Leo G  Member

Website: http://www.lrgwood.com

Was planning on using epoxy or contact cement. Using FlexBoard which has a hardboard surface (not tempered). I need to find out how the veneer is going to react with the epoxy.

I don't have a vacuum bagging system or I'd use PVA.

Now that is a surprise about the mil rating. I would have never guessed the paper was what the measurement was for. Any idea how thick the wood veneer is going to be (best guess)?

4/24/13       #4: 20mil vs 10mil ...
Robert Member

My guess would be is that the veneer itself is thinner than a strand of human hair. Seems to be the norm now a days.

4/24/13       #5: 20mil vs 10mil ...
Leo G  Member

Website: http://www.lrgwood.com

That was exactly why I was asking about the thickness. Trying to find out what I'll have there to sand. I'm hoping it's not going to be the standard .015 that I've been seeing on 4x8 plywood. I really can't figure out how the heck they make it that thin and then expect us to be able to work with it.

4/24/13       #6: 20mil vs 10mil ...
Wyatt

It may vary by supplier but I was told the veneer on 10 mil is .020 and on 20 mil it's .035. You could buy loose veneer and seam it yourself. You would have much more thickness for sanding. I wouldn't use epoxy or contact cement. If you are planning on laying up the veneer prior to bending can you get someone with the proper equipment to press it for you with pva?

4/24/13       #7: 20mil vs 10mil ...
JeffD

Leo, I would call around and question your suppliers about the veneer thickness. I work mostly with domestic hardwoods and the veneer I get is a bit thicker than what I get on ply or mdf. The worst I've seen is foil backed at another shop I worked at. That stuff probably is as thin as a human hair! I've sanded a LOT of veneered panels over time and I've never encountered anything else that thin.

I would not use contact for veneer. If you do some searching on the web there's a lot of good info out there on veneering. I have a vac so use TB cold press. If you can swing it they're great tools to have. You'll find yourself using it for other things you may not have thought of before.

good luck,
JeffD

4/24/13       #8: 20mil vs 10mil ...
Charles  Member

Website: http://www.northcreekwoodworks.com

Here's my shameless pitch: We can make 2 or 3 ply wood on wood for you the exact size(s) you need and matched if req. It can provide it un-sanded or hit & miss sanded if you wish ( we rarely use tape on our faces). The best way to apply 3 ply (unless you have a press of some sort) is to contact cement it except for a 3/4-1" area around the edge which can be white glued.

FYI: most veneer these days is cut at .024" (1/42"); i doubt anyone would make a paper back product at .035, but who knows.

4/24/13       #9: 20mil vs 10mil ...
Rich

If you don't have veneer equipment, why veneer? Ribbon stripe sapele isn't hard to get as solid stock. Why not glue it up like barrel staves and be done with it. No messing around with questionable gluing methods, or thin veneer that are tough to sand.

4/24/13       #10: 20mil vs 10mil ...
Charles  Member

Website: http://www.northcreekwoodworks.com

.....because it will not match and will probably crack...or maybe it won't. Can't be sure.

4/24/13       #11: 20mil vs 10mil ...
Leo G  Member

Website: http://www.lrgwood.com

Because one desk is 17' long and the other is 9'. It would take too long and be to cumbersome to do it that way.

4/24/13       #12: 20mil vs 10mil ...
JeffD

Be fun to check the shrinkulator to see how much 17' of solid sapele will move seasonally:>0

Yup....veneers the way to go.

JeffD

4/24/13       #13: 20mil vs 10mil ...
Leo G  Member

Website: http://www.lrgwood.com

Ya, that would be the other reason ;)

4/25/13       #14: 20mil vs 10mil ...
Rich

Nice to know the desk is 17'. Maybe a piece of information we could have used in the beginning. Charles, Solid wood would not match what? And why would it crack? There must be some information around this post I don't know about.

4/25/13       #15: 20mil vs 10mil ...
Charles  Member

Website: http://www.northcreekwoodworks.com

Rich:

Not match: As in inconsistent color, aka the butcher block look. People (not all) like the consistent look of veneer.

Crack: As in when the wood contacts over 17 ft of width (which we now know) it will split. If a 17 ft wide solid panel contracts 1/2 of 1 %, that would be 1" !!!!!

No need to 'esplain.

On a positive note, you are correct about vague descriptions and lack of details. Drawings should be required with questions per the above.

4/25/13       #16: 20mil vs 10mil ...
JeffD

Hmmm, I agree in general that more info = better questions = better answers.

However when the question is specifically about veneer characteristics and the OP never mentioned solid wood in any way so was never part of the conversation..... I think the OP was fine here;>)

JeffD

4/25/13       #17: 20mil vs 10mil ...
Leo G  Member

Website: http://www.lrgwood.com

Either way.

I ordered the 20 mil.

The veneer is a pathetic 1/42"

Thanks for the insight


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)