Need advice on large panel raise

11/3/16       
chad@adamsarch.com

Website: http://adamsarch.com

I have a contractor asking if we can build a door with a large panel raise. My guys in the shops have discussed several ways that we could possibly do it but we can't settle on one way or the other. Attached is a picture of the door. Here are a couple ideas we have in the shop.

1.) Put the panel on the CNC and step route it out. And then sand the heck out of it to get rid of the ridges.

2.) Buy a large knife and put on a shaper and then run through. Very scary due to how long the knife is.

3.) We have a shaper that has a spindle that runs horizontally. Put a knife into spindle a run the part. In order to put the raise on the other side we will have to make a jig to hold the panel straight and level.

Do you guys have any other thoughts or experience with running long raised panel profiles safely and effectively?


View higher quality, full size image (652 X 990)

11/3/16       #2: Need advice on large panel raise ...
Mark B Member

If none of the panel raise profiles exceed 7" run then on a W&H (open ended).

11/3/16       #3: Need advice on large panel raise ...
Rick W

It looks like you could do the outside profile of the raised panel with a standard shaper and appropriate cutters.
I would do the pyramidal inner profile with hand planes. I'd use a plane with a radiused blade, like a scrub or jack plane to rough it out, and a smooth plane to finish. It will probably take a lot less time than you think it will.

11/3/16       #4: Need advice on large panel raise ...
JeffD

If you can run it through the horizontal spindle I think that's how I'd do it, or if it's only a one-off Rick's suggestion would be pretty good.

I would not raise both sides of the same piece of wood. I would instead have two panels back to back.

good luck,
JeffD

11/4/16       #5: Need advice on large panel raise ...
Mark  Member

Are the existing panels one piece?
I did something similar to the pyramidal(sp?)
panels some time ago, but paint grade. Made the panels in the planer with a taper sled and cut the ends on a tablesaw with a 16" blade- as I remember, had to finish the end cut with a handsaw and plane smooth.On some wide panels, made in two halves and glued back together.
If the existing panels are one piece and you have to follow suit, I'd say get knives ground to run them vertically if you have a shaper with the space under the nut.
Another way might be to resaw the panel portion off the blank, mill the panel and glue back together to keep the grain (mostly)matched. One last way would be a router jig, but that may be slooow.......

11/4/16       #6: Need advice on large panel raise ...
Tom Gardiner

The pyramidal portion of the panels can be programmed fairly simply in V-carve Pro. Or any 3d cad/cam package. I would think it would take about fifteen minutes per pane side to run the pyramid then run the tongue in V-carve. Clean up would be perhaps a handplane then sand to remove scallops.

11/4/16       #7: Need advice on large panel raise ...
doug mclaren  Member

bandsaw bevel, clean up on jointer, shape perimeter with shaper or saw. looks like enough of offset.

11/4/16       #8: Need advice on large panel raise ...
Chad

Website: http://www.adamsarch.com

Thanks for your responses. With your feedback I would say we are leaning towards using the horizontal spindle shaper or programming it on V-carve and cutting it on the CNC.

I do like the idea on the W&H, however we sold ours about 2 years ago and hard to justify a new machine for one job at this time.

We have also made a sled for our planer in the past to make wooden sills for windows or thresholds for doors.

It is nice to get some feedback that is along the same lines as what we are thinking - it gives you a lot more confidence in moving forward.

11/4/16       #9: Need advice on large panel raise ...
TonyF

If it were me, I would run the basic raised panel such as the one on the bottom, which looks like the same profile that is repeated on the perimeter of the upper panels.

I would band the perimeter raised panels to prevent wood movement.

For the pyramids, I would miter together a pyramid out of 3/4" veneered panels, and attach it to the panel with the perimeter raise. This would prevent a sizeable area of end grain and be easier to finish, and if you used veneered panels for the pyramid it would prevent wood movement.

If this were a painted door, I would do the panel parts out of fiberboard. If this were an exterior door, I would pass on the project, as it would be a warranty nightmare.

My two cents.
TonyF

11/4/16       #10: Need advice on large panel raise ...
Chad

Hi Tony - thanks for your feedback.

Although the picture makes it look like I am building this for an interior door - the contractor needs this door for the front entry of a house.

11/4/16       #11: Need advice on large panel raise ...
doug mclaren  Member

seems it would be a nightmare to sand machine marks from cnc. thats a lot of cross grain to shape even if you gang then rip then do long grain

11/4/16       #12: Need advice on large panel raise ...
David R Sochar Member

I have done several variants of this a few times. This one is easy because you can make the panel in 3 pieces, maybe 4.

Plan on the two pyramid faces to be made and then attached to the flat panel "perimeter". If you prefer, do it as one flat panel or two thinner ones, then pair them up and put them in the rabbets.

Make the pyramids one of three ways: Bandsaw and joiner, as mentioned; horizontal shaper with a knife of lesser projection; a 12" or 14" table saw with a fixture to fasten the bottom - flat - side of the panel to; a large planer and a jig to sit the panel into and subsequent passes.

I think in all cases, I would make the pyramid parts loose and apply to the panel afterwards, instead of all out of solid.

But all that is moot since a CNC can do anything (insert some damn emoji thing here denoting cynical humor). Sand out the steps?!? Can a CNC do that?

And as for those lower panels in the photo, my CSI door skills tell me that those panels are replacements as the originals rotted away.

11/5/16       #13: Need advice on large panel raise ...
Wood dust

I too agree with others on the point that I wouldn't make that 1 panel raised on both sides , that would be two loose panels back to back .

In our shop that would be done on our CNC . That's a fairly easy cut in alphacam . The run time would be some where around 20 minutes with very little sanding when it came off . I just wouldn't justify the cost of a custom knife for the horizontal shaper .

Looking back 3 years ago , our only option would of been to run these with a horizontal shaper . Which when I look at that point , I wonder if the feed rollers will just break or flatten that point . And also foresee you needing to make a sled to push those through anyways .

Best of luck and keep us posted on your end result .

11/5/16       #14: Need advice on large panel raise ...
Tom Gardiner

By programming the cnc to ramp down on the angle of the bevels the only clean up required is a small scallop between the parallel toolpaths. You can determine the best compromise between cnc run time and sanding when you decide on the closeness of the tool passes. A 1/2" ballnose will make quick and clean work of it.

11/7/16       #15: Need advice on large panel raise ...
doug mclaren  Member

just curious, how long does it take to program something like that?

11/7/16       #16: Need advice on large panel raise ...
Wood Dust

I just did a quick test run on programing it in Alphacam, took me 10 minutes to draw and create the tool path.

11/8/16       #17: Need advice on large panel raise ...
B.H. Davis Member

I've done similar pyramid projects on our CNC using Enroute software. With a step over of .025" per pass on a half inch core box bit it made for surprisingly little sanding.

BH Davis

11/18/16       #18: Need advice on large panel raise ...
Wood Dust

Chad, I am curious to know how you ended up going about this?


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)