Pitch builds on left side of blade only -- 0 -- 
12/31

Website: http://www.jeffscabinets.com
Why is it that my saw blade always gets pitch build up on the left side only? I have measured the fence to blade using a combination square , same tooth, front and back to make sure the fence is parallel.
I find the hardest thing to do for each job is making up face frame stock and having it all come out the same width. We used to rip 1/16 oversize then plane the edges but it seemed the edges would get out of square because the pieces would tip a bit.
The last job we ran one edge over the jointer then ripped 1/16 over size, then ripped again removing only 1/16 of material. The saw blade ( Forrest Woodworker 2) makes a much smoother cut when only removing that 1/16 of material. Last step, we kiss the edge on the edge sander before assembly. Seems like a lot of work but our frames come out nice every time.
Just got me wondering how other guys go about making up precise stock.
Thank you!
Jeff C
12/31 #2: Pitch builds on left side of blade ...

The only way to be sure your blade isn't healing is to use a dial indicator. I like the setup Woodcraft sells I think they call a Oneway? http://www.woodcraft.com/Product/126979/oneway-multi-gauge.aspx
It is an indicator mounted in a nice casting that is square and has 4 machined edges. Set your crosscut gauge on exactly 0, put the 4 way indicator against it and check the blade front to back (adjust trunion to crosscut gauge not gauge to blade), once this is correct you can adjust your rip fence by using the One way against the fence and checking blade front to back. Pitch on one side of the blade is almost always a product of the blade healing (dragging). Also while your at it make sure blade stays plumb during vertical moves - many do not!
12/31 #3: Pitch builds on left side of blade ...

I generally joint, rip, then gang up pieces and run them through the planer with good results.I use a Delta lunchbox planer with a 1/32" cut and get no snipe and square edges. You may need to tune up your planer. For slower but guaranteed square milled edges, run the jointed edge against an outboard fence on a powerfed shaper after ripping, climb cutting if necessary to eliminate tearout. You can also gang feed ripped stock through the wide belt sander. You can control for rolling of material by using a sled with fences at the edges and trailing end of ganged stock as you plane or sand them. If sanding, you need to keep the rips as consistent as possible to reduce sanding time; a power feed on the ripsaw can help here.
Double ripping and edge sanding seems unnecessarily laborious and inaccurate. The rip quality should be at least as good with the initial cut as when removing a final 1/16". The pitch buildup probably is caused by misalignment of the blade and fence, and Chris offers a good method for adjusting that.
1/1 #4: Pitch builds on left side of blade ...

Website: http://www.jeffscabinets.com
Thank you guys for your responses. I checked out the oneway gauge and that looks like a very useful tool so I will get one for sure. I did not know a blade can go out of plumb in a vertical move, that will be interesting to see. Kevin, your probably right that me planer needs a tune up. And I am interested in making a sled to use with the planer to keep the stock standing up straight. Thanks again for your help guys! - See more at the following link:
http://www.woodweb.com/cgi-bin/forums/cabinetmaking.pl?form=771622#sthash.lydR5J4V.dpuf
1/1 #5: Pitch builds on left side of blade ...

Website: http://www.awwtx.com
You don't saw what type of saw you're using. Regardless, the blade should be set parallel to the miter slot and the fence set parallel to the miter slot. If your fence doesn't lock parallel consistently either get in the habit of checking it, front and back, against the miter slot or consider replacing the fence.
My stock preparation method depends on the project. Furniture grade stock is face jointed, planed to thickness, edge jointed, ripped 1/4" over, cut edge jointed straight, ripped to 1/32" over (first jointed edge is the waste edge), then a final jointer pass to clean up the cut edge.
For cabinet work the stock is planed to thickness, jointed one edge, ripped 1/16" over, and run through the planer in groups. That helps keep the edges square.
1/1 #6: Pitch builds on left side of blade ...

Website: http://www.jeffscabinets.com
Bill, it is a Powermatic model 66.
Thank for your response.
1/1 #7: Pitch builds on left side of blade ...

n lieu of an S4S machine, why not run it thru a powerfed shaper with a sticking plate with outboard fence like offered by Weaver?
Yields dead on width and removes saw marks at same time. Would require two runs thru the machine to get both edges.
Would also eliminate chance for tipped and rolled over edges associated with jointing, planing or sanding on edge.
1/3 #8: Pitch builds on left side of blade ...

We rough cut our stock on the SLR. Then it goes through the planer and sander on edge ganged up. I place the stock on edge and clamp or hold the stock tightly together. Then I run masking tape around the ends and remove the clamp etc. There is no need for a sled but I have used one on the past. I like taping the stock because you can run one edge through the planer then right through the sander and then the other face with minimal set up time. IF you don't have a sander you could still leave the pcs taped and hit them with an orbital or belt sander to speed that process as well
Before this method we ran all of our stock through the shaper with an outboard fence and a four wing cutter with replaceable carbides. If I'm doing a large volume the shaper is the way to go but for 10 -50 pcs the planer and sander is the fastest.
2/23 #9: Pitch builds on left side of blade ...

Edgetek makes a disc to use in the table saw for edge sanding that works really well for making face frame stock square, straight, and uniform width. It is beveled, so you need to set the bevel to 2 degrees and then just push the material through a few times. They have 80 & 120 grit discs; I like the 80 grit because it cuts fast and takes off enough material to get rid of saw marks, etc. quickly. It is a little work, but the stock comes out perfect, especially if you use it to sand the faces first (for stock that is not too wide). I find that a little work up front saves more work later on.
0 -- 
Buy & Sell Exchanges | Forums | Galleries | Other Resources | Site Map
Buy and Sell Exchanges
Job Opportunities and Services Exchange
Employment opportunities and services within the woodworking industry
Lumber Exchange
A worldwide buy/sell exchange for lumber and wood products
Machinery Exchange
A worldwide buyer and seller exchange for woodworking machinery and equipment.
Classified Ad Exchange
Classified advertising for the woodworking industry (for advertisements that do not include machinery, lumber products and employment listings)
Forums
Adhesives Forum
Discussing topics related to adhesives within the woodworking industry
Architectural Woodworking Forum
Discussing quality standards and production of architectural wood products
Business and Management Forum
A forum for the discussion of business topics: from sales and marketing to dealing with difficult customers.
Cabinet and Millwork Installation Forum
Discussing all aspects of installation issues encountered by cabinet and millwork installers.
Cabinetmaking Forum
Discussing 32mm and face frame cabinet construction including fabrication, casegoods design, and installation.
CAD Forum
Shedding light on the all-too-often shadowy world of CAD.
CNC Forum
Discussing CNC (computer numerically controlled) woodworking equipment, software, and automated product manufacturing.
Dust Collection, Safety and Plant Operation Forum
Discussing topics related to maintaining a safe and productive working environment.
Professional Finishing Forum
Finishing issues for the production environment
Forestry Forum
The science and art of forest cultivation and timber management, planting, surveying, tree diseases, silviculture and timber harvesting
Professional Furniture Making Forum
Helping professional furniture makers improve quality, save time, and increase profits
Laminating and Solid Surfacing Forum
Issues related to laminating and solid surface materials and processes
Commercial Kiln Drying Forum
Discussions covering issues faced be commercial drying operations that process at least 750,000 bd. ft. of lumber per year
Sawing and Drying Forum
Discussing topics related to primary processing and drying of lumber
Solid Wood Machining Forum
Discussing topics related to the machining of solid wood
Value Added Wood Products Forum
Learn how to improve your output, find new markets, and boost sales of your lumber products
Veneer Forum
Discussing topics related to veneer processing, manufacturing, and fabrication
WOODnetWORK
An electronic discussion group for woodworkers throughout the world
Galleries
Project Gallery
Where professional woodworkers can post examples of their work
Sawmill Gallery
Professional primary processing companies display and describe their sawmill facilities
Shop Gallery
Professional woodworkers display and describe their shop facilities, products and equipment
Shopbuilt Equipment Gallery
Professional woodworker's jigs, rigs, and shopbuilt equipment
Other Resources
Industry News
Late-breaking news from all sectors of the wood industry
Video Library
Index of industrial woodworking related digital videos on the web
Auctions, Sales and Special Offers
Advertisers offering woodworkers discounted prices on good and services, and announcements of upcoming auctions
FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)
WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
A valid email return address must be included with each message.
Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
Subject lines may be edited for length and clarity.
"Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
(return to top).
Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.
You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.
WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.
Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).
Libel: Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.
Improper Decorum: Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).
Advertising: The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).
Repeated Forum Abuse:
Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.
There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).
The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)
Forum Posting Form Guidelines
|
Your Name
|
The name you enter in this field will be the name that appears with your post or response (return to form).
|
Your Website
|
Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
|
E-Mail Address
|
Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
|
Subject
|
Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
|
Thread Related Link and Image Guidelines
|
Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
|
Thread Related File Uploads
|
Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .FLV .MP4 (Image Upload Tips) If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
|
|
|
|