equipment upgrades? -- 0 -- 
1/20

I'm a one man shop that does both residential and commercial. My largest client has more than doubled their order for this year and I'm looking to speed things up. These are just edgebanded melamine casework and shelving. Currently I cross cut on vertical panel saw, rip on cabinet saw, clean edged on router table, edgeband on bander, then assemble with pocket hole joinery.
Does anyone see where a different process or a added machine would benefit? I was thinking a sliding table saw with scoring to skip the clean up step. As it is now it takes about 7 hrs to cut 68 sheets into 700 pieces and have them ready to band.
1/20 #2: equipment upgrades? ...

68 sheets of what ?
sounds like your going around in circles
Why not purchase a quality vertical panel saw with a scoring blade ?
1/20 #3: equipment upgrades? ...

A bander with premill would also save you, The vertical panel saw with scoring would also help a lot
1/21 #4: equipment upgrades? ...

No shelf pin holes ?? is cnc and a bander a consideration ?
1/21 #5: equipment upgrades? ...

Right now I use the metal standards and clips for shelves. I got the senco stapler which sped it up from screwing on. I'm on the lookout for a 23 hole line bore now. I got the kreg foreman and I'm going to up grade to the more industrial version that has two drills. As far as cnc goes it's crossed my mind but don't know if the investment is worth it just for simple cuts. I got about $20k for tool upgrade.
1/21 #6: equipment upgrades? ...

With a 4 x 8 Atc or X3 model at 28-38 new you would come off machine ready to edgeband. with the economy a lot of shops who used medium and lighter machines to grow into larger CNC's are selling and getting bigger machines. I would not rule it out. if you have 20 k in pocket you have some buying power shop diligently.
1/21 #8: equipment upgrades? ...

I'm not familiar at all with cnc. Is there any brand to look for or stay away from? It makes sense to go that route having all machines in one but I don't know about the learning curve.
1/21 #9: equipment upgrades? ...

I'm looking at your original post.
Have you considered out sourcing the sheet cutting to some other shop with large capacity and you just assemble ?
This is just a thought so that you can focus in on the custom high dollar items that generate added profit ?
just a thought
1/21 #10: equipment upgrades? ...

Website: closetexperts.com
CNC requires investment in electric, dust collection, and vacuum pump in addition to CNC. New set of issues with associated learning curve. My perspective is CNC is best after CAD software.
I was a one man shop making closet parts. I loved the vertical and was glad I did not go sliding table. I would be after minimizing waste with the equipment I have.
I would figure out how to eliminate the cleanup step and the motion between the two saws, cross cutting and ripping. I used a vertical panel saw without scoring to cut exclusively melamine. Downside was having to use two to three blade changes to cut 66 sheets. Fortunately they are quick changes. Scoring would cut that.
The value of the vertical is to stack cut and cross cut as much as possible, turning rips into cross cuts, where the vertical excels.
Finally, I would set up my process for more flow, processing a certain number of sheets from cutting through assembly, as my space would allow.
I assume you are familiar with Paul Akers and Lean. If not, I suggest you start watching his videos. or purchase his 2 Second Lean book.
Good luck!
1/21 #11: equipment upgrades? ...

I did what cabinetmaker suggested, I took bigger jobs, did two large Amazon complexes by using Cabparts and made a good buck. take your time there are lots of ways to do this.
when the time for a CNC gets there it will be apparent so I would start looking into it. buying one is a process of Due diligence and nothing to take likely. the learning curve has been greatly reduce from what it was a few years ago. there are several discussion forums you can look to as a small cabinetmaker, two of the strongest are camheads.org and letstalkshopbot.com you do not have to purchase a machine to join these discussions but there are lots of guys like us on both of them.
1/21 #12: equipment upgrades? ...

Are you having to do any secondary operations such as line boring, assembly borings, grooving or dadoing?
I would first focus on processing the panels-are these rectangular pieces, any angles(certainly doable on vertical with jigs)?
If so I would look at a quality vertical-Striebig, HH, Hendrick...benefit is edgebander ready parts, stack cutting, safety and easier handling.
Have you considered a PTP? Not near the upfront costs on the machine, software, learning curve, ect.
Most somewhat current PTP's have routing as well as line and construction boring and grooving capability plus the software is onboard and programmed on the fly at the machine.
I bought a 98 Weeke BP60 with I think 4hrs on the clock from a high school for 3400.00 The kids were using it for a picnic table. My tech offered 12k before we hooked power to it-rare time capsule find but persistence pays off.
A lot depends on your final product and any repetition involved.
I do residential cabinetry so I'm dealing with cookie cutter end panel stuff for the most part -recall the program, vac it on the pods, press the zone start, remove and repeat.
I process panel stock on a 26 yr old Striebig, go to the PTP, edgeband and assemble with confirmats.
1/21 #13: equipment upgrades? ...

Website: http://morantzcabinets.com
Vertical with scoring or slider with scoring. I think vertical alone should do the job. Double line boring machine set up for 32mm system holes and dedicated hinge borer to drill insert cams into shelves /top/bottom. No pocket holes needed. Most closet companies do it this way.harold
1/22 #14: equipment upgrades? ...

68 sheets of melamine in a day...I herniated a disc just thinking about it. Hope you have a vacuum panel lift?
Seems like anything you can do to cut out the cleanup on the router table would be a huge benefit.
1/22 #15: equipment upgrades? ...

100pc./hour! Want a job? That is faster than our CNC. Improvements: a saw (Striebig) to eliminate the edge cleanup, a linebore machine (Conquest) to eliminate the 255 standards. Neither of these will make you faster than 100 pc. / hour though.
1/22 #16: equipment upgrades? ...

No lift. Just move stack near saw and go at it. I've been building these same cabinets for about 5 years do For the tools I got I have found the the perfect system. But it's a lot of hard work so I'm trying to simplify it. What is a ptp? And till last year I would do about 1800 feet of peel and stick. The edgebander has been a wonderful addition so I'm hoping to find something that makes that type of impact on the shop.
1/22 #17: equipment upgrades? ...

Website: http://mcgrewwoodwork.com
A ptp, takes a precut panel and can correct size, drill construction holes, drill shelf holes and any other needed machining. I had one and sold it.
A nested CNC table will take a panel cut all parts to size, do any face panel machining holes etc. and will not as a standard cnc to horizontal boring. it will however do much more than panels. I like to make all kinds of parts fluted columns, custom panels, carvings, My cnc has made me some real Chump ($$$$) that was in addition to my panels.
1/22 #18: equipment upgrades? ...

Whats the end product? That will drive the joint selection, and machinery needed to produce it.
First order of business is to produce a bander ready edge off the saw. That's where I would stake 1/3 to 1/2 of my budget capital.
Next lose the 255's. They cost money to buy and a lot of labor to install to gain a product that looks like something off a 1968 episode of Dragnet.
A double line borer is the way to go if not going cnc or ptp. The market is flooded with them after everybody jumped on the nested router bandwagon.
1/22 #19: equipment upgrades? ...

I would not expect the same degree of improvement as you gained from the bander. That was a huge change.
I would look at how I could eliminate the edge clean up and the pilasters. A cnc can accomplish both at the same time with a large investment on many levels.
Or you can change to scoring saw to address the chipping and a line borer to eliminate the pilaster and its material cost. With a line borer you can use it for part alignment too, by inserting location dowels to speed alignment. Either of these would be much simpler to implement, and can be done in stages.
If a high percentage of your work is from the one customer, I would be reluctant to overextend my investment. On the other hand, if you want to expand your business and be able to widen your product scope, the cnc will aid with that.
Outsourcing the component sizing and line boring is an option if you want to free up time and pursue other work to justify the cnc investment.
I would not expect to be able to maintain your own physical output indefinitely. You are humping!
1/22 #20: equipment upgrades? ...

A ptp sounds like something to look into. After burning up the top trimmer on my k201 yesterday i was talking to previous owner and he gave me a number to a guy who sells cnc that he refurbishes, so I think I'll see what he has available. And I agree that the 255s look outdated but for the tools I have their fast but after 5 years I'm sure I've paid for a few line boring machines.
So if I'm following correct a ptp would clean up my chipped edges from current cutting, then replace the kreg foreman and use of 255.
The end product is melamine carcass base cabinets with .018 banding, and basically melamine bookcases. The pocket holes are all hidden from view for most part but if there's a faster and easier joint I'm open to it.
1/22 #21: equipment upgrades? ...

We said good bye to pocket joinery a long time ago. we use a finished panel for ends unless laminated. GO see machines different shops and methods. I saw one fellow get way layed into a machine he did not need by a personality conflict, he bought old and used and payed too much. now he is crying in his milk and praying for an exit. take your time, GO see machines and shops. lots of ways to do that !!! there is no substitute for Due diligence.
1/22 #22: equipment upgrades? ...

That level of output for 5 years?!
I suggest you write in large letters "Work Smarter, not Harder" and put it above your saw.
Put that energy into production management - the science of manufacturing - and you will see real growth and income, and not have all that hard physical labor that will age you before your time. Your work ethic is admirable, but not sustainable. My guess is that you are selling well under the market value, and that is why you are so busy, yet ill equipped.
Get yourself to a couple of shows - Las Vegas is coming up in August - and make a plan for growth. See your options and pick a path.
When purchasing machines, it is common to plan for a payback within 5 years. You have already 'paid' for all the machines, you just don't have them.
1/22 #23: equipment upgrades? ...

As far as price I'm right in there with everyone else. ive had other shops do sites for me when too busy or didn't feel like driving across the country and we were pretty close. I plan on going to Vegas this year and at least gain knowledge. I'm in southern Minnesota but travel a lot so if anyone is open to a shop tour and a shop talk lunch I'd appreciate it.
My father is an advanced machinist with about 25 years experience programming so that would help with the learning curve with cnc I think.
This customer is eventually going to disappear so I have a good 2 years left that I want to set my shop up perfectly and debt free so I can go back to the wonderful world of residential and hopefully have continued success. Woodweb has been a great help from the start.
1/22 #24: equipment upgrades? ...

I can tell you one thing is that if your from Minn. your a tough bird. I have relatives out that way. I myself could not cut that many sheets per day on my Striebig.
Need a job? ..... I bit the bullet a few years ago and dove in head first into a flat bed CNC purchase....Took over a year for me to get comfortable using it and every day I learn something new. Its also exciting ...Arch's and curves, seems like the only limitation is what's between your ears. I would start your research....BTW I paid off the CNC machine in less then two years. Not bad for a one man shop !!
1/22 #25: equipment upgrades? ...

I get offered a job a lot when people hear what I get done. I was taught to make a work day count or its not worth being there. I'm meeting with my tax lady today who also has an employment service on trying out some help. Because the workload is catching up to me. Wife don't care how much is being brought in if I'm never home.
I've always have wanted a cnc but the investment and learning curve has held me back.
Thanks guys for all the shared wisdom. I'll try not to waste it.
1/26 #26: equipment upgrades? ...

What about a beam saw? All my parts are rectangles. And most of the time I'll have 5-10 sheets of all the same cuts before switching to another layout.
As far as joint construction other than pocket holes. If all my exposed ends are melamine would I be wanting to switch to a dowel system?
Cnc looks great and I could use it for many things but I don't think it would be faster, just easier than my current way. I had Hired help this weekend and I really need to get a line boring machine. The 255s are costing me about $.75 each in labor alone.
0 -- 
Buy & Sell Exchanges | Forums | Galleries | Other Resources | Site Map
Buy and Sell Exchanges
Job Opportunities and Services Exchange
Employment opportunities and services within the woodworking industry
Lumber Exchange
A worldwide buy/sell exchange for lumber and wood products
Machinery Exchange
A worldwide buyer and seller exchange for woodworking machinery and equipment.
Classified Ad Exchange
Classified advertising for the woodworking industry (for advertisements that do not include machinery, lumber products and employment listings)
Forums
Adhesives Forum
Discussing topics related to adhesives within the woodworking industry
Architectural Woodworking Forum
Discussing quality standards and production of architectural wood products
Business and Management Forum
A forum for the discussion of business topics: from sales and marketing to dealing with difficult customers.
Cabinet and Millwork Installation Forum
Discussing all aspects of installation issues encountered by cabinet and millwork installers.
Cabinetmaking Forum
Discussing 32mm and face frame cabinet construction including fabrication, casegoods design, and installation.
CAD Forum
Shedding light on the all-too-often shadowy world of CAD.
CNC Forum
Discussing CNC (computer numerically controlled) woodworking equipment, software, and automated product manufacturing.
Dust Collection, Safety and Plant Operation Forum
Discussing topics related to maintaining a safe and productive working environment.
Professional Finishing Forum
Finishing issues for the production environment
Forestry Forum
The science and art of forest cultivation and timber management, planting, surveying, tree diseases, silviculture and timber harvesting
Professional Furniture Making Forum
Helping professional furniture makers improve quality, save time, and increase profits
Laminating and Solid Surfacing Forum
Issues related to laminating and solid surface materials and processes
Commercial Kiln Drying Forum
Discussions covering issues faced be commercial drying operations that process at least 750,000 bd. ft. of lumber per year
Sawing and Drying Forum
Discussing topics related to primary processing and drying of lumber
Solid Wood Machining Forum
Discussing topics related to the machining of solid wood
Value Added Wood Products Forum
Learn how to improve your output, find new markets, and boost sales of your lumber products
Veneer Forum
Discussing topics related to veneer processing, manufacturing, and fabrication
WOODnetWORK
An electronic discussion group for woodworkers throughout the world
Galleries
Project Gallery
Where professional woodworkers can post examples of their work
Sawmill Gallery
Professional primary processing companies display and describe their sawmill facilities
Shop Gallery
Professional woodworkers display and describe their shop facilities, products and equipment
Shopbuilt Equipment Gallery
Professional woodworker's jigs, rigs, and shopbuilt equipment
Other Resources
Industry News
Late-breaking news from all sectors of the wood industry
Video Library
Index of industrial woodworking related digital videos on the web
Auctions, Sales and Special Offers
Advertisers offering woodworkers discounted prices on good and services, and announcements of upcoming auctions
FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)
WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
A valid email return address must be included with each message.
Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
Subject lines may be edited for length and clarity.
"Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
(return to top).
Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.
You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.
WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.
Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).
Libel: Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.
Improper Decorum: Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).
Advertising: The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).
Repeated Forum Abuse:
Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.
There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).
The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)
Forum Posting Form Guidelines
|
Your Name
|
The name you enter in this field will be the name that appears with your post or response (return to form).
|
Your Website
|
Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
|
E-Mail Address
|
Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
|
Subject
|
Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
|
Thread Related Link and Image Guidelines
|
Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
|
Thread Related File Uploads
|
Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .FLV .MP4 (Image Upload Tips) If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
|
|
|
|