Hello,
We are trying to work the bugs out of using pre-finished plywood interiors using a face frame construction method. Right now our finish room is a major bottle neck so we're trying to get as many cabinets as possible to by pass that area. We would still have all of the face frames go in there ahead time to get finished and then come back out into the building area to be applied. Now since the frames are finished we do not want to face nail the frames on the cabinet so this means all frames would have to be clamped on, correct? Also, for flush ends we are experimenting with 1/4'' scribes and then applying a 1/4'' veneered skin. This would still allow the entire cabinet to be pre-finished but then it would still have to go back to the finish room for a final coat due to the flush end. I believe all angled cabinets would have to be built first and then go into the finish room with the interior being taped off to prevent over spray? I believe a lot of shops are using pre-finished ply. or melamine interiors and we're just looking for tips to make things go smoother.
Thanks
12/28 #2: Trying to use pre-finished ply. int ...

John, since you're adding a panel on the end for end-runs, you can use pocket holes, dado's and glue... the pocket holes are covered by the skin, and you don't see the pocket holes for unfinished ends...
Most use pre-finished nowadays because the level of finish is more than acceptable than what most shops can produce finish-wise and it much more economical from a materials/labor POV...
If you want or still feel it's necessary, you can still even add more coats and just consider the pre-finish as your first two coats...
12/28 #3: Trying to use pre-finished ply. int ...

John,
I switched to prefinished about 4 years ago and it was a great move. Here is a little info on how I do it, maybe it will work for you or give you an idea of your own.
I use all 2" wide material for face frames. For my finished ends, if they are raised panel, I mill a dado only 1/4" deep win the fense set 1/4". After all the finish work is done my panel side will get pocket screwed and glued into that groove and then the prefinished 1/2" ply on the inside is applied covering the pockets.(basically what Kap said). If my finished side is 1/2" ply then I mill that groove 3/8 deep and glue it and pin nail it behind the groove at an angle into the face frame. The pins hold it until the glue dries. I make 1/4" skins for the bottom. Some cabinets as you mention like islands have to basically be built all the way before finishing. I mast the floor off at the front where the ply meets the face and then cut cardboard and screw it to the back of the face frame to block out over spray. Once you work the bugs out and get a routine down pat you'll love working with the prefinished.it has saved me gobs of time and money. Heck, I can't even buy the finish for the price difference on the ply, now I don't even have to spray it. If you need anymore info feel free to email me and I'll try to help.
12/30 #5: Trying to use pre-finished ply. int ...

Website: http://csaw.com
We have a lot of guys using the Tenso connector for just this application: flat finishing their face frames and then applying them to pre-finished cabinet boxes. It's a hidden clamping connector. I'm the Lamello product manager here at Colonial now, but I ran a cabinet shop for years - believe me, it's worth taking a look at. We have a free demo machine program if you want to try it out. Let me know.
Lamello - P-14 Clip
12/30 #6: Trying to use pre-finished ply. int ...

Website: http://morantz cabinets.com
We build only frameless cabinets, but have been using the lamello clip system for almost a year. Great for quick closet assembly on site and for assembling with prefinished or laminated end panels. We find more uses every week. If lamello is offering a free trial period, I highly recommend it. The clips are not cheap, but they save so much time that they more than pay for themselves. You can glue your face frame and let clips hold tight till glue drys, but I think the clips by themselves would do the trick. Try them out. Harold.
12/31 #7: Trying to use pre-finished ply. int ...

Chris,
Those look very interesting, but as we can see with those or pocket holes, the idea is "insta-clamping" while glue dries with both systems being a back-up if glue fails...
I'd be interested in how using that is superior to pocket holes from your perspective...
12/31 #8: Trying to use pre-finished ply. int ...

Website: http://csaw.com
KAP,
I used to use pocket hole screws for a long time, and I was always frustrated how they'd "walk" on me, especially on face frames. My reveals would get all funky. Then, I'd always have to put a cover strip on over the oblong holes on the inside of the cabinets. I was kind of particular how the insides looked and those Kreg plugs were a pain.
All P system connectors (including Tenso) are self-aligning, but also allow lateral adjustment just prior to final clamping. Being totally invisible is in itself a huge advantage. You can also set up a Zeta very easily to position the connectors so that you'll achieve a fixed reveal on your FF overhang.
Yes, the purpose of the Tenso is to take the place of a clamp, and it's recommended that you always use adhesive if you're installing a permanent face frame or building a cabinet box with Tenso. However, you could accomplish the same thing with the Clamex connector and not use glue (200 lbs. clamping force). See video below. Some applications you could use Tenso without glue are valances, scribes, toe kicks, etc. As Harold mentions, once guys get the system in their hands they start finding all kinds of different ways to use it.
In addition to Swiss build quality and unmatched tolerances, Lamello will be introducing at least one new P system connector per year (this year, there were 2). So, there's a lot in can do now and it won't remain static.
Contact me at the MA office, I'd be glad to help you out directly too. 781.585.4364 x.206
http://www.lamello.com/en/home/join-wood/p-system/zeta-p2.html
4/24 #9: Trying to use pre-finished ply. int ...

That lamello biscuit cutter is damn cool. But the little holes for the allen key still kills me.
If they could figure out how how to make a cutter that drills a very shallow ring around the allen hole exactly the way the FastCap drill bit works I would completely switch over my entire method of construction.
Then just buy the little round stickers in whatever wood or prefinished color that go perfectly flush into the hole and hide the screw hole.
Send me a free tool system when you guys finally implement that idea into your system.
0 -- 
Buy & Sell Exchanges | Forums | Galleries | Other Resources | Site Map
Buy and Sell Exchanges
Job Opportunities and Services Exchange
Employment opportunities and services within the woodworking industry
Lumber Exchange
A worldwide buy/sell exchange for lumber and wood products
Machinery Exchange
A worldwide buyer and seller exchange for woodworking machinery and equipment.
Classified Ad Exchange
Classified advertising for the woodworking industry (for advertisements that do not include machinery, lumber products and employment listings)
Forums
Adhesives Forum
Discussing topics related to adhesives within the woodworking industry
Architectural Woodworking Forum
Discussing quality standards and production of architectural wood products
Business and Management Forum
A forum for the discussion of business topics: from sales and marketing to dealing with difficult customers.
Cabinet and Millwork Installation Forum
Discussing all aspects of installation issues encountered by cabinet and millwork installers.
Cabinetmaking Forum
Discussing 32mm and face frame cabinet construction including fabrication, casegoods design, and installation.
CAD Forum
Shedding light on the all-too-often shadowy world of CAD.
CNC Forum
Discussing CNC (computer numerically controlled) woodworking equipment, software, and automated product manufacturing.
Dust Collection, Safety and Plant Operation Forum
Discussing topics related to maintaining a safe and productive working environment.
Professional Finishing Forum
Finishing issues for the production environment
Forestry Forum
The science and art of forest cultivation and timber management, planting, surveying, tree diseases, silviculture and timber harvesting
Professional Furniture Making Forum
Helping professional furniture makers improve quality, save time, and increase profits
Laminating and Solid Surfacing Forum
Issues related to laminating and solid surface materials and processes
Commercial Kiln Drying Forum
Discussions covering issues faced be commercial drying operations that process at least 750,000 bd. ft. of lumber per year
Sawing and Drying Forum
Discussing topics related to primary processing and drying of lumber
Solid Wood Machining Forum
Discussing topics related to the machining of solid wood
Value Added Wood Products Forum
Learn how to improve your output, find new markets, and boost sales of your lumber products
Veneer Forum
Discussing topics related to veneer processing, manufacturing, and fabrication
WOODnetWORK
An electronic discussion group for woodworkers throughout the world
Galleries
Project Gallery
Where professional woodworkers can post examples of their work
Sawmill Gallery
Professional primary processing companies display and describe their sawmill facilities
Shop Gallery
Professional woodworkers display and describe their shop facilities, products and equipment
Shopbuilt Equipment Gallery
Professional woodworker's jigs, rigs, and shopbuilt equipment
Other Resources
Industry News
Late-breaking news from all sectors of the wood industry
Video Library
Index of industrial woodworking related digital videos on the web
Auctions, Sales and Special Offers
Advertisers offering woodworkers discounted prices on good and services, and announcements of upcoming auctions
FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)
WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
A valid email return address must be included with each message.
Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
Subject lines may be edited for length and clarity.
"Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
(return to top).
Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.
You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.
WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.
Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).
Libel: Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.
Improper Decorum: Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).
Advertising: The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).
Repeated Forum Abuse:
Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.
There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).
The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)
Forum Posting Form Guidelines
|
Your Name
|
The name you enter in this field will be the name that appears with your post or response (return to form).
|
Your Website
|
Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
|
E-Mail Address
|
Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
|
Subject
|
Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
|
Thread Related Link and Image Guidelines
|
Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
|
Thread Related File Uploads
|
Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .FLV .MP4 (Image Upload Tips) If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
|
|
|
|